Direct Tracking of Charge Carrier Drift and Extraction from Perovskite Solar Cells by Means of Transient Electroabsorption Spectroscopy AITranslate
Abstract AITranslate
The best perovskite solar cells currently demonstrate more than 25% efficiencies, yet many fundamental processes that determine the operation of these devices are still not fully understood. In particular, even though the device performance strongly depends on charge carrier transport across the perovskite layer to selective electrodes, information about this process is still very controversial. Here, we investigate charge carrier motion and extraction from an archetypical CH3NH3PbI3 (MAPI) perovskite solar cell. We use the ultrafast electric-field-modulated transient absorption technique, which allows us to evaluate the electric field dynamics from the time-resolved electroabsorption spectra and to visualize the motion of charge carriers with subpicosecond time resolution. We demonstrate that photogenerated holes drift across the mesoporous TiO2/perovskite layer during hundreds of picoseconds. On the other hand, their extraction into the spiro-OMeTAD hole transporting layer lasts for more than 1 nanosecond, suggesting that the hole extraction is limited by the perovskite/spiro-OMeTAD interface rather than by the hole transport through the perovskite layer. Additionally, we use the ultrafast time-resolved fluorescence technique that reveals fluorescence decay during tens of picoseconds, which we attribute to the spatial separation of electrons and holes.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01346
Chinese Library Classification Number:
Citation Information:
The best perovskite solar cells currently demonstrate more than 25% efficiencies, yet many fundamental processes that determine the operation of these devices are still not fully understood. In particular, even though the device performance strongly depends on charge carrier transport across the perovskite layer to selective electrodes, information about this process is still very controversial. Here, we investigate charge carrier motion and extraction from an archetypical CH3NH3PbI3 (MAPI) perovskite solar cell. We use the ultrafast electric-field-modulated transient absorption technique, which allows us to evaluate the electric field dynamics from the time-resolved electroabsorption spectra and to visualize the motion of charge carriers with subpicosecond time resolution. We demonstrate that photogenerated holes drift across the mesoporous TiO2/perovskite layer during hundreds of picoseconds. On the other hand, their extraction into the spiro-OMeTAD hole transporting layer lasts for more than 1 nanosecond, suggesting that the hole extraction is limited by the perovskite/spiro-OMeTAD interface rather than by the hole transport through the perovskite layer. Additionally, we use the ultrafast time-resolved fluorescence technique that reveals fluorescence decay during tens of picoseconds, which we attribute to the spatial separation of electrons and holes.
quote
| GB/T 7714-2015 | [1] Vidmantas Jašinskas, Marius Franckevičius, Andrius Gelžinis, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01346. |
| MLA | [1] Vidmantas Jašinskas, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01346. |
| APA | [1] Vidmantas Jašinskas, Marius Franckevičius, Andrius Gelžinis, Jevgenij Chmeliov, & Vidmantas Gulbinas. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01346 |