Thermodynamic Study on Vanadium Precipitation with Calcium Salt AITranslate

School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

According to the principle of simultaneous equilibrium and the law of mass conservation, thermodynamic equilibrium diagrams of Ca-V(V )-H2O system were established with different concentrations of total free calcium at 25 ℃, and then thermodynamic analysis was made of the system. The results show that the six stable solid regions of V2O5 ,Ca(VO3)2, Ca2V207 ,Ca3 (VO4)2 ,CaB (VO4)2 +Ca(OH)2 and Ca(OH)2 appear in turn with increase of the system pH value. When total free calcium concentration is 0.01 mol/L in the equilibrium system,at the pH region of 5.1-9.8,vanadium is precipitated in the form of Ca(VO3)2 and vanadium concentration can be reduced to 2.2× 10^-3 mol/L. At pH region of 9.8-10.3, Ca2 V2 O7 is formed and corresponding vanadium concentration can be decreased to 1.2 × 10 ^-2 mol/L. At the pH region of 10.3-12.6 ,Ca3 (VO4)2 is precipitated and the minimum vanadium concentration can reach to 2.4 × 10^-4 mol/L, which is the best vanadium precipitation effect. When total free calcium concentration is 0.01-1.0 mol/L,theoretical optimum pH value for vanadium precipitation is kept at about 11.0-12.6.

KeyWords AITranslate

vanadium precipitation with calcium salt Ca-V( V )-H2O system thermodynamic equilibrium diagram stable solid region

1漆明鉴.从石煤中提钒现状及前景[J].湿法冶金,1999,18(4):1-10. 被引量:128

2陈庆根.石煤钒矿提钒工艺技术的研究进展[J].矿产综合利用,2009(2):30-34. 被引量:35

3宁顺明,马荣骏.我国石煤提钒的技术开发及努力方向[J].矿冶工程,2012,32(5):57-61. 被引量:25

4丁瑞锋,刘桂华.溶液中钒分离富集技术的研究进展[J].湖南有色金属,2011,27(3):15-19. 被引量:8

5谢培川,秦念华,张灌鲁.用钙盐沉淀法从钠化钒渣中提钒收钠[J].钢铁钒钛,1986,(2):44-49.

6Zhao Zhuo, Long Hongming, Li Xiaobin,et al. Precipita- tion of vanadium from Bayer liquor with lime[J]. Hy- drometallurgy, 2012,115-116 .. 52-56.

7白万全,杨巧芳,尹中林.一种拜耳法种分母液回收五氧化二钒的方法[P].中国专利:200610109366.8,2007-01-03.

8赵东峰,田侣,丁瑞锋,刘桂华,周秋生,李小斌,彭志宏.铬酸钠碱性液中加石灰除钒[J].中国有色金属学报,2011,21(12):3162-3168. 被引量:11

9孙健程,冯其明,陈云.碱性体系中铝-钒-钼分离技术研究[J].稀有金属与硬质合金,2008,36(3):19-23. 被引量:6

10James G Speight. Lange's handbook of chemistry (16th edition) [M]. NewYork: McGraw-Hill, 2005.

1朱茂兰,黄中省,衷水平,陈杭,胡志彪.镓精矿中镓的提取工艺[J].中国有色金属学报,2018,28(11):2351-2357. 被引量:2

2包申旭,陈波,张一敏.我国钒页岩提钒技术研究现状及前景[J].金属矿山,2020(10):20-33. 被引量:8

3关月明,张成,袁胜华,刘美,丁巍.结晶沉淀法回收废催化剂碱浸液中的钼和钒[J].稀有金属与硬质合金,2021,49(6):9-14.

1潘岩,鄢锋,郭徽,唐昭辉,杨静雅,曾祥吉.有色金属冶炼自动控制研究现状与展望[J].中国有色金属学报,2021,31(1):96-105. 被引量:2

2赖永传,杨鑫龙,孙建之,尚鹤,高文成,温建康.含钒页岩酸浸液中钒的选择性萃取研究现状[J].稀有金属,2022,46(1):109-119. 被引量:3

3阳建国,韩康,李恒,陈勇.陕西某钒矿石预富集工艺研究[J].现代矿业,2022,38(4):128-130.

4张一敏,薛楠楠,刘涛,黄晶.钒页岩全湿法绿色提取技术[J].中国矿业大学学报,2022,51(3):520-531. 被引量:1

5密静强,陈远荣,于浩,张宏,凌尔仲,王延俊,杜佳云,邓明华.广西平果沉积型铝土矿Ga的分布特征与沉积环境关联性探讨[J].地质力学学报,2022,28(3):417-431.

6张占兵,胡佩伟,谢志诚,胡超.分散剂强化细粒级含钒页岩的钒浸出及作用机理[J].中国有色金属学报,2022,32(9):2753-2763. 被引量:2

7杨小慧,李望,朱晓波.D751螯合树脂吸附酸性溶液中钒(Ⅳ)离子的机制[J].中国有色金属学报,2022,32(12):3862-3870.

8赖永传,杨鑫龙,孙建之,尚鹤,莫晓兰,温建康.石煤含氟酸浸液中V(Ⅴ)-Fe(Ⅲ)-F-H_(2)O系钒铁分离热力学研究[J].中南大学学报:自然科学版,2023,54(5):1703-1712.

9张云,叶国华,梁雪崟,项新月,荣一阳,宋昌溆.页岩钒矿直接酸浸提钒的强化与活化研究进展[J].钢铁钒钛,2023,44(2):1-8.

10王淼,温建康,李文娟,杨鑫龙,赖永传,杨洪英.选冶联合回收石煤中伴生战略金属钒镍钼的研究进展[J].稀有金属,2023,47(6):881-892.

1杨亮,赵中伟,何利华,霍广生,陈爱良.钼酸铵溶液镁盐沉淀法除砷的热力学分析[J].中南大学学报:自然科学版,2012,43(5):1610-1615. 被引量:7

2吴永谦,吴贤,孟晗琪,陈昆昆.从含高钼的钨溶液中回收钨钼的研究[J].稀有金属与硬质合金,2016,44(5):1-5. 被引量:1

3杨树峰,李京社,张立峰,唐海燕,高锦国,姜桂连.不同脱氧剂对气瓶钢洁净度的影响[J].钢铁钒钛,2009,30(3):61-64. 被引量:2

4张刚,赵中伟,曹才放,黄少波.磷酸盐分解钼酸钙的热力学[J].北京科技大学学报,2009,31(11):1394-1399. 被引量:5

5李昆,宋文臣,郑权,李宏.熔融态钒渣氧化钙化后酸浸研究[J].钢铁钒钛,2013,34(5):15-18. 被引量:6

6刘永康,王淀佐,罗文平,何伯泉.添加剂对高铁赤泥煤基直接还原的催化作用[J].湖南冶金,1995,23(6):5-7. 被引量:1

7吴玉霜.硬质合金中镍和钴的连续测定[J].稀有金属与硬质合金,1996,24(2):40-43.

8一种从石煤钒矿中提钒的焙烧工艺[J].钢铁钒钛,2009,30(1):76-77.

9江秋月.高铅硅锌渣绿色回收锗铟的新工艺研究[J].有色金属:冶炼部分,2014(4):51-53. 被引量:13

10梁伦龙.钢渣中游离氧化钙快速测定方法研究[J].涟钢科技与管理,2000(6):6-7.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]

Citation Information:

According to the principle of simultaneous equilibrium and the law of mass conservation, thermodynamic equilibrium diagrams of Ca-V(V )-H2O system were established with different concentrations of total free calcium at 25 ℃, and then thermodynamic analysis was made of the system. The results show that the six stable solid regions of V2O5 ,Ca(VO3)2, Ca2V207 ,Ca3 (VO4)2 ,CaB (VO4)2 +Ca(OH)2 and Ca(OH)2 appear in turn with increase of the system pH value. When total free calcium concentration is 0.01 mol/L in the equilibrium system,at the pH region of 5.1-9.8,vanadium is precipitated in the form of Ca(VO3)2 and vanadium concentration can be reduced to 2.2× 10^-3 mol/L. At pH region of 9.8-10.3, Ca2 V2 O7 is formed and corresponding vanadium concentration can be decreased to 1.2 × 10 ^-2 mol/L. At the pH region of 10.3-12.6 ,Ca3 (VO4)2 is precipitated and the minimum vanadium concentration can reach to 2.4 × 10^-4 mol/L, which is the best vanadium precipitation effect. When total free calcium concentration is 0.01-1.0 mol/L,theoretical optimum pH value for vanadium precipitation is kept at about 11.0-12.6.

quote

GB/T 7714-2015 [1] LI He, LIU Xu-heng, HE Li-hua. Thermodynamic Study on Vanadium Precipitation with Calcium Salt[J]. Rare Metals and Cemented Carbides, 2014(1): 15-19.
MLA [1] LI He, et al., "Thermodynamic Study on Vanadium Precipitation with Calcium Salt." Rare Metals and Cemented Carbides, no. 1, 2014, pp. 15-19.
APA [1] LI He, LIU Xu-heng, & HE Li-hua. (2014). Thermodynamic Study on Vanadium Precipitation with Calcium Salt. Rare Metals and Cemented Carbides(1), 15-19.
IEEE [1] LI He, LIU Xu-heng, and HE Li-hua, "Thermodynamic Study on Vanadium Precipitation with Calcium Salt," Rare Metals and Cemented Carbides, no. 1, pp. 15-19, 2014. keywords: {vanadium precipitation with calcium salt;Ca-V( V )-H2O system;thermodynamic equilibrium diagram;stable solid region}