Synthesis and Luminescent Properties of CaTiO3Pr3+ AITranslate

Department of Chemistry, Hunan Normal University;Department of Chemistry, Hunan Normal University;Department of Chemistry, Hunan Normal University;Department of Chemistry, Hunan Normal University;Department of Chemistry, Hunan Normal University;Department of Chemistry, Hunan Normal University;Department of Chemistry, Hunan Normal University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The method of synthesising CaTiO3 doped with rare earth ions Pr3+ was reported in this paper. The emission peaking at 613nm is corresponding to the spectral tranision1D23H4 of Pr3+ inos. The dependence of luminescent properties of CaTiO3Pr3+ on different synthesis condition was investigated.

KeyWords AITranslate

CaTiO3Pr3+ synthesis luminescence

1刘应亮.发光学研究及应用[M].合肥:中国科技大学出版社,1992.179.

1夏威,熊楚耀,肖志国,雷明凯.新型蓄光发光材料产业化现状及趋势[J].新材料产业,2006(7):31-34.

2贺干武,刘应亮,雷炳富.钙钛矿CaSnO_3∶Pr^(3+)磷光体的发光特性[J].发光学报,2007,28(3):389-392. 被引量:8

3王荣,孟建新.水热法制备长余辉发光材料CaTiO_3:Pr,Al及其发光性能[J].中国稀土学报,2009,27(3):349-352. 被引量:4

4张秀梅,牟艳男,宋文绪,杨海滨.稀土Pr掺杂纳米发光材料Sr_(0.2)Ca_(0.8)TiO_3的结构及光学性质[J].物理实验,2010,30(7):9-12.

5刘雪飞,肖林久,贺明睿,谢颖,陈永杰,李文泽,于维珂.Sol-gel法制备CaSnO3∶Eu3+发光粉过程中添加PEG的作用[J].发光学报,2010,31(4):484-488. 被引量:2

6王晓楠,左斌.纳米粉末Zn_(0.2)Ca_(0.8)TiO_3:Pr的合成与表征[J].吉林化工学院学报,2011,28(1):19-22. 被引量:2

7邱敏,牟艳男,张秀平,刘立.纳米粉末Ba_(0.2)Ca_(0.8)TiO_3∶Pr的合成及XRD研究[J].大学物理实验,2013,26(2):1-3. 被引量:1

8樊国栋,王钰,杨溦.Pr^(3+)掺杂SrWO_4荧光材料的制备与发光性能的研究[J].现代化工,2015,35(4):104-107. 被引量:1

1刘雪飞,肖林久,贺明睿,谢颖,陈永杰,李文泽,于维珂.Sol-gel法制备CaSnO3∶Eu3+发光粉过程中添加PEG的作用[J].发光学报,2010,31(4):484-488. 被引量:2

2杨英,陈永杰,李郎楷,耿秀娟.橙红色荧光粉Mg_(2-x)SnO_4∶Eu_x^(3+)发光性能的研究[J].沈阳化工大学学报,2011,25(1):12-14.

3郭宇,刘玉学,闫小磊,严端廷,刘春光,赵立竹,徐长山.双波长Pr^(3+)掺杂12CaO·7Al_2O_3的光存储特性[J].发光学报,2011,32(4):313-318. 被引量:4

4付作岭,付喜宏,孙桂娟.白光LED用红色荧光粉CaSnO_3∶Eu^(3+)的制备及光学性质[J].发光学报,2011,32(7):660-664. 被引量:5

5赖昌,王广川.YAlO_3晶体中Pr^(3+)的4f^2能级[J].发光学报,2011,32(9):885-889. 被引量:3

6琚建勇,孙鸣翔,时炜,沈雷军,李波.稀土长余辉发光材料在消防标志中的应用进展[J].稀土,2011,32(6):89-93. 被引量:1

7王晓楠,左斌.稀土发光材料Mg_(0.2)Ca_(0.8)TiO_3:Pr的合成与表征[J].吉林化工学院学报,2012,29(1):9-12.

8曹仕秀,魏宁,杨小琴.化学共沉淀法制备Ca_2MgSi_2O_7:Eu^(2+)荧光粉[J].重庆文理学院学报:自然科学版,2012,31(5):17-19.

9史强,杨冰,李丽华,孙桂芳.德拜相法测晶格常数实验数据处理方法分析[J].大学物理实验,2014,27(1):99-100.

10张霞,陶军,于方丽.水热法制备CaTiO_3∶Pr^(3+)微纳米荧光粉及其发光性能[J].人工晶体学报,2014,43(2):350-354. 被引量:10

1陈芮,魏琼,塔娜,张博,陈栋华.超声分散辅助合成CaTiO_3∶Pr^(3+)红色长余辉材料及其发光性能[J].中南民族大学学报:自然科学版,2008,27(3):25-28. 被引量:3

2杨伟,张君诚,王旭升,姚熹.B位Zr^(3+)掺杂CaTiO_3∶Pr^(3+)红色发光材料的发光性能研究[J].材料导报,2010,24(4):11-13. 被引量:1

3杨志平,郭智,王文杰,朱胜超.Pr^(3+)摩尔浓度对CaTiO_3:Pr^(3+)红色长余辉材料的影响[J].功能材料与器件学报,2003,9(4):473-476. 被引量:16

4杨志平,王文杰,郭智,朱胜超.红色长余辉材料CaTiO_3:Pr^(3+)中两种电子陷阱的研究[J].光电子.激光,2004,15(3):332-336. 被引量:15

5姚连增,程庭柱,阮耀钟,张裕恒.Pr^(3+)离子及Na_5Pr(WO_4)_4晶体的光谱性质[J].中国激光,1992,19(6):451-454. 被引量:1

6谢英娜,安胜利,袁春华.La^(3+)-Pr^(3+)共掺杂纳米TiO_2粉体的光催化性能[J].复合材料学报,2012,29(6):97-101. 被引量:9

7陈栋华,李秋霞,黄佳平.一种新型的蓝光激发白光LED用荧光粉Ba_(0.5)Sr_(0.5)MoO_4∶_(0.02)Pr^(3+)[J].中南民族大学学报:自然科学版,2010,29(3):14-17. 被引量:11

8李云白,王虹,徐征,张光寅,陈晓波.温度对稀土离子掺杂ZBLAN玻璃上转换发光的影响[J].发光学报,1997,18(4):304-306. 被引量:3

9黄国华,谢清连,徐建梅,周东祥.Nd^(3+)、Li^(1+)对CaTiO_3微波介电性能的影响[J].压电与声光,2006,28(2):185-187. 被引量:5

10周德,袁颖.CaTiO_3含量对PTFE/TiO_2复合材料性能的影响[J].电子元件与材料,2012,31(12):18-21. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TN383.04[电子电信—物理电子学];TB39[一般工业技术—材料科学与工程]

Citation Information:

The method of synthesising CaTiO3 doped with rare earth ions Pr3+ was reported in this paper. The emission peaking at 613nm is corresponding to the spectral tranision1D23H4 of Pr3+ inos. The dependence of luminescent properties of CaTiO3Pr3+ on different synthesis condition was investigated.

quote

GB/T 7714-2015 [1] ZHANG Hua-jing, LIAN Shi-xun, WU Zhen-guo, et al. Synthesis and Luminescent Properties of CaTiO3Pr3+[J]. Rare Metals and Cemented Carbides, 1999(2): 38-39.
MLA [1] ZHANG Hua-jing, et al., "Synthesis and Luminescent Properties of CaTiO3Pr3+." Rare Metals and Cemented Carbides, no. 2, 1999, pp. 38-39.
APA [1] ZHANG Hua-jing, LIAN Shi-xun, WU Zhen-guo, LI Cheng-zhi, MAO Xiang-hui, MA Ming, & LIU Lian-ying. (1999). Synthesis and Luminescent Properties of CaTiO3Pr3+. Rare Metals and Cemented Carbides(2), 38-39.
IEEE [1] ZHANG Hua-jing, LIAN Shi-xun, WU Zhen-guo, LI Cheng-zhi, MAO Xiang-hui, MA Ming, and LIU Lian-ying, "Synthesis and Luminescent Properties of CaTiO3Pr3+," Rare Metals and Cemented Carbides, no. 2, pp. 38-39, 1999. keywords: {CaTiO3Pr3+;synthesis;luminescence}