Dual Role of Magnetic Ionic Liquids as Curing Agents of Epoxy Resin and Microwave-Absorbing Additives AITranslate

Universidade Federal do Rio de Janeiro; Universidade Federal do Rio de Janeiro; Universidade Federal do Rio de Janeiro; Universidade Federal do Rio de Janeiro; Universidade Federal do Rio de Janeiro; Universidade Federal do Rio de Janeiro
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The dual role of phosphonium- and imidazolium-based ionic liquids (ILs) combined with FeCl4 counteranions as hardeners for epoxy resin (ER) and additives for improving the microwave-absorbing properties was investigated. The influence of the chemical nature of the cation on the curing process of ER was evaluated by rheometric and differential scanning calorimetry (DSC) analysis. No significant curing process was observed for the ER-based systems until 7 days of storage at room temperature. DSC analysis under the dynamic mode was carried out at different heating rates to evaluate the best curing protocol and the kinetic parameters. Phosphonium-based ILs promoted faster curing rate and lower activation energy of the epoxy system, higher cross-link density observed by dynamic mechanical analysis, and better thermal stability. Moreover, ER cured with phosphonium ILs presented good microwave-absorbing properties, with minimum reflection loss values of −13.5 dB (at 9.5 GHz) and −11.5 dB (at 14.5 GHz), corresponding to more than 90% of electromagnetic attenuation. These results indicate that ER cured with these magnetic ILs can be used as promising microwave-absorbing materials in both X-band (8–12 GHz) and Ku-band (12–18 GHz).

KeyWords AITranslate

epoxy network magnetic ionic liquids kinetic parameters microwaveabsorbing materials thermal analysis dynamic mechanical Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01584

Chinese Library Classification Number:

Citation Information:

The dual role of phosphonium- and imidazolium-based ionic liquids (ILs) combined with FeCl4 counteranions as hardeners for epoxy resin (ER) and additives for improving the microwave-absorbing properties was investigated. The influence of the chemical nature of the cation on the curing process of ER was evaluated by rheometric and differential scanning calorimetry (DSC) analysis. No significant curing process was observed for the ER-based systems until 7 days of storage at room temperature. DSC analysis under the dynamic mode was carried out at different heating rates to evaluate the best curing protocol and the kinetic parameters. Phosphonium-based ILs promoted faster curing rate and lower activation energy of the epoxy system, higher cross-link density observed by dynamic mechanical analysis, and better thermal stability. Moreover, ER cured with phosphonium ILs presented good microwave-absorbing properties, with minimum reflection loss values of −13.5 dB (at 9.5 GHz) and −11.5 dB (at 14.5 GHz), corresponding to more than 90% of electromagnetic attenuation. These results indicate that ER cured with these magnetic ILs can be used as promising microwave-absorbing materials in both X-band (8–12 GHz) and Ku-band (12–18 GHz).

quote

GB/T 7714-2015 [1] Ruan R. Henriques, Caroline P. de Oliveira, Raiany Stein, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01584.
MLA [1] Ruan R. Henriques, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01584.
APA [1] Ruan R. Henriques, Caroline P. de Oliveira, Raiany Stein, Ketly Pontes, Adriana A. Silva, & Bluma G. Soares. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01584
IEEE [1] Ruan R. Henriques, Caroline P. de Oliveira, Raiany Stein, Ketly Pontes, Adriana A. Silva, and Bluma G. Soares, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01584. keywords: {epoxy network;magnetic ionic liquids;kinetic parameters;microwaveabsorbing materials;thermal analysis;dynamic mechanical;Show More}