daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

All-Aqueous Direct Deposition of Fragrance-Loaded Nanoparticles onto Fabric Surfaces by Electrospraying AITranslate

Zhejiang University; Zhejiang University; Zhejiang University; Zhejiang University; Zhejiang University; Zhejiang University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Encapsulation of bioactive aroma compounds into nanostructured matrixes has emerged as an attractive means to prolong the longevity of perfumery products. Existing technologies applied for fragrance micro/nanoencapsulation primarily rely on wet chemical processes, which suffer from some drawbacks such as the tedious preparation involving emulsion formulations and possible contamination of residual additives. Herein, we proposed an all-aqueous electrospraying method to prepare composite nanoparticles made up of fragrance/2-hydroxypropyl-β-cyclodextrin complexes and regenerated silk fibroin with a greater than 90% aroma-encapsulation efficiency within the matrixes. Compared to fragrance/CD inclusion complexes, the as-prepared silk nanocomposites are capable of more effectively preserving the volatile cargo and exhibited an ideal zero-order release kinetics with slow release rate upon the treatment of alcohol. Furthermore, a great benefit of this approach is that it allows the direct deposition of fragrance-carrying nanoparticles on the silk fabrics during the electrospraying fabrication.

KeyWords AITranslate

fragrance silk fibroin nanoencapsulation electrospray sustained release fabric
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00457

Chinese Library Classification Number:

Citation Information:

Encapsulation of bioactive aroma compounds into nanostructured matrixes has emerged as an attractive means to prolong the longevity of perfumery products. Existing technologies applied for fragrance micro/nanoencapsulation primarily rely on wet chemical processes, which suffer from some drawbacks such as the tedious preparation involving emulsion formulations and possible contamination of residual additives. Herein, we proposed an all-aqueous electrospraying method to prepare composite nanoparticles made up of fragrance/2-hydroxypropyl-β-cyclodextrin complexes and regenerated silk fibroin with a greater than 90% aroma-encapsulation efficiency within the matrixes. Compared to fragrance/CD inclusion complexes, the as-prepared silk nanocomposites are capable of more effectively preserving the volatile cargo and exhibited an ideal zero-order release kinetics with slow release rate upon the treatment of alcohol. Furthermore, a great benefit of this approach is that it allows the direct deposition of fragrance-carrying nanoparticles on the silk fabrics during the electrospraying fabrication.

quote

GB/T 7714-2015 [1] Long Ye, Zixie Li, Rui Niu, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00457.
MLA [1] Long Ye, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00457.
APA [1] Long Ye, Zixie Li, Rui Niu, Zhuxian Zhou, Youqing Shen, & Liming Jiang. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00457
IEEE [1] Long Ye, Zixie Li, Rui Niu, Zhuxian Zhou, Youqing Shen, and Liming Jiang, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00457. keywords: {fragrance;silk fibroin;nanoencapsulation;electrospray;sustained release;fabric}