daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Controlling the Pretilt Angles of Guest–Host Liquid Crystals via a Hydrophilic Polyimide Layer through Oxygen Plasma Treatment AITranslate

Hefei University of Technology; Hefei University of Technology; Hefei University of Technology; Hefei University of Technology; Hefei University of Technology; AVIC Beijing Aeronautic Manufacturing Technology Research Institute; AVIC Beijing Aeronautic Manufacturing Technology Research Institute; Hefei University of Technology; Hefei University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The control of the liquid crystal (LC) alignment is an important factor for practical applications. The conventional method typically used is the rubbing of the polyimide (PI) layer. However, it is difficult to obtain intermediate pretilt angles by employing such a method. In this paper, control of the pretilt angle of the LC is achieved by modifying the surface wettability of the PI films via oxygen plasma treatment. A new mode for guest–host liquid crystal (GHLC) smart windows is achieved with intermediate initial transmittance by controlling the pretilt angle, which can turn from the initial state to either the transparent or dark states. Different modes for the GHLC-based smart windows can be fabricated that are dependent on the environmental conditions.

KeyWords AITranslate

pretilt angle liquid crystal alignment guest−host liquid crystals wettability liquid crystal displays smart window
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00868

Chinese Library Classification Number:

Citation Information:

The control of the liquid crystal (LC) alignment is an important factor for practical applications. The conventional method typically used is the rubbing of the polyimide (PI) layer. However, it is difficult to obtain intermediate pretilt angles by employing such a method. In this paper, control of the pretilt angle of the LC is achieved by modifying the surface wettability of the PI films via oxygen plasma treatment. A new mode for guest–host liquid crystal (GHLC) smart windows is achieved with intermediate initial transmittance by controlling the pretilt angle, which can turn from the initial state to either the transparent or dark states. Different modes for the GHLC-based smart windows can be fabricated that are dependent on the environmental conditions.

quote

GB/T 7714-2015 [1] Yuge Liang, Yumeng Wang, Mengmeng Zhu, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00868.
MLA [1] Yuge Liang, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00868.
APA [1] Yuge Liang, Yumeng Wang, Mengmeng Zhu, Longzhen Qiu, Jun Zhu, Bo Zhang, Ying Liu, Hongbo Lu, & Miao Xu. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00868
IEEE [1] Yuge Liang, Yumeng Wang, Mengmeng Zhu, Longzhen Qiu, Jun Zhu, Bo Zhang, Ying Liu, Hongbo Lu, and Miao Xu, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00868. keywords: {pretilt angle liquid crystal alignment guest−host liquid crystals wettability liquid crystal displays smart window}