daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Synthesis of a Multielement Flame Retardant and Its Application in Epoxy Resin AITranslate

Wuhan University of Technology; Wuhan University of Technology; Wuhan University of Technology; Wuhan University of Technology; Wuhan University of Technology; Wuhan University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

For the purpose of obtaining flame-retardant epoxy resin (FREP) with exceptional comprehensive properties, a multielement flame retardant SVPM was synthesized by sulfathiazole, 9, 10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide (DOPO), methylvinyldichlorosilane and vanillin. The effects of SVPM on the thermal stability, heat resistance, mechanical behavior and flame retardancy of epoxy resin (EP) were systematically revealed, and the flame-retardant mechanism of SVPM was deeply explored. In the presence of only 0.12 wt% phosphorus content in the system, FREP achieved V-0 rating of vertical combustion (UL-94) and the limiting oxygen index (LOI) value reached 31.1%. Additionally, SVPM reduced the smoke and heat release of EP. The mechanical properties of EP were enhanced by SVPM; specifically, the maximum increment of tensile strength and flexural strength of FREP were 26.23% and 16.67% respectively. The investigation of flame-retardant mechanism showed that the phosphorus-containing free radicals and SO2 decomposed by SVPM can quench the active free radicals in the combustion process, thus interrupting the chain reaction of combustion, and the noncombustible gas generated by SVPM during combustion can reduce the concentration of combustible volatiles. In the condensation phase, phosphoric acid and silicon dioxide produced by SVPM degradation can promote the stability and densification of the char layer, eventually effectively reducing the combustion intensity.

KeyWords AITranslate

Epoxy resin High efficiency Flame retardant Heat resistance Mechanical properties
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01875

Chinese Library Classification Number:

Citation Information:

For the purpose of obtaining flame-retardant epoxy resin (FREP) with exceptional comprehensive properties, a multielement flame retardant SVPM was synthesized by sulfathiazole, 9, 10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide (DOPO), methylvinyldichlorosilane and vanillin. The effects of SVPM on the thermal stability, heat resistance, mechanical behavior and flame retardancy of epoxy resin (EP) were systematically revealed, and the flame-retardant mechanism of SVPM was deeply explored. In the presence of only 0.12 wt% phosphorus content in the system, FREP achieved V-0 rating of vertical combustion (UL-94) and the limiting oxygen index (LOI) value reached 31.1%. Additionally, SVPM reduced the smoke and heat release of EP. The mechanical properties of EP were enhanced by SVPM; specifically, the maximum increment of tensile strength and flexural strength of FREP were 26.23% and 16.67% respectively. The investigation of flame-retardant mechanism showed that the phosphorus-containing free radicals and SO2 decomposed by SVPM can quench the active free radicals in the combustion process, thus interrupting the chain reaction of combustion, and the noncombustible gas generated by SVPM during combustion can reduce the concentration of combustible volatiles. In the condensation phase, phosphoric acid and silicon dioxide produced by SVPM degradation can promote the stability and densification of the char layer, eventually effectively reducing the combustion intensity.

quote

GB/T 7714-2015 [1] Chao Wan, Huajun Duan, Chenhao Zhang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01875.
MLA [1] Chao Wan, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01875.
APA [1] Chao Wan, Huajun Duan, Chenhao Zhang, Chentao Liu, Huijuan Zhao, & Huiru Ma. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01875
IEEE [1] Chao Wan, Huajun Duan, Chenhao Zhang, Chentao Liu, Huijuan Zhao, and Huiru Ma, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01875. keywords: {Epoxy resin;High efficiency;Flame retardant;Heat resistance;Mechanical properties}