Spin Solar Cell Phenomenon on a Single-Molecule Magnet (SMM) Impacted CoFeB-Based Magnetic Tunnel Junctions Spin Solar Cell Phenomenon on a Single-Molecule Magnet (SMM) Impacted CoFeB-Based Magnetic Tunnel Junctions AITranslate

University of the District of Columbia; National Institute of Standards and Technology; University of the District of Columbia; University of Valencia; University of Valencia; University of the District of Columbia
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The single-molecule magnet (SMM) is demonstrated here to transform conventional magnetic tunnel junctions (MTJs), a memory device used in present-day computers, into solar cells. For the first time, we demonstrated an electronic spin-dependent solar cell effect on an SMM-transformed MTJ under illumination from unpolarized white light. We patterned cross-junction-shaped devices to form a CoFeB/MgO/CoFeB-based MTJ. The MgO barrier thickness at the intersection between the two exposed junction edges was less than the SMM extent, which enabled the SMM molecules to serve as channels to conduct spin-dependent transport. The SMM channels yielded a region of long-range magnetic ordering around these engineered molecular junctions. Our SMM possessed a hexanuclear [Mn6(μ3-O)2(H2N-sao)6(6-atha)2(EtOH)6] [H2N-saoH = salicylamidoxime, 6-atha = 6-acetylthiohexanoate] complex and thioesters end groups to form bonds with metal films. SMM-doped MTJs were shown to exhibit a solar cell effect and yielded ≈80 mV open-circuit voltage and ≈10 mA/cm2 saturation current density under illumination from one sun equivalent radiation dose. A room-temperature Kelvin Probe AFM (KPAFM) study provided direct evidence that the SMM transformed the electronic properties of the MTJ’s electrodes over a lateral area in excess of several thousand times larger in extent than the area spanned by the molecular junctions themselves. The decisive factor in observing this spin-photovoltaic effect is the formation of SMM spin channels between the two different ferromagnetic electrodes, which in turn is able to catalyze the long-range transformation in each electrode around the junction area.

KeyWords AITranslate

spin SMM MTJ solar cell photovoltaic effect
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00369

Chinese Library Classification Number:

Citation Information:

The single-molecule magnet (SMM) is demonstrated here to transform conventional magnetic tunnel junctions (MTJs), a memory device used in present-day computers, into solar cells. For the first time, we demonstrated an electronic spin-dependent solar cell effect on an SMM-transformed MTJ under illumination from unpolarized white light. We patterned cross-junction-shaped devices to form a CoFeB/MgO/CoFeB-based MTJ. The MgO barrier thickness at the intersection between the two exposed junction edges was less than the SMM extent, which enabled the SMM molecules to serve as channels to conduct spin-dependent transport. The SMM channels yielded a region of long-range magnetic ordering around these engineered molecular junctions. Our SMM possessed a hexanuclear [Mn6(μ3-O)2(H2N-sao)6(6-atha)2(EtOH)6] [H2N-saoH = salicylamidoxime, 6-atha = 6-acetylthiohexanoate] complex and thioesters end groups to form bonds with metal films. SMM-doped MTJs were shown to exhibit a solar cell effect and yielded ≈80 mV open-circuit voltage and ≈10 mA/cm2 saturation current density under illumination from one sun equivalent radiation dose. A room-temperature Kelvin Probe AFM (KPAFM) study provided direct evidence that the SMM transformed the electronic properties of the MTJ’s electrodes over a lateral area in excess of several thousand times larger in extent than the area spanned by the molecular junctions themselves. The decisive factor in observing this spin-photovoltaic effect is the formation of SMM spin channels between the two different ferromagnetic electrodes, which in turn is able to catalyze the long-range transformation in each electrode around the junction area.

quote

GB/T 7714-2015 [1] Marzieh Savadkoohi, Daniel Gopman, Pius Suh, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00369.
MLA [1] Marzieh Savadkoohi, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00369.
APA [1] Marzieh Savadkoohi, Daniel Gopman, Pius Suh, Carlos RojasDotti, José MartínezLillo, & Pawan Tyagi. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00369