Abstract AITranslate
In the paper are summarized the market development of tantalum and niobium electrolytic capacitors and progress on the development and manufacturing of Ta/Nb capacitors both at home and abroad.
KeyWords AITranslate
1潘伦桃(译).钽固体电解电容器[J].钽铌工业进展,2001,(2):21-21.
2内藤一美.铌电容器及其制造方法[P].中国专利:1363102A.2002-02-06.
3左藤信之.铌粉末和固体电解电容器用阳极[P].中国专利:1367511A.2002-09-04.
4马强.三工位片式钽电容器真空预烧炉的研制[J].真空,2001,38(5):33-36. 被引量:3
5潘伦桃(译).固体电解电容器阳极体的制造方法[J].钽铌工业进展,1999,(1):11-11.
6徐友龙,季锐,王飞.电聚合条件对聚吡咯钽电解电容器容量与损耗的影响[J].西安交通大学学报,2001,35(6):608-611. 被引量:2
7陈青(译).固体电解电容器及其制造方法[J].钽铌工业进展,1998,(2):21-21.
8王桂川(译).钽固体电解电容器[J].钽铌工业进展,1998,(4):17-17.
9潘伦桃(译).钽固体电解电容器的制造方法[J].钽铌工业进展,1999,(4):21-21.
10佚名.新プロセスで高CV值のニォブ粉を开发[J].金属时评(日),2000,(1774):1-1.
1米玺学,马春红,万军,严国元.钽电容器用高纯硝酸锰的制备[J].湿法冶金,2013,32(5):333-335.
1欧阳一凤,李荐,姜翠玲,钟海云,刘建清,王德全.钽、铌电解电容器工艺研究进展[J].稀有金属与硬质合金,2003,31(4):32-35. 被引量:3
2铌电解电容器将成替代品[J].国际电子变压器,2005(5).
3张荣详.中频技术的发展及其市场动态[J].电工技术交流,1993(1):35-39.
4亚洲钽电解电容器市场动态[J].电子元件与材料,1998,17(5):44-45.
5钟晖,李荐,戴艳阳,钟海云.铌电解电容器最新研究发展动态[J].稀有金属,2002,26(2):139-142. 被引量:10
6卢云,蒋美莲,杨邦朝.铌电解电容器研究动态[J].材料导报,2005,19(5):23-25. 被引量:3
7刘春娜.国内光伏发电市场动态[J].电源技术,2011,35(2):133-135. 被引量:2
8温晓立,袁宁峰,王丹鹏,张庆生.铌电容器及其性能[J].有色冶炼,2002,31(6):99-101.
9康涵昌,王贵欣,陈妙,郭和一,李成佳,刘睿,闫康平.磷酸铁锂的最新研究现状[J].贵州化工,2012,37(5):21-23.
10张辉,邸永江,晁明明,侯强.YAG:Ce^(3+)荧光粉的溶胶-凝胶法制备工艺研究进展[J].中国照明电器,2014(6):5-7.
Basic Information:
DOI:
Chinese Library Classification Number:TM535.1[电气工程—电器]
Citation Information:
In the paper are summarized the market development of tantalum and niobium electrolytic capacitors and progress on the development and manufacturing of Ta/Nb capacitors both at home and abroad.
quote
| GB/T 7714-2015 | [1] OU Yang-yi-feng, LI Jian, JIANG Cui-ling, et al. Progress on the Technological Study for Tantalum/Niobium Electrolytic Capacitor[J]. Rare Metals and Cemented Carbides, 2004(1): 52-55. |
| MLA | [1] OU Yang-yi-feng, et al., "Progress on the Technological Study for Tantalum/Niobium Electrolytic Capacitor." Rare Metals and Cemented Carbides, no. 1, 2004, pp. 52-55. |
| APA | [1] OU Yang-yi-feng, LI Jian, JIANG Cui-ling, ZHONG Hai-yun, LIU Jian-qing, & WANG De-quan. (2004). Progress on the Technological Study for Tantalum/Niobium Electrolytic Capacitor. Rare Metals and Cemented Carbides(1), 52-55. |
| IEEE | [1] OU Yang-yi-feng, LI Jian, JIANG Cui-ling, ZHONG Hai-yun, LIU Jian-qing, and WANG De-quan, "Progress on the Technological Study for Tantalum/Niobium Electrolytic Capacitor," Rare Metals and Cemented Carbides, no. 1, pp. 52-55, 2004. keywords: {niobium electrolytic capacitor;tantalum electrolytic capacitor;technological study;market trend} |