daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Microstructure and Properties of TiC-Reinforced Nickel-Based Gradient Coatings Generated in Situ AITranslate

School of Mechanical Engineering and Automation,Liaoning University of Technology;School of Mechanical Engineering and Automation,Liaoning University of Technology;School of Mechanical Engineering and Automation,Liaoning University of Technology;School of Mechanical Engineering and Automation,Liaoning University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

TiC-reinforced Ni-based single coatings and gradient coatings were generated in situ on the sur-face of H13 steel by laser cladding technology.The micromorphology,composition distribution,phase com-position,microhardness and frictional wear resistance of the coatings were analyzed and compared by scan-ning electron microscope,energy spectrometer,X-ray diffractometer,microhardness tester and universal friction and wear testing machine.The results show that the single coating is prone to macroscopic pores,cracks,poor bonding with the matrix and other defects,while the gradient coating can realize the gradient change of composition,microstructure and properties,and form a good metallurgical bonding with the ma-trix.Fe-Cr,TiC and other reinforcing phases generate in the gradient coating,which significantly improves the surface hardness and wear resistance of the steel.The average hardness of the gradient coating is about 1.44 times that of the single coating and about 2.58 times that of the matrix.The average wear loss of the gradient coating is 45.6%of that of single coating and 32.4%of that of the matrix.The wear mechanism of the gradient coating is mainly abrasive wear and adhesive wear.

KeyWords AITranslate

gradient coating TiC-reinforced nickel-based coating laser cladding in-situ generation micro-hardness frictional wear
No data

Basic Information:

DOI:

Chinese Library Classification Number:TG178[金属学及工艺—金属表面处理]

Citation Information:

TiC-reinforced Ni-based single coatings and gradient coatings were generated in situ on the sur-face of H13 steel by laser cladding technology.The micromorphology,composition distribution,phase com-position,microhardness and frictional wear resistance of the coatings were analyzed and compared by scan-ning electron microscope,energy spectrometer,X-ray diffractometer,microhardness tester and universal friction and wear testing machine.The results show that the single coating is prone to macroscopic pores,cracks,poor bonding with the matrix and other defects,while the gradient coating can realize the gradient change of composition,microstructure and properties,and form a good metallurgical bonding with the ma-trix.Fe-Cr,TiC and other reinforcing phases generate in the gradient coating,which significantly improves the surface hardness and wear resistance of the steel.The average hardness of the gradient coating is about 1.44 times that of the single coating and about 2.58 times that of the matrix.The average wear loss of the gradient coating is 45.6%of that of single coating and 32.4%of that of the matrix.The wear mechanism of the gradient coating is mainly abrasive wear and adhesive wear.

quote

GB/T 7714-2015 [1] LI Jin-hua, LI Xiao-xiao, YAO Fang-ping, et al. Microstructure and Properties of TiC-Reinforced Nickel-Based Gradient Coatings Generated in Situ[J]. Rare Metals and Cemented Carbides, 2024(5): 84-91.
MLA [1] LI Jin-hua, et al., "Microstructure and Properties of TiC-Reinforced Nickel-Based Gradient Coatings Generated in Situ." Rare Metals and Cemented Carbides, no. 5, 2024, pp. 84-91.
APA [1] LI Jin-hua, LI Xiao-xiao, YAO Fang-ping, & LI Xiang-xin. (2024). Microstructure and Properties of TiC-Reinforced Nickel-Based Gradient Coatings Generated in Situ. Rare Metals and Cemented Carbides(5), 84-91.
IEEE [1] LI Jin-hua, LI Xiao-xiao, YAO Fang-ping, and LI Xiang-xin, "Microstructure and Properties of TiC-Reinforced Nickel-Based Gradient Coatings Generated in Situ," Rare Metals and Cemented Carbides, no. 5, pp. 84-91, 2024. keywords: {gradient coating;TiC-reinforced nickel-based coating;laser cladding;in-situ generation;micro-hardness;frictional wear}