Environmentally friendly membranes with on-demand oil/water separation ability have recently received increasing attention in the application field of oily wastewater treatment. Herein, a facile and sustainable approach to prepare a flexible electrospun nanofiber/nanonet membrane using biodegradable polymers, chitosan (CS), and polycaprolactone (PCL) for controllable oil/water separation was demonstrated. The CS@PCL membranes are superamphiphilic, with both water and oil contact angles in air of 0°. The CS@PCL membrane shows underoil superhydrophobicity and underwater superoleophobicity. The membrane can effectively separate various oil/water mixtures, including immiscible oil/water mixtures and oil-in-water and water-in-oil emulsions by a simple prewetting approach. The obtained membrane exhibits a high separation efficiency of above 94.6% for immiscible light/heavy oil/water mixtures. Furthermore, the membrane shows excellent separation efficiencies for oil-in-water emulsions and water-in-oil emulsions, as above 99.9 and 94.5%, respectively.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00463
Chinese Library Classification Number:
Citation Information:
Environmentally friendly membranes with on-demand oil/water separation ability have recently received increasing attention in the application field of oily wastewater treatment. Herein, a facile and sustainable approach to prepare a flexible electrospun nanofiber/nanonet membrane using biodegradable polymers, chitosan (CS), and polycaprolactone (PCL) for controllable oil/water separation was demonstrated. The CS@PCL membranes are superamphiphilic, with both water and oil contact angles in air of 0°. The CS@PCL membrane shows underoil superhydrophobicity and underwater superoleophobicity. The membrane can effectively separate various oil/water mixtures, including immiscible oil/water mixtures and oil-in-water and water-in-oil emulsions by a simple prewetting approach. The obtained membrane exhibits a high separation efficiency of above 94.6% for immiscible light/heavy oil/water mixtures. Furthermore, the membrane shows excellent separation efficiencies for oil-in-water emulsions and water-in-oil emulsions, as above 99.9 and 94.5%, respectively.
quote
| GB/T 7714-2015 | [1] Hoan Ngoc Doan, Phu Phong Vo, Andrea Baggio, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00463. |
| MLA | [1] Hoan Ngoc Doan, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00463. |
| APA | [1] Hoan Ngoc Doan, Phu Phong Vo, Andrea Baggio, Masaki Negoro, Kenji Kinashi, Yasuro Fuse, Wataru Sakai, & Naoto Tsutsumi. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00463 |
| IEEE | [1] Hoan Ngoc Doan, Phu Phong Vo, Andrea Baggio, Masaki Negoro, Kenji Kinashi, Yasuro Fuse, Wataru Sakai, and Naoto Tsutsumi, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00463. keywords: {electrospinning;polycaprolactone;chitosan;oil/water separation;emulsion separation} |