Research on Mechanism of Preparation of Crystalline Yttrium Carbonate by Precipitation of Ammonium Bicarbonate AITranslate
Abstract AITranslate
Crystalline hydrated yttrium carbonate and hydrated crystalline ammonium and yttrium carbonate compound are obtained by precipitation of yttrium sulphate solutions with different amount of ammonium bicarbonate under given conditions.The process and mechanism of conversion of amorphous precipitate into crystalline precipitate during precipitation and aging were studied by element anaysis,X-ray powder diffractometry,infra-red spectrometry,thermal analysis and scanning electron microscope.
KeyWords AITranslate
1贺伦燕.碳酸铵淋洗从离子型稀土矿中提取稀土工艺的研究[J].稀土,1983,(3):1-1.
2贺伦燕,王似男.我国南方离子吸附型稀土矿[J].稀土,1989(1):39-44. 被引量:52
3贺伦燕,王似男,周新木,胡平贵,辜子英,魏坤,李永绣,何小彬,文芝玉.碳酸稀土晶粒状沉淀制取工艺的研究[J].稀有金属与硬质合金,1993,21(4):18-21. 被引量:10
4李先柏,喻庆华.晶型钐、铕、钆、铽碳酸盐的合成[J].稀土,1993,14(5):7-11. 被引量:5
5李先柏,喻庆华.晶型镧、铈、镨、钕碳酸盐的合成[J].稀有金属与硬质合金,1994,22(3):1-6. 被引量:4
1闫勇,朱伟长,李辉生.氧化钇纳米粉体材料的制备[J].化工新型材料,2004,32(7):11-12. 被引量:5
2闻雷,其鲁,孙旭东,徐国祥.碳酸盐沉淀法制备Y_2O_3纳米粉及透明陶瓷[J].中国有色金属学报,2006,16(2):235-240. 被引量:10
3潘艳,李玮楠,陆敏.稀土掺杂的纳米晶材料化学制备方法的研究[J].武汉理工大学学报,2007,29(E01):150-153.
4霍地,孙旭东,修稚萌,李晓东.制备工艺对超细氧化钇粉体形态与烧结性的影响[J].中国稀土学报,2007,25(5):566-572. 被引量:12
5郭易芬,马伟民,闻雷,沈世妃,王华栋,尹凯.碳酸氢铵共沉淀法制备(Y,Gd)2O3:Eu^3+纳米材料及光谱特性[J].人工晶体学报,2009,38(3):746-750. 被引量:5
6李永超,谭亚军.纳米YAG粉体的制备与表征[J].贵州大学学报:自然科学版,2011,28(5):45-48. 被引量:1
7刘宇晖,余荣旻,欧阳宇平,苏正夫,邵春欣,王志坚,刘吉波.粒度可控氧化钇粉体的制备[J].有色金属科学与工程,2015,6(3):22-25.
8高国华,赖安邦,廖春发,刘钧云,任卫,肖燕飞.Na2CO3沉淀制备超细Y2O3粉体的研究[J].中国稀土学报,2020,38(5):622-632. 被引量:5
1李家茂,龙世刚,樊传刚,闫勇.氧化钇纳米粉浸渍处理对氧化铝陶瓷抗钢液腐蚀性能的影响[J].中国稀土学报,2006,24(6):701-704. 被引量:2
2何镜泉,廖列文,史爱华.沉淀法制备纳米稀土氧化物的研究进展[J].仲恺农业技术学院学报,2007,20(1):66-71. 被引量:5
3霍地,孙旭东,刘亦农,张牧,修稚萌,李晓东.超细粉体制备Nd∶Y2O3透明陶瓷[J].中国稀土学报,2008,26(1):56-60. 被引量:6
4柳召刚,李梅,胡艳宏,王觅堂,史振学.Preparation of large particle rare earth oxides by precipitation with oxalic acid[J].稀土学报:英文版,2008,26(2):158-162. 被引量:16
5刘晶,马伟民,闻雷,李喜坤,沈世妃,郭易芬.共沉淀法制备BaHfO_3:Ce纳米粉体及发光性能[J].中国有色金属学报,2008,18(8):1492-1497. 被引量:3
6缪飞,余林,孙明,李朝圣,张雷.纳米氧化钇的制备与表征[J].精细化工,2009,26(4):313-317.
7沈世妃,马伟民,闻雷,郭易芬,尹凯,王华栋.(Y,Gd)2O3:Eu闪烁体材料的研究进展[J].人工晶体学报,2009,38(2):465-470. 被引量:1
8郭易芬,马伟民,闻雷,沈世妃,王华栋,尹凯.碳酸氢铵共沉淀法制备(Y,Gd)2O3:Eu^3+纳米材料及光谱特性[J].人工晶体学报,2009,38(3):746-750. 被引量:5
9申晨,薛玉君,刘红彬,韩红彪,刘义.超声电沉积法制备Ni-Y_2O_3纳米复合镀层的工艺[J].材料保护,2009,42(7):25-28. 被引量:9
10何庭秋,闻芳,高会焕,雷牧云,黄存新,宋庆海,李法荟.Y_2O_3∶Nd透明陶瓷的制备[J].硅酸盐通报,2009,28(6):1336-1339.
1贺伦燕,王似男,周新木,胡平贵,辜子英,魏坤,李永绣,何小彬,文芝玉.碳酸稀土晶粒状沉淀制取工艺的研究[J].稀有金属与硬质合金,1993,21(4):18-21. 被引量:10
2刘志强,李杏英,梁振锋.碳铵沉淀法制备纳米氧化钇过程中氯离子的行为[J].中国稀土学报,2005,23(3):373-377. 被引量:13
3李常清,李才生,涂小珍,吴新根.碳酸氢铵沉淀制备高松装密度氧化铈[J].江西冶金,2005,25(6):1-3. 被引量:2
4邓红梅,徐燕,顾翼东.超细均分散胶体Y(OH)Co_3的热力学稳定性[J].中国稀土学报,1995,13(2):116-118.
5韦群燕,谢刚,李荣兴,杨项军,谭富彬.化学沉淀制备超细银粉及其形貌特征[J].云南冶金,2004,33(1):32-34. 被引量:9
6张俊卿,吴志华,韩莉.从少铕氯化稀土中提取氧化铈的研究──碳酸氢铵作为沉淀剂的探讨[J].包头钢铁学院学报,1995,14(1):42-44.
7韩彦利.海洋锰结核的试验研究──Ni(Ⅱ)在H_2O—NH_3—SO_2—MnO_2体系[J].中国锰业,1996,14(2):57-61.
8刘志强,梁振锋,李杏英.纳米氧化钇的制备及表征[J].矿冶工程,2006,26(3):78-80. 被引量:6
9胡慧萍,谢丽芳,陈启元,王树宾.碱法浸出含锌废催化剂制备硫化锌[J].有色金属:冶炼部分,2012(1):42-45. 被引量:9
10戴红.Mo和Ru纳米粉末的生长机制及热稳定性[J].有色金属,2002,54(B07):57-60. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:TF845.2[冶金工程—有色金属冶金]
Citation Information:
Crystalline hydrated yttrium carbonate and hydrated crystalline ammonium and yttrium carbonate compound are obtained by precipitation of yttrium sulphate solutions with different amount of ammonium bicarbonate under given conditions.The process and mechanism of conversion of amorphous precipitate into crystalline precipitate during precipitation and aging were studied by element anaysis,X-ray powder diffractometry,infra-red spectrometry,thermal analysis and scanning electron microscope.
quote
| GB/T 7714-2015 | [1] HE Lun-yan, LI Nan-ping. Research on Mechanism of Preparation of Crystalline Yttrium Carbonate by Precipitation of Ammonium Bicarbonate[J]. Rare Metals and Cemented Carbides, 2002(1): 1-5. |
| MLA | [1] HE Lun-yan, and LI Nan-ping. "Research on Mechanism of Preparation of Crystalline Yttrium Carbonate by Precipitation of Ammonium Bicarbonate." Rare Metals and Cemented Carbides, no. 1, 2002, pp. 1-5. |
| APA | [1] HE Lun-yan, & LI Nan-ping. (2002). Research on Mechanism of Preparation of Crystalline Yttrium Carbonate by Precipitation of Ammonium Bicarbonate. Rare Metals and Cemented Carbides(1), 1-5. |
| IEEE | [1] HE Lun-yan and LI Nan-ping, "Research on Mechanism of Preparation of Crystalline Yttrium Carbonate by Precipitation of Ammonium Bicarbonate," Rare Metals and Cemented Carbides, no. 1, pp. 1-5, 2002. keywords: {precipitation of ammonium bicarbonate;yttrium carbonate;NH 3-Yt carbonate compound;crystalline precipitation;amorphous precipitation} |