Redox-Responsive 2-Aminoanthraquinone Core–Shell Particles for Structural Colors and Carbon Capture AITranslate
Abstract AITranslate
Quinone-containing materials have attracted significant attention for energy storage and electroswing carbon capture. Tailored redox-responsive core–shell particles are obtained in the present work via semicontinuous starved-feed emulsion polymerization and subsequent postmodification strategies with redox-responsive quinone moieties. The use of glycidyl methacrylate within the shell material offers the possibility of a ring-opening reaction with the redox-responsive 2-aminoanthraquinone (2-AAQ), which possesses a high affinity toward electrophilic carbon dioxide. The successful preparation of monodisperse particles, an essential prerequisite for colloidal self-assembly, was investigated by dynamic light scattering and transmission electron microscopy. The presence of reactive epoxy functionalities was achieved by the ring-opening reaction with the Preussmann reagent. Postsynthesis modification was investigated using X-ray photoelectron spectroscopy and cyclic voltammetry measurements. The redox-responsive core–shell particles were subjected to the melt-shear organization technique to prepare free-standing opal films featuring structural colors. The monodisperse 2-AAQ-containing particles were investigated for self-assembly inside conductive carbon felts, and their electrochemically mediated carbon capture capabilities were studied.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00746
Chinese Library Classification Number:
Citation Information:
Quinone-containing materials have attracted significant attention for energy storage and electroswing carbon capture. Tailored redox-responsive core–shell particles are obtained in the present work via semicontinuous starved-feed emulsion polymerization and subsequent postmodification strategies with redox-responsive quinone moieties. The use of glycidyl methacrylate within the shell material offers the possibility of a ring-opening reaction with the redox-responsive 2-aminoanthraquinone (2-AAQ), which possesses a high affinity toward electrophilic carbon dioxide. The successful preparation of monodisperse particles, an essential prerequisite for colloidal self-assembly, was investigated by dynamic light scattering and transmission electron microscopy. The presence of reactive epoxy functionalities was achieved by the ring-opening reaction with the Preussmann reagent. Postsynthesis modification was investigated using X-ray photoelectron spectroscopy and cyclic voltammetry measurements. The redox-responsive core–shell particles were subjected to the melt-shear organization technique to prepare free-standing opal films featuring structural colors. The monodisperse 2-AAQ-containing particles were investigated for self-assembly inside conductive carbon felts, and their electrochemically mediated carbon capture capabilities were studied.
quote
| GB/T 7714-2015 | [1] Tamara Winter, Martin Bitsch, Frank Müller, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00746. |
| MLA | [1] Tamara Winter, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00746. |
| APA | [1] Tamara Winter, Martin Bitsch, Frank Müller, Sahag Voskian, T. Alan Hatton, Karin Jacobs, Volker Presser, & Markus Gallei. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00746 |
| IEEE | [1] Tamara Winter, Martin Bitsch, Frank Müller, Sahag Voskian, T. Alan Hatton, Karin Jacobs, Volker Presser, and Markus Gallei, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00746. keywords: {quinone containing core−shell particles;emulsion polymerization;polymer analogous reaction;redox responsiveness;Show More} |