daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Cellulose Nanocrystals Mimicking Micron-Sized Fibers to Assess the Deposition of Latex Particles on Cotton AITranslate

Université de Paris;Solvay Research & Innovation Center Singapore, 1 Biopolis Drive;Solvay Paris, 52 rue de la Haie-Coq;Solvay Paris, 52 rue de la Haie-Coq;Solvay Research & Innovation Center Singapore, 1 Biopolis Drive;Centre de Recherches sur les Macromolécules Végétales (CERMAV) BP 53, Grenoble 38041;Université de Paris
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We report the interactions of cationic latex particles synthesized by reversible addition–fragmentation chain transfer/macromolecular design by the interchange of xanthates-mediated emulsion polymerization with anionic cellulose nanocrystals (CNCs) and cotton fabrics. Latexes in the size range of 200–300 nm with poly(butyl acrylate) or poly(2-ethylhexyl acrylate) hydrophobic cores and a hydrophilic shell are synthesized. We show that the latex/CNC interaction is mediated by electrostatics, the interaction being the strongest with the most charged particles. The adsorption process is efficient and does not require any functionalization step for either cellulose or latex. A major result is the observation by cryogenic transmission electron microscopy of latexes coated with entangled arrays of CNCs, and for the softer particles, a notable deformation of their structure into faceted polyhedra. By labeling the latexes with hydrophobic carbocyanine dyes, their deposition on woven cotton fabrics is studied in situ and quantified by fluorescence microscopy. As with the CNCs, the highest deposition on cotton in the wet and dried states is achieved with the most charged latexes. This demonstrates that CNCs can serve as models to adjust the interactions of latex particles with cotton and thus optimize manufacturing processes for the development of advanced textiles.

KeyWords AITranslate

core−shell copolymers latex particles cellulose nanocrystals (CNCs) electrostatic adsorption cotton fabric Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01411

Chinese Library Classification Number:

Citation Information:

We report the interactions of cationic latex particles synthesized by reversible addition–fragmentation chain transfer/macromolecular design by the interchange of xanthates-mediated emulsion polymerization with anionic cellulose nanocrystals (CNCs) and cotton fabrics. Latexes in the size range of 200–300 nm with poly(butyl acrylate) or poly(2-ethylhexyl acrylate) hydrophobic cores and a hydrophilic shell are synthesized. We show that the latex/CNC interaction is mediated by electrostatics, the interaction being the strongest with the most charged particles. The adsorption process is efficient and does not require any functionalization step for either cellulose or latex. A major result is the observation by cryogenic transmission electron microscopy of latexes coated with entangled arrays of CNCs, and for the softer particles, a notable deformation of their structure into faceted polyhedra. By labeling the latexes with hydrophobic carbocyanine dyes, their deposition on woven cotton fabrics is studied in situ and quantified by fluorescence microscopy. As with the CNCs, the highest deposition on cotton in the wet and dried states is achieved with the most charged latexes. This demonstrates that CNCs can serve as models to adjust the interactions of latex particles with cotton and thus optimize manufacturing processes for the development of advanced textiles.

quote

GB/T 7714-2015 [1] Evdokia K. Oikonomou, Konstantin Golemanov, PierreEmmanuel Dufils, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01411.
MLA [1] Evdokia K. Oikonomou, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01411.
APA [1] Evdokia K. Oikonomou, Konstantin Golemanov, PierreEmmanuel Dufils, James Wilson, Ritu Ahuja, Laurent Heux, & JeanFrançois Berret. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01411
IEEE [1] Evdokia K. Oikonomou, Konstantin Golemanov, PierreEmmanuel Dufils, James Wilson, Ritu Ahuja, Laurent Heux, and JeanFrançois Berret, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01411. keywords: {core−shell copolymers;latex particles;cellulose nanocrystals (CNCs);electrostatic adsorption;cotton fabric;Show More}