Study on Process and Kinetics of Oxygen-Pressure Water Leaching of Molybdenite Concentrate AITranslate
Abstract AITranslate
Orthogonal experiments were used to determine the optimal process conditions for oxygen-pressure water leaching of molybdenite concentrate,and the kinetics study of MoS2 oxidative decomposition reaction during oxygen-pressure water leaching was carried out under the optimal process conditions.The results show that under the optimal conditions of ore particle size D90=46 μm,oxygen pressure of 1.1 MPa,temperature of 230 ℃,liquid-solid ratio of 7∶1,and reaction time of 1 h,the highest molybdenum conversion ratio can reach 99.77%,with the copper leaching ratio of 97.56%,and the iron leaching ratio of 88.71%.Within the leaching temperature range of 170~230 ℃(other process conditions are set at the above-mentioned optimal values),the oxidative decomposition reaction of MoS2 in molybdenite concentrate follows the unreacted nucleus shrinking model and is primarily controlled by chemical reaction with an apparent activation energy of 45.71 kJ/mol.
KeyWords AITranslate
1袁雨瑾,肖习羽,李青松,李玉瑛,吴俊文,戴惠林.VUV/UV/NaClO及UV/NaClO去除百里香酚:降解机制及水质影响因素[J].高校化学工程学报,2024,38(2):328-340.
2邹旬,刘冠男,王同尧,郭利,张玉,翟明.高温热解生物质焦含氧结构演变规律研究[J].节能技术,2024,42(3):200-203.
3朱若璇,刘睿莹,谢婧,陈香香,王志远,曹振.Co_(0.6)Ni_(0.4)/NC催化剂的制备及其催化氨硼烷水解制氢性能研究[J].石油炼制与化工,2024,55(7):69-76.
4马海飞,廖亚龙,武敏,贾小宝,杨双宇.湿法炼铜浸出液萃取分离硫酸机理[J].化工进展,2024,43(6):3410-3419.
5温珊,易娟,吴旭.锌铜合金灰选择性浸出分离回收铜试验研究[J].有色金属工程,2024,14(6):76-83.
6李恒,田保红,周孟,马紫鹏,景柯,刘勇.Al_(2)O_(3)-Cu/25Cr复合材料的热变形行为与热加工图[J].材料热处理学报,2024,45(6):139-146.
7李扬,李杰,程文婷.混酸协同浸出火电行业废脱硝催化剂中钒的实验研究[J].电力科技与环保,2024,40(3):304-312.
8曹国鑫,董建新,张胜,姚志浩,解国良,聂志华,马腾飞,付宝全.超高W含量NiW中/重合金热加工行为研究[J].稀有金属材料与工程,2024,53(5):1371-1377.
9钱雪雅,温博伦,王乐乐,刘慧姝,张国正.HIF-1α上调Mfn1的表达促进线粒体融合在宫缩维持中的机制研究[J].中国计划生育和妇产科,2024,16(6):88-92.
10王福元,余浔,王立刚,陈少学,张帆,周峰.刚果(金)某氧化铜钴矿还原浸出试验[J].现代矿业,2024,40(5):157-160.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.2[冶金工程—有色金属冶金]
Citation Information:
Orthogonal experiments were used to determine the optimal process conditions for oxygen-pressure water leaching of molybdenite concentrate,and the kinetics study of MoS2 oxidative decomposition reaction during oxygen-pressure water leaching was carried out under the optimal process conditions.The results show that under the optimal conditions of ore particle size D90=46 μm,oxygen pressure of 1.1 MPa,temperature of 230 ℃,liquid-solid ratio of 7∶1,and reaction time of 1 h,the highest molybdenum conversion ratio can reach 99.77%,with the copper leaching ratio of 97.56%,and the iron leaching ratio of 88.71%.Within the leaching temperature range of 170~230 ℃(other process conditions are set at the above-mentioned optimal values),the oxidative decomposition reaction of MoS2 in molybdenite concentrate follows the unreacted nucleus shrinking model and is primarily controlled by chemical reaction with an apparent activation energy of 45.71 kJ/mol.
quote
| GB/T 7714-2015 | [1] PENG Yi-long, QIN Qing-wei, TONG Yi-zhe, et al. Study on Process and Kinetics of Oxygen-Pressure Water Leaching of Molybdenite Concentrate[J]. Rare Metals and Cemented Carbides, 2024(3): 1-6. |
| MLA | [1] PENG Yi-long, et al., "Study on Process and Kinetics of Oxygen-Pressure Water Leaching of Molybdenite Concentrate." Rare Metals and Cemented Carbides, no. 3, 2024, pp. 1-6. |
| APA | [1] PENG Yi-long, QIN Qing-wei, TONG Yi-zhe, & WANG Heng-hui. (2024). Study on Process and Kinetics of Oxygen-Pressure Water Leaching of Molybdenite Concentrate. Rare Metals and Cemented Carbides(3), 1-6. |
| IEEE | [1] PENG Yi-long, QIN Qing-wei, TONG Yi-zhe, and WANG Heng-hui, "Study on Process and Kinetics of Oxygen-Pressure Water Leaching of Molybdenite Concentrate," Rare Metals and Cemented Carbides, no. 3, pp. 1-6, 2024. keywords: {molybdenite concentrate;oxygen-pressure water leaching;oxidative decomposition of MoS;orthogonal experiment;kinetics} |