Lightweight and High Mechanical Strength Silver Nanowire/Hydroxypropyl Methylcellulose Electromagnetic Interference Shielding Composite AITranslate
Abstract AITranslate
Harmful electromagnetic radiation has become a serious problem. High-performance electromagnetic shielding materials play a vital role in controlling or reducing electromagnetic radiation conduction. The high density and poor environmental stability of common metal-based electromagnetic shielding materials severely limit their further development. Ag nanowire (NW) aerogels are feasible lightweight and high-performance electromagnetic shielding materials. Here, we report a hydroxypropyl methylcellulose (HPMC) and Ag NWs composite aerogel that has low density (<77 mg cm–3), high porosity (>95.09%), excellent mechanical properties (tensile strength of 0.27 MPa and compressive stress of 1.3 MPa), and electromagnetic shielding performance of above 89 dB.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00823
Chinese Library Classification Number:
Citation Information:
Harmful electromagnetic radiation has become a serious problem. High-performance electromagnetic shielding materials play a vital role in controlling or reducing electromagnetic radiation conduction. The high density and poor environmental stability of common metal-based electromagnetic shielding materials severely limit their further development. Ag nanowire (NW) aerogels are feasible lightweight and high-performance electromagnetic shielding materials. Here, we report a hydroxypropyl methylcellulose (HPMC) and Ag NWs composite aerogel that has low density (<77 mg cm–3), high porosity (>95.09%), excellent mechanical properties (tensile strength of 0.27 MPa and compressive stress of 1.3 MPa), and electromagnetic shielding performance of above 89 dB.
quote
| GB/T 7714-2015 | [1] Yong Zhu, Wei Wei, Ruoyi Zhao, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00823. |
| MLA | [1] Yong Zhu, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00823. |
| APA | [1] Yong Zhu, Wei Wei, Ruoyi Zhao, Zhang Chen, Liying Zhang, Xiaojun Zeng, & Yanfeng Gao. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00823 |