The Latest Study on Extrusion Molding Binder and Production Technology of Cemented Carbide AITranslate
Abstract AITranslate
The extrusion molding technology of cemented carbide is introduced in detail including the devel opment of molding hinder and the production technology and equipment of each procedure. The actual op erating essentials of each step are introduced in detail,and the future development of cemented carbide ex trusion molding technology is pointed out.
KeyWords AITranslate
1王晓瑾,卢宏(翻译).影响挤压硬质合金棒材质量的因素分析[J].江西冶金,2006,26(6):13-15. 被引量:4
2羊建高,谭敦强,陈颢.硬质合金[M].长沙:中南大学出版社,2012.
3卓海宇,卓萍.硬质合金混合料制备过程中的质量控制[J].湖南理工学院学报:自然科学版,2004,17(4):68-70. 被引量:5
4郭幸华.硬质合金真空挤压成型剂及其制备方法[P].中国专利:100441343C,2008-1210.
5郭幸华.一种活塞式真空挤压机[P].中国专利:2915483Y,2007-06-27.
6周继承,黄伯云.增塑粉末挤压成形用新成形剂的研制[J].粉末冶金技术,2002,20(1):13-15. 被引量:6
1张梅琳,朱世根,朱守星.超细及纳米硬质合金中碳含量的变化及对组织性能的影响[J].材料导报,2006,20(8):65-68. 被引量:24
2孙丹,张鹤年,孙卫权,李广生.一种新型超细硬质合金棒料挤压成形剂的设计[J].硬质合金,2009,26(3):176-179. 被引量:5
3罗向阳,马益诚.压铸技术与装备的新发展[J].机电工程,2005,22(4):50-54.
4陈双琳,付坤,周建华,孙宝琦.硬质合金成形剂石蜡的改进研究[J].稀有金属与硬质合金,2014,42(3):58-62. 被引量:3
5张立,吴冲浒,王振波,单成,熊湘君.硬质合金常用模压成形剂的热分解特性[J].粉末冶金材料科学与工程,2010,15(6):674-678. 被引量:7
6刘晓焱,王晓飞.冲床上触指挤压成形技术[J].热加工工艺,2012,41(17):95-96.
7林亚冬.刍议冲床上触指挤压成形技术[J].广东科技,2014,23(18):161-162.
8林信平,曹顺华,李炯义.温压工艺在硬质合金制备中的应用[J].中国钼业,2004,28(3):29-33. 被引量:3
9李峰,石文勇,武英博,边楠.金属挤压成形技术研究与应用进展[J].精密成形工程,2014,6(5):45-49. 被引量:3
10刘兆刚,王维一,谢垚,王战宏,李峰,买学峰,于伟.铍铝合金挤压成形技术研究[J].湖南有色金属,2015,31(2):49-53. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG124.3[金属学及工艺—金属学]
Citation Information:
The extrusion molding technology of cemented carbide is introduced in detail including the devel opment of molding hinder and the production technology and equipment of each procedure. The actual op erating essentials of each step are introduced in detail,and the future development of cemented carbide ex trusion molding technology is pointed out.
quote
| GB/T 7714-2015 | [1] GUO Xing-hua. The Latest Study on Extrusion Molding Binder and Production Technology of Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2014(6): 46-48. |
| MLA | [1] GUO Xing-hua. "The Latest Study on Extrusion Molding Binder and Production Technology of Cemented Carbide." Rare Metals and Cemented Carbides, no. 6, 2014, pp. 46-48. |
| APA | [1] GUO Xing-hua. (2014). The Latest Study on Extrusion Molding Binder and Production Technology of Cemented Carbide. Rare Metals and Cemented Carbides(6), 46-48. |
| IEEE | [1] GUO Xing-hua, "The Latest Study on Extrusion Molding Binder and Production Technology of Cemented Carbide," Rare Metals and Cemented Carbides, no. 6, pp. 46-48, 2014. keywords: {cemented carbide extrusion molding molding binder production technology} |