Silicon Removal from the Alkali Leach Liquor of Carbonaceous Shale Containing Vanadium AITranslate
Abstract AITranslate
In view of the high silicon concentration in the alkali leach liquor of carbonaceous shale containing vanadium, most of the silicon was removed by coagulating sedimentation. The results show that under the optimal conditions,that is adding 102 g/L Al2 (SO4)3 solution by 3% the volume of the alkali leach liquor (98 ℃ and pH 10.5),controlling the final pH value at 9.0,keeping the liquor volume nearly unchanged, and maintaining the liquor temperature for 1 h, the silicon removal rate is up to 90 % and vanadium loss rate less than 1.5%.
KeyWords AITranslate
1米玺学,兰玮锋.从石煤钒矿石中提取五氧化二钒工艺综述[J].湿法冶金,2008,27(4):208-210. 被引量:16
2李硕文,陈扬,李峻,许燕.改性活性硅酸(PSA)制备及水处理性能的试验研究[J].中国给水排水,1994,10(5):18-21. 被引量:2
3Christopher Gabelioh J.The role of dissolved aluminum in silica chemistry for membrane processes[J].Desalination,2005,108:307-319.
4Gallup D L.Aluminum silicate scale formation and inhibition:scale characterization and laboratory experiment[J].Geothermics,1997,26(4):483-499.
5徐如人.沸石分子筛的结构与合成[M].长春:吉林大学出版社,1986.
1段冉,李青刚.从钒酸钠溶液中深度除磷制备高纯V_2O_5的研究[J].稀有金属,2011,35(4):543-547. 被引量:11
2邓棹栩,叶宇玲,杨虎.利用制钒废水中回收的含钒铬渣制备多钒酸铵的工艺研究[J].化工技术与开发,2012,41(4):15-17. 被引量:4
3何静,王涛,罗超,王小能,郭瑞,蓝明艳.高纯硫酸盐溶液微量硅脱除工艺研究[J].有色金属:冶炼部分,2012(10):1-3.
4龙思思,冯其明,张国范,欧乐明,卢毅屏.V-Si-CO_3^(2-)H_2O体系浸出液中硅和钒的回收及浸出剂的再生[J].中南大学学报:自然科学版,2014,45(3):663-670.
5刘珍珍,刘勇,周吉奎,刘牡丹.协同沉淀法深度净化钒酸钠溶液中硅和磷[J].稀有金属与硬质合金,2018,46(3):6-9.
6高志强,任倩.沉淀法去除钼酸钠溶液中磷和硅试验研究[J].中国钼业,2023,47(3):41-44.
1朱军,郭继科,齐建云,刘新运,薛晶晶,王娜.石煤焙烧物料提钒的试验研究[J].稀有金属,2012,36(5):804-810. 被引量:6
2李静,王素素,徐辉,高峰,颜文斌.硫酸镁去除工业偏钒酸铵中磷和硅的研究[J].广州化工,2012,40(22):64-66. 被引量:6
3吴恩辉,朱荣,杨绍利,郭亚光.从含钒铬物料中分离提取钒铬的研究进展[J].湿法冶金,2013,32(4):214-216. 被引量:7
4危青,戴子林,吴海鹰,李桂英.石煤提钒富液直接制备高纯V_2O_5[J].金属矿山,2013(12):66-69. 被引量:5
5张东.钒铬还原渣资源化利用技术进展[J].有色矿冶,2014,30(5):52-54. 被引量:4
6尹丹凤,孙朝晖,景涵,杜光超,陈海军.多钒酸铵返溶的动力学研究[J].钢铁钒钛,2015,36(6):13-17. 被引量:1
7杨明平,王远望.利用失效钒电解液回收钒制备偏钒酸铵工艺[J].化工进展,2016,35(9):2982-2986. 被引量:5
8周嘉郁,张一敏,包申旭,段继华.用电容去离子技术去除含钒酸浸液中的磷[J].金属矿山,2016,45(9):107-111. 被引量:2
9彭荣华.从钒电池废电解液中回收钒制备五氧化二钒的工艺研究[J].现代化工,2016,36(10):64-67. 被引量:3
10刘珍珍,刘勇,周吉奎,刘牡丹.协同沉淀法深度净化钒酸钠溶液中硅和磷[J].稀有金属与硬质合金,2018,46(3):6-9.
1肖超,肖连生,成宝海,曹佐英.石煤钒矿碱性浸出液提取钒新工艺[J].稀有金属与硬质合金,2011,39(1):4-7. 被引量:10
2漆杰,佘文华,李勇,冯晓军,宋智义,陈泽华.电解铝渣场含氟废水处理实践[J].中国有色冶金,2013,42(2):80-82. 被引量:1
3吴宋超,杨玲,赖华生.铝钙渣硫酸浸出提铝研究[J].有色金属科学与工程,2011,2(4):21-25. 被引量:3
4陈惠,张岩岩,李建文,司士辉.石煤微波辅助提钒及浸出液除杂研究[J].稀有金属与硬质合金,2011,39(2):1-5. 被引量:3
5郭英姿,王鹏.氨法焙烧粉煤灰浸出液联合法除铁工艺研究[J].轻金属,2014(4):17-21.
6张曦,邹晓勇.含钒液体除硅过程的研究[J].金属材料与冶金工程,2007,35(6):19-22.
7童秋桃,朱高远,肖奇.铝土矿选矿尾矿酸法提铝除铁实验研究[J].湖南有色金属,2012,28(1):21-24. 被引量:4
8刘晓红,刘守信,邹美琪,柯春兰,许春晓.从铝灰中回收铝制备超细氧化铝粉体过程研究[J].轻金属,2009(12):18-20. 被引量:14
9李静,王素素,徐辉,高峰,颜文斌.硫酸镁去除工业偏钒酸铵中磷和硅的研究[J].广州化工,2012,40(22):64-66. 被引量:6
10曹耀华,刘红召,高照国,杨绍文.从彩钼铅粗精矿碱性浸出液中提取钼的新工艺[J].湿法冶金,2012,31(2):118-121. 被引量:6
Basic Information:
DOI:
Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]
Citation Information:
In view of the high silicon concentration in the alkali leach liquor of carbonaceous shale containing vanadium, most of the silicon was removed by coagulating sedimentation. The results show that under the optimal conditions,that is adding 102 g/L Al2 (SO4)3 solution by 3% the volume of the alkali leach liquor (98 ℃ and pH 10.5),controlling the final pH value at 9.0,keeping the liquor volume nearly unchanged, and maintaining the liquor temperature for 1 h, the silicon removal rate is up to 90 % and vanadium loss rate less than 1.5%.
quote
| GB/T 7714-2015 | [1] XIAO Chao, XIAO Lian-sheng, LI Qing-gang. Silicon Removal from the Alkali Leach Liquor of Carbonaceous Shale Containing Vanadium[J]. Rare Metals and Cemented Carbides, 2010(1): 8-10. |
| MLA | [1] XIAO Chao, et al., "Silicon Removal from the Alkali Leach Liquor of Carbonaceous Shale Containing Vanadium." Rare Metals and Cemented Carbides, no. 1, 2010, pp. 8-10. |
| APA | [1] XIAO Chao, XIAO Lian-sheng, & LI Qing-gang. (2010). Silicon Removal from the Alkali Leach Liquor of Carbonaceous Shale Containing Vanadium. Rare Metals and Cemented Carbides(1), 8-10. |
| IEEE | [1] XIAO Chao, XIAO Lian-sheng, and LI Qing-gang, "Silicon Removal from the Alkali Leach Liquor of Carbonaceous Shale Containing Vanadium," Rare Metals and Cemented Carbides, no. 1, pp. 8-10, 2010. keywords: {alkali leach liquor of carbonaceous shale containing vanadium;silicon removal;coagulating sedi- mentation} |