Anti(-bio)fouling Nanostructured Membranes Based on the Cross-Linked Assembly of Stimuli-Responsive Zwitterionic Microgels AITranslate

Indian Institute of Technology Delhi; Indian Institute of Technology Delhi;Department of Molecular Medicine, Jamia Hamdard; Indian Institute of Technology Delhi
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This study embodies the development of a thermoresponsive nanostructured antifouling membrane based on cross-linkable zwitterionic microgels for tunable water filtration and molecular separation applications. The zwitterionic vinylimidazole propane sultone (VIPS) comonomer was synthesized by reacting vinylimidazole with 1,3-propane sultone. The microgels were synthesized utilizing a one-step precipitation polymerization approach by taking 10 and 20 wt % of the VIPS with N-isopropyl acrylamide (NIPAm), 2-aminoethyl methacrylate (AEMA), with the cross-linker N,N′-methylene bis(acrylamide) (BIS) to produce MG-10 and 20, respectively. Various chemical and morphological characterizations were carried out to establish the synthesis and characteristics of microgels. Suction filtration of a dilute MG-20 dispersion was used to construct cross-linked microgel membranes of different thicknesses over a track-etched membrane support in the next step. Surface and morphological analyses validate the packed microgel layer formation. The constructed layer was temperature-switchable, resulting in a twofold increase in water flux from room temperature to 40 °C. The thin and closely packed microgel particles resulted in a sub-2 nm surface pore size, allowing for strong rejection (>99%) of small molecules. Because of the presence of VIPS, both of the microgels displayed excellent anti(-bio)fouling properties against bacterial and protein foulants. The surface demonstrated ultralow protein adsorption and a high flux-recovery ratio (>90%), resulting in antifouling performance. The stability of the cross-linked robust microgel layer without any leaching warrants dimensional stability and long-term permeability. This smart gating membrane with improved anti(-bio)fouling activity expands the scope of thermoresponsive microgel-based nanostructured membranes and has significant potential in water purification and molecular separation applications.

KeyWords AITranslate

zwitterionic microgels thermoresponsive membrane anti(bio)fouling molecular separation water purification
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00302

Chinese Library Classification Number:

Citation Information:

This study embodies the development of a thermoresponsive nanostructured antifouling membrane based on cross-linkable zwitterionic microgels for tunable water filtration and molecular separation applications. The zwitterionic vinylimidazole propane sultone (VIPS) comonomer was synthesized by reacting vinylimidazole with 1,3-propane sultone. The microgels were synthesized utilizing a one-step precipitation polymerization approach by taking 10 and 20 wt % of the VIPS with N-isopropyl acrylamide (NIPAm), 2-aminoethyl methacrylate (AEMA), with the cross-linker N,N′-methylene bis(acrylamide) (BIS) to produce MG-10 and 20, respectively. Various chemical and morphological characterizations were carried out to establish the synthesis and characteristics of microgels. Suction filtration of a dilute MG-20 dispersion was used to construct cross-linked microgel membranes of different thicknesses over a track-etched membrane support in the next step. Surface and morphological analyses validate the packed microgel layer formation. The constructed layer was temperature-switchable, resulting in a twofold increase in water flux from room temperature to 40 °C. The thin and closely packed microgel particles resulted in a sub-2 nm surface pore size, allowing for strong rejection (>99%) of small molecules. Because of the presence of VIPS, both of the microgels displayed excellent anti(-bio)fouling properties against bacterial and protein foulants. The surface demonstrated ultralow protein adsorption and a high flux-recovery ratio (>90%), resulting in antifouling performance. The stability of the cross-linked robust microgel layer without any leaching warrants dimensional stability and long-term permeability. This smart gating membrane with improved anti(-bio)fouling activity expands the scope of thermoresponsive microgel-based nanostructured membranes and has significant potential in water purification and molecular separation applications.

quote

GB/T 7714-2015 [1] Biswajit Mishra, Swayamprakash Biswal, Nidhi C. Dubey, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00302.
MLA [1] Biswajit Mishra, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00302.
APA [1] Biswajit Mishra, Swayamprakash Biswal, Nidhi C. Dubey, & Bijay P. Tripathi. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00302
IEEE [1] Biswajit Mishra, Swayamprakash Biswal, Nidhi C. Dubey, and Bijay P. Tripathi, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00302. keywords: {zwitterionic microgels;thermoresponsive membrane;anti(bio)fouling;molecular separation;water purification}