Thermophysical systematics of Ni3In and Ni3Sn compounds: Ab initio database and interrelations AITranslate
Abstract AITranslate
The subject of the paper is the use of density-functional-theory methods to determine the zero-kelvin cohesive and elastic properties, as well as the vibrational contribution to the thermal properties of the Ni3X (X = In,Sn) compounds, which are interesting in the field of lead-free soldering materials. The phases are stable at low temperatures in the DO19 (hP8) structure, and at high pressures in the cubic L12 (cP4) structure. In the current work, the T = 0 K energy-volume relations given by the VASP are combined with phonon calculations using the PHONOPY code to develop a quasi-harmonic-approximation account of the vibrational contribution to the thermal properties. The resulting ab initio database is used to: i) analyze trends in the composition dependence of the cohesive energy, the bulk modulus, the elastic constants, the engineering elastic moduli and three Debye temperatures; ii) test some rather general, as well as various material-dependent correlations between these properties; and, iii) test with the present compounds the theory-based interrelations between cohesive and vibrational properties previously established in studies of the transition metals and of a large class of related Cu-X and Ni-X (X = In,Sn) compounds. In particular, the cohesive energy of the present elements and compounds is shown to correlate with an entropy-based characteristic energy, and with the vibrational contribution to the thermal expansion coefficient evaluated at the Einstein temperature.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.calphad.2020.102205
Chinese Library Classification Number:
Citation Information:
The subject of the paper is the use of density-functional-theory methods to determine the zero-kelvin cohesive and elastic properties, as well as the vibrational contribution to the thermal properties of the Ni3X (X = In,Sn) compounds, which are interesting in the field of lead-free soldering materials. The phases are stable at low temperatures in the DO19 (hP8) structure, and at high pressures in the cubic L12 (cP4) structure. In the current work, the T = 0 K energy-volume relations given by the VASP are combined with phonon calculations using the PHONOPY code to develop a quasi-harmonic-approximation account of the vibrational contribution to the thermal properties. The resulting ab initio database is used to: i) analyze trends in the composition dependence of the cohesive energy, the bulk modulus, the elastic constants, the engineering elastic moduli and three Debye temperatures; ii) test some rather general, as well as various material-dependent correlations between these properties; and, iii) test with the present compounds the theory-based interrelations between cohesive and vibrational properties previously established in studies of the transition metals and of a large class of related Cu-X and Ni-X (X = In,Sn) compounds. In particular, the cohesive energy of the present elements and compounds is shown to correlate with an entropy-based characteristic energy, and with the vibrational contribution to the thermal expansion coefficient evaluated at the Einstein temperature.
quote
| GB/T 7714-2015 | [1] Dalía S. Bertoldi, Susana B. Ramos, A. Fernández Guillermet. Calphad, 2020(71). DOI:10.1016/j.calphad.2020.102205. |
| MLA | [1] Dalía S. Bertoldi, et al., Calphad, no. 71, 2020, https://doi.org/10.1016/j.calphad.2020.102205. |
| APA | [1] Dalía S. Bertoldi, Susana B. Ramos, & A. Fernández Guillermet. (2020). Calphad(71). https://doi.org/10.1016/j.calphad.2020.102205 |
| IEEE | [1] Dalía S. Bertoldi, Susana B. Ramos, and A. Fernández Guillermet, Calphad, no. 71, 2020, doi: 10.1016/j.calphad.2020.102205. |