daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Electrochemical Interaction of Sn-Containing MAX Phase (Nb2SnC) with Li-Ions AITranslate

Jilin University; University College London; Jilin Jianzhu University; Jilin University; Drexel University; Jilin University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this Letter, we report on the interaction of Nb2SnC ternary transition metal carbide (MAX phase) with Li ions. Because of the presence of Sn layers, which can undergo alloying reaction with Li, this material may be promising for energy storage. Contrary to most electrodes, the performance of this material improves along with the cycle number; specifically, the capacity increases gradually from 87 to 150 mAh g–1 at a current density of 500 mA g–1 during 600 charge/discharge cycles. Postcycling study suggests that the alloying reaction makes the material break into smaller particles, increasing capacity. Because Nb2SnC is just one of many MAX phases, this work lays the foundation for exploration of the MAX phases in lithium-ion or other batteries.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01580

Chinese Library Classification Number:

Citation Information:

In this Letter, we report on the interaction of Nb2SnC ternary transition metal carbide (MAX phase) with Li ions. Because of the presence of Sn layers, which can undergo alloying reaction with Li, this material may be promising for energy storage. Contrary to most electrodes, the performance of this material improves along with the cycle number; specifically, the capacity increases gradually from 87 to 150 mAh g–1 at a current density of 500 mA g–1 during 600 charge/discharge cycles. Postcycling study suggests that the alloying reaction makes the material break into smaller particles, increasing capacity. Because Nb2SnC is just one of many MAX phases, this work lays the foundation for exploration of the MAX phases in lithium-ion or other batteries.

quote

GB/T 7714-2015 [1] Shuangshuang Zhao, Yohan Dall’Agnese, Xuefeng Chu, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01580.
MLA [1] Shuangshuang Zhao, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01580.
APA [1] Shuangshuang Zhao, Yohan Dall’Agnese, Xuefeng Chu, Xin Zhao, Yury Gogotsi, & Yu Gao. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01580
IEEE [1] Shuangshuang Zhao, Yohan Dall’Agnese, Xuefeng Chu, Xin Zhao, Yury Gogotsi, and Yu Gao, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01580.