Arylacetylene End-Capped Triarylamine-Based D–A System for Switching from Binary to Ternary Memory Behavior Arylacetylene End-Capped Triarylamine-Based D–A System for Switching from Binary to Ternary Memory Behavior AITranslate
Abstract AITranslate
Introducing a different acceptor into the same molecular backbone with a definite acceptor strength is the key to developing multilevel memory devices. A series of Y-shaped imidazole- and triarylamine-based compounds was designed and synthesized for multilevel data storage. The influence of various donor and acceptor end-cap units on the photophysical, electrochemical, and memory performance was evaluated. The electrochemical analysis reveals a high highest occupied molecular orbital (HOMO) level of around ∼5.0 eV and a low band gap with irreversible anodic peaks (1.05–1.08 V), which indicates facile charge transport in the donor/acceptor end-capped D–A systems. Switching the memory behavior from binary to ternary was achieved by tuning the acceptor strength in the molecular structure. The compounds with the terminal electron-withdrawing groups displayed a ternary memory with an ON/OFF ratio of 104 with a long-lasting retention time. tert-Butylphenyl and methoxyphenyl end-capped compounds demonstrated binary memory with a low threshold voltage (−1.42 and −1.38 V) and an ON/OFF ratio of 105. The molecular simulation confirms the charge transfer and trapping mechanism associated with the compound binary/ternary memory behavior. This work demonstrates that slight modification in the molecular structure can change the memory behavior from binary to ternary and renders a new pathway for updating the multilevel storage devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c01293
Chinese Library Classification Number:
Citation Information:
Introducing a different acceptor into the same molecular backbone with a definite acceptor strength is the key to developing multilevel memory devices. A series of Y-shaped imidazole- and triarylamine-based compounds was designed and synthesized for multilevel data storage. The influence of various donor and acceptor end-cap units on the photophysical, electrochemical, and memory performance was evaluated. The electrochemical analysis reveals a high highest occupied molecular orbital (HOMO) level of around ∼5.0 eV and a low band gap with irreversible anodic peaks (1.05–1.08 V), which indicates facile charge transport in the donor/acceptor end-capped D–A systems. Switching the memory behavior from binary to ternary was achieved by tuning the acceptor strength in the molecular structure. The compounds with the terminal electron-withdrawing groups displayed a ternary memory with an ON/OFF ratio of 104 with a long-lasting retention time. tert-Butylphenyl and methoxyphenyl end-capped compounds demonstrated binary memory with a low threshold voltage (−1.42 and −1.38 V) and an ON/OFF ratio of 105. The molecular simulation confirms the charge transfer and trapping mechanism associated with the compound binary/ternary memory behavior. This work demonstrates that slight modification in the molecular structure can change the memory behavior from binary to ternary and renders a new pathway for updating the multilevel storage devices.
quote
| GB/T 7714-2015 | [1] Deivendran Harshini, Varghese Maria Angela, Predhanekar Mohamed Imran, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01293. |
| MLA | [1] Deivendran Harshini, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01293. |
| APA | [1] Deivendran Harshini, Varghese Maria Angela, Predhanekar Mohamed Imran, & Samuthira Nagarajan. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01293 |
| IEEE | [1] Deivendran Harshini, Varghese Maria Angela, Predhanekar Mohamed Imran, and Samuthira Nagarajan, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01293. keywords: {imidazole triarylamine nonvolatile memory multilevel storage ternary memory} |