Unveiling the Potential of HfO2/WS2 Bilayer Films: Robust Analog Switching and Synaptic Emulation for Advanced Memory and Neuromorphic Computing AITranslate

Dongguk University;Department of Advanced Battery Convergence Engineering, Seoul 04620; Dongguk University; Dongguk University; Korea National University of Transportation; Dongguk University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nonvolatile memories using two-dimensional materials and high-k oxides have gained attention for their potential to achieve robust analog switching, easy memristive device integration, and low-energy consumption. In this study, we fabricated Pt/TiN/HfO2/WS2/Pt memristive devices. To implement these devices, a WS2 film was thermally evaporated under high vacuum conditions followed by HfO2 growth using atomic layer deposition at 400 °C. Detailed analysis using high-resolution transmission electron microscopy and X-ray photoelectron spectroscopy revealed diffusion of W and S atoms within the HfO2 layer and extraction of oxygen by W atoms, thus resulting in a multilayer structure (HfWOySx, Wx–1OySx, and W1–xOySx) with varying ratios of oxygen, tungsten, and sulfur atoms (x and y). The fabricated devices demonstrated consistent and stable analogue switching over numerous cycles, with exceptional endurance (2000 cycles) and retention (103 s). They exhibited high cycle-to-cycle consistency, as evidenced by the low-coefficient of variation (3.5% and 4.0% for the set and reset voltages, respectively). By modulating the reset stop voltage, we achieved five-level resistance states, thus making these devices capable of being used in artificial synapses. Furthermore, we observed analog switching with gradual resistance changes under different current compliance conditions by incrementally adjusting the reset–stop voltage. The memristor-based artificial synapses exhibited fundamental synaptic functions, such as long-term potentiation, long-term depression, paired-pulse facilitation, paired-pulse depression, and spike-timing-dependent plasticity for long-term and short-term plasticity. Moreover, we employed a three-layer artificial neural network for image recognition, achieving 94% accuracy using identical pulse amplitudes. These findings highlight the potential of HfO2/WS2 bilayer films, enable controllable analogue switching, and simulate synaptic functions. They hold promise for future data storage memory and neuromorphic computing systems.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00600

Chinese Library Classification Number:

Citation Information:

Nonvolatile memories using two-dimensional materials and high-k oxides have gained attention for their potential to achieve robust analog switching, easy memristive device integration, and low-energy consumption. In this study, we fabricated Pt/TiN/HfO2/WS2/Pt memristive devices. To implement these devices, a WS2 film was thermally evaporated under high vacuum conditions followed by HfO2 growth using atomic layer deposition at 400 °C. Detailed analysis using high-resolution transmission electron microscopy and X-ray photoelectron spectroscopy revealed diffusion of W and S atoms within the HfO2 layer and extraction of oxygen by W atoms, thus resulting in a multilayer structure (HfWOySx, Wx–1OySx, and W1–xOySx) with varying ratios of oxygen, tungsten, and sulfur atoms (x and y). The fabricated devices demonstrated consistent and stable analogue switching over numerous cycles, with exceptional endurance (2000 cycles) and retention (103 s). They exhibited high cycle-to-cycle consistency, as evidenced by the low-coefficient of variation (3.5% and 4.0% for the set and reset voltages, respectively). By modulating the reset stop voltage, we achieved five-level resistance states, thus making these devices capable of being used in artificial synapses. Furthermore, we observed analog switching with gradual resistance changes under different current compliance conditions by incrementally adjusting the reset–stop voltage. The memristor-based artificial synapses exhibited fundamental synaptic functions, such as long-term potentiation, long-term depression, paired-pulse facilitation, paired-pulse depression, and spike-timing-dependent plasticity for long-term and short-term plasticity. Moreover, we employed a three-layer artificial neural network for image recognition, achieving 94% accuracy using identical pulse amplitudes. These findings highlight the potential of HfO2/WS2 bilayer films, enable controllable analogue switching, and simulate synaptic functions. They hold promise for future data storage memory and neuromorphic computing systems.

quote

GB/T 7714-2015 [1] Muhammad Ismail, Maria Rasheed, Sunghun Kim, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00600.
MLA [1] Muhammad Ismail, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00600.
APA [1] Muhammad Ismail, Maria Rasheed, Sunghun Kim, Chandreswar Mahata, Myounggon Kang, & Sungjun Kim. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00600
IEEE [1] Muhammad Ismail, Maria Rasheed, Sunghun Kim, Chandreswar Mahata, Myounggon Kang, and Sungjun Kim, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00600.