巯基环烷酸对镧、钕、钐萃取性能的研究(I) AITranslate

Yueyang University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

本文研究了巯基环烷酸对镧、钕、钐的萃取性能,发现其萃取能力比环烷酸强,应用酸度范围广,且能避免乳化,可望成为工业萃取剂。

KeyWords AITranslate

巯基环烷酸 萃取 镧 钕 钐

1洪涌,成本诚.α—氯代环烷酸对稀土萃取的研究[J].稀有金属与硬质合金,1990(2):1-3. 被引量:3

2[日]关根达也,长谷川佑子 著,腾藤.溶剂萃取化学[M]原子能出版社,1981.

1李效军,雒佳莉,王凯,孙树娟,贾睿生.2,2'-硫代双对叔辛基苯酚萃取镍的性能[J].有色金属,2009,61(4):65-67.

Basic Information:

DOI:

Chinese Library Classification Number:TF845.6[冶金工程—有色金属冶金]

Citation Information:

本文研究了巯基环烷酸对镧、钕、钐的萃取性能,发现其萃取能力比环烷酸强,应用酸度范围广,且能避免乳化,可望成为工业萃取剂。

quote

GB/T 7714-2015 [1] YI Jian-min. Rare Metals and Cemented Carbides, 1993(2): 6-8.
MLA [1] YI Jian-min. Rare Metals and Cemented Carbides, no. 2, 1993, pp. 6-8.
APA [1] YI Jian-min. (1993). Rare Metals and Cemented Carbides(2), 6-8.
IEEE [1] YI Jian-min, Rare Metals and Cemented Carbides, no. 2, pp. 6-8, 1993.