Pretreatment of Hevea Latex by Sorbitol: Improving the Efficacy of Silica Dispersion by a Biomimetic Approach AITranslate
Abstract AITranslate
Incorporating a high amount of silica in cis-1,4-polyisoprene (CPI) by conventional dry mixing is a Herculean task. A biomimicking approach is adopted herein through incorporation of a bio-based sugar alcohol (sorbitol) into the CPI latex, which creates protein–carbohydrate interactions in the latex called protein–sugar conjugates. These treatments unveiled a significant improvement in key properties of the CPI vulcanizates, like >15% reduction in tan δ at a high temperature, besides better dispersion as evident from morphological studies. The protein and phospholipid ends were cleaved by respective enzymes for a clearer percipience of their individual effects on compounds’ key properties. The molecular dynamics study reveals a faster convergence of root-mean-square deviation (RMSD) and maximum radius of gyration (Rg) values of the sorbitol-treated latex, confirming a stable conformation of the CPI matrix in the presence of silica. Subsequently, a greater number of hydrogen bonds between the functional groups of protein and sorbitol demonstrates successful blocking of the functional groups (protein–sugar conjugates) of CPIs’ unwanted substances.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c01588
Chinese Library Classification Number:
Citation Information:
Incorporating a high amount of silica in cis-1,4-polyisoprene (CPI) by conventional dry mixing is a Herculean task. A biomimicking approach is adopted herein through incorporation of a bio-based sugar alcohol (sorbitol) into the CPI latex, which creates protein–carbohydrate interactions in the latex called protein–sugar conjugates. These treatments unveiled a significant improvement in key properties of the CPI vulcanizates, like >15% reduction in tan δ at a high temperature, besides better dispersion as evident from morphological studies. The protein and phospholipid ends were cleaved by respective enzymes for a clearer percipience of their individual effects on compounds’ key properties. The molecular dynamics study reveals a faster convergence of root-mean-square deviation (RMSD) and maximum radius of gyration (Rg) values of the sorbitol-treated latex, confirming a stable conformation of the CPI matrix in the presence of silica. Subsequently, a greater number of hydrogen bonds between the functional groups of protein and sorbitol demonstrates successful blocking of the functional groups (protein–sugar conjugates) of CPIs’ unwanted substances.
quote
| GB/T 7714-2015 | [1] Abhijit Bera, Bharat Manna, Debabrata Ganguly, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01588. |
| MLA | [1] Abhijit Bera, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01588. |
| APA | [1] Abhijit Bera, Bharat Manna, Debabrata Ganguly, S. K. P. Amarnath, Samik Nanda, Amit Ghosh, & Santanu Chattopadhyay. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01588 |
| IEEE | [1] Abhijit Bera, Bharat Manna, Debabrata Ganguly, S. K. P. Amarnath, Samik Nanda, Amit Ghosh, and Santanu Chattopadhyay, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01588. keywords: {green tire;natural rubber;biobased blocking agent;silica;protein;phospholipid;enzymes} |