Power-Level Electrical Switch Enabled by a Liquid-Metal Bridge Power-Level Electrical Switch Enabled by a Liquid-Metal Bridge AITranslate

Xi’an Jiaotong University; Xi’an Jiaotong University; Xi’an Jiaotong University; Xi’an Jiaotong University; Xi’an Jiaotong University; University of Birmingham; Xi’an Jiaotong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Soft electronic components possess the potential to be developed into next-generation electrical devices that can provide superior performance to solid-state counterparts. Among commonly used components, electrical switches are an essential control element in electrical and electronic systems. Both solid-state mechanical and semiconductor switches are blamed for some intrinsic shortcomings. For example, the former suffers from contact surface degradation, while the latter functions with a high conduction loss. To overcome the limitations, here, a liquid metal (LM)-enabled electrical switch is reported by incorporating a Galinstan liquid bridge into a pair of solid electrodes. The electrical switch operation is realized by the coalescence of LM droplets and the breakup of the LM bridge. Extraordinarily, the device is capable of interrupting a DC 220 V, 1–5 A circuit within 11 ms, outperforming a common mechanical switch by a factor of 4–20 in terms of interruption speed. During the breakup process of an LM bridge in the presence of a current, three regimes characterized by electrical arc behaviors are identified and investigated. The rupture distance formed before pinch-off is critical to regulate the arc plasma behaviors. The presented applications and discoveries have a vast potential in both practical technologies, involving high-current electrical and electronic equipment, and fundamental research fields relevant to soft electronics, fluid mechanics, and plasma science.

KeyWords AITranslate

liquid metal Galinstan liquid bridge electrical switch soft electrical components
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00352

Chinese Library Classification Number:

Citation Information:

Soft electronic components possess the potential to be developed into next-generation electrical devices that can provide superior performance to solid-state counterparts. Among commonly used components, electrical switches are an essential control element in electrical and electronic systems. Both solid-state mechanical and semiconductor switches are blamed for some intrinsic shortcomings. For example, the former suffers from contact surface degradation, while the latter functions with a high conduction loss. To overcome the limitations, here, a liquid metal (LM)-enabled electrical switch is reported by incorporating a Galinstan liquid bridge into a pair of solid electrodes. The electrical switch operation is realized by the coalescence of LM droplets and the breakup of the LM bridge. Extraordinarily, the device is capable of interrupting a DC 220 V, 1–5 A circuit within 11 ms, outperforming a common mechanical switch by a factor of 4–20 in terms of interruption speed. During the breakup process of an LM bridge in the presence of a current, three regimes characterized by electrical arc behaviors are identified and investigated. The rupture distance formed before pinch-off is critical to regulate the arc plasma behaviors. The presented applications and discoveries have a vast potential in both practical technologies, involving high-current electrical and electronic equipment, and fundamental research fields relevant to soft electronics, fluid mechanics, and plasma science.

quote

GB/T 7714-2015 [1] Xiaonan Zhu, Fei Yang, Haoran Wang, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00352.
MLA [1] Xiaonan Zhu, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00352.
APA [1] Xiaonan Zhu, Fei Yang, Haoran Wang, Siyuan Zhao, Yi Wu, ShiYang Tang, & Mingzhe Rong. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00352
IEEE [1] Xiaonan Zhu, Fei Yang, Haoran Wang, Siyuan Zhao, Yi Wu, ShiYang Tang, and Mingzhe Rong, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00352. keywords: {liquid metal Galinstan liquid bridge electrical switch soft electrical components}