Preparation and Properties of YPO_4:Tb3+ Fluorescent Material with Polyacrylamide Gel Method AITranslate

School of Chemistry and Materials Science, Guizhou Normal University;School of Chemistry and Materials Science, Guizhou Normal University;School of Chemistry and Materials Science, Guizhou Normal University;School of Chemistry and Materials Science, Guizhou Normal University;School of Chemistry and Materials Science, Guizhou Normal University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Tb3+ doped YPO4 samples were successfully synthesized with a polyacrylamide gel method. The crystal structure, particle size,morphology and luminescence properties of the as-synthesized samples were investigated by XRD,TEM and PL. The effects of Tb3+ doping concentration,the precursor solution pH and the molar ratio between RE (RE=Y and Tb) and P on the phase structure and luminescence properties of the products were investigated. The results show that the single-phase tetragonal YPO4 : Tb3+ crystal with particle size of about 6- 10 nm can be obtained with polyacrylamide gel method. The photoluminescence spectra of Tb3+ doped YPO4 samples show a characteristic green luminescence of Th3+ under 222 nm UV light excitation. Furthermore,the concentration quenching is observed when the Tb3+ doping concentration is over 60% ,indicating that the n(Y+Tb)/n(P) has a significant influence on the phase structure and luminescence properties of the samples, while precursor solution pH only affects their luminescence properties. Under the conditions of n(Y+Tb)/n(P)=l : 1 and pH=6,the products of high luminescence intensity can be obtained.

KeyWords AITranslate

YPO4 Tb3+ doping polyacrylamide gel method luminescence property

1Rodriguez-Liviano S,Aparicio F J,Rojas T C,et al. Mi- crowave- assisted synthesis and luminescence of meso- porous RE-doped YPO4 (RE= Eu,Ce,Tb,and Ce+Tb) nanophosphors with lenticular shape[J]. Crystal Growth and Design,2012,12(2) :635-645.

2Li Chunxia, Hou Zhiyao, Zhang Cuimiao, et al. Con- trolled synthesis of Ln^3+ (Ln=Tb,Eu,Dy) and V^5+ ion -doped YPO4 nano-/microstructures with tunable lumi nescent colors [J]. Chemistry of Materials, 2009, 21 (19):4 598-4 607.

3Balakrishnaiah R, Kim D W, Yi S S, et al. NIR to VIS frequency upconversion luminescence properties of Er^3+- doped YPO4 phosphors[J]. Thin Solid Films, 2010,518 (22):6 145-6 148.

4He Y,Zhao M,Song Y,et al. Effects of excitation wave- length and Y^3+ content on luminescent properties of YMO4 : Dy^3+ (M=V,P) phosphors induced by ultravi- olet excitation[J]. Materials Research Bulletin, 2012,47 (7):1 821-1 826.

5Li G, Liu S,Chu Z, et al. Synthesis and photolumines- cence of core-shell structured spherical SiO2 @YPO4:Tb^3+ phosphors via sol-gel process[J]. Journal of Lumi- nescence,2012,132(11) :2 961-2 967.

6Guan H, Lv C, Han C, et al. Luminescent and magnetism properties of YPO4 : Eu^3+ octahedron microcrystals[J]. Materials Letters, 2012,81 : 92-94.

7P. Psuja,W. Strek.Influence of concentration and sintering temperature on luminescence properties of Eu^(3+):SnO_2 nanocrystallites[J].稀土学报:英文版,2012,30(7):627-631. 被引量:6

8Hassanzadeh-Tabrizi S A. Polymer-assisted synthesis and luminescence properties of MgAl2O4 : Tb nanop owder[J]. Optical Materials,2011,33(11):1 607-1 609.

9Lide D R. CRC handbook of chemistry and physics (87th edition) [M]. Boca Raton : Taylor and Francis, 2007.

10Nedelec J M, Avignant D, Mahiou R. Soft chemistry routes to YPO4-based phosphors: Dependence of tex- tural and optical properties on synthesis pathways[J]. Chemistry of Materials, 2002,14(2) :651-655.

1覃利琴,陶萍芳,王荣芳,陆发权.Tb^(3+)掺杂稀土YPO_4的溶剂热合成及其荧光性能[J].玉林师范学院学报,2015,36(2):45-50. 被引量:1

2郑义,付兵.Sr^(2+)共掺杂LaPO_(4):Tb^(3+)发光材料的水热合成与性能[J].山东化工,2023,52(10):50-53.

1肖勇强,陈鹏,朱月华,张娜,卓宁泽.UVC荧光粉YPO4:Bi^3+的制备及发光性能表征[J].中国稀土学报,2020,38(6):724-729. 被引量:1

1莎仁,高娃,德格吉呼,王喜贵.CeF_3:Tb^(3+)纳米棒的制备与发光性能[J].分子科学学报,2013,29(5):358-362.

2陈星星,杜景红,甘国友,严继康,易健宏.高分子网络凝胶法制备Fe掺杂TiO_2粉体的研究[J].功能材料,2013,44(20):2999-3002. 被引量:1

3杨锦瑜,罗林,苏玉长,申婧.高分子凝胶法合成YPO4:Sm^(3+)纳米荧光材料的结构与光学性能[J].粉末冶金材料科学与工程,2014,19(3):493-498. 被引量:6

4滕冰,钟德高,李煜燚,于萌华,景贺琳,张世明,杨利廷.Yb:YPO_4晶体的生长及光谱表征[J].青岛大学学报:自然科学版,2015,28(1):1-2.

5陈雪冰,邵忠宝,杨雪.高分子网络凝胶法制备纳米α-Fe_2O_3粉体[J].化学与生物工程,2005,22(12):34-36.

6陈雪冰,邵忠宝,田彦文,杨雪.纳米复合材料TiO_2/ZnFe_2O_4的制备及光催化性能[J].材料研究学报,2008,22(4):353-356. 被引量:2

7李世龙,吕超,闵鑫,房明浩,黄朝晖,刘艳改.La_7O_6(BO_3)(PO_4)_2∶Eu^(3+)/Tb^(3+)荧光材料的制备及其光致发光性能[J].无机化学学报,2017,33(5):761-768. 被引量:5

8莎仁,杨明学.Tb^(3+)掺杂ZnWO_4基绿色荧光粉的发光性能[J].稀有金属,2015,39(2):130-135. 被引量:1

9卢旭东,姜承志,邵忠财.高分子凝胶网络法制备La_(0.65)Sr_(0.35)MnO_3及光催化性能[J].有色矿冶,2006,22(6):41-42. 被引量:4

10李晶晶,王喜贵.Tb^(3+)掺杂ZnO-3SiO_2发光材料的制备与发光性质[J].液晶与显示,2013,28(6):817-822. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:O614.33[理学—无机化学]

Citation Information:

Tb3+ doped YPO4 samples were successfully synthesized with a polyacrylamide gel method. The crystal structure, particle size,morphology and luminescence properties of the as-synthesized samples were investigated by XRD,TEM and PL. The effects of Tb3+ doping concentration,the precursor solution pH and the molar ratio between RE (RE=Y and Tb) and P on the phase structure and luminescence properties of the products were investigated. The results show that the single-phase tetragonal YPO4 : Tb3+ crystal with particle size of about 6- 10 nm can be obtained with polyacrylamide gel method. The photoluminescence spectra of Tb3+ doped YPO4 samples show a characteristic green luminescence of Th3+ under 222 nm UV light excitation. Furthermore,the concentration quenching is observed when the Tb3+ doping concentration is over 60% ,indicating that the n(Y+Tb)/n(P) has a significant influence on the phase structure and luminescence properties of the samples, while precursor solution pH only affects their luminescence properties. Under the conditions of n(Y+Tb)/n(P)=l : 1 and pH=6,the products of high luminescence intensity can be obtained.

quote

GB/T 7714-2015 [1] LUO Lin, CENG Xiao-dao, JIA Xiao-hui, et al. Preparation and Properties of YPO_4:Tb3+ Fluorescent Material with Polyacrylamide Gel Method[J]. Rare Metals and Cemented Carbides, 2014(5): 14-19.
MLA [1] LUO Lin, et al., "Preparation and Properties of YPO_4:Tb3+ Fluorescent Material with Polyacrylamide Gel Method." Rare Metals and Cemented Carbides, no. 5, 2014, pp. 14-19.
APA [1] LUO Lin, CENG Xiao-dao, JIA Xiao-hui, ZHU Li-ping, & YANG Jin-yu. (2014). Preparation and Properties of YPO_4:Tb3+ Fluorescent Material with Polyacrylamide Gel Method. Rare Metals and Cemented Carbides(5), 14-19.
IEEE [1] LUO Lin, CENG Xiao-dao, JIA Xiao-hui, ZHU Li-ping, and YANG Jin-yu, "Preparation and Properties of YPO_4:Tb3+ Fluorescent Material with Polyacrylamide Gel Method," Rare Metals and Cemented Carbides, no. 5, pp. 14-19, 2014. keywords: {YPO4;Tb3+ doping;polyacrylamide gel method;luminescence property}