Latest Development of One-dimensional Nanometer-materials AITranslate
Abstract AITranslate
The paper reviews the latest development of one-dimensional nanometer structures.Description is made of the preparation of one-dimensional nanometer structures such asnanotubes,nanorods,nanowires and nanobands by chemical vapor deposition,thermal decomposition precursor,formwork synthesis and arc plasma synthesis,etc.The author has summarized its characterization,the growth mechanism and the applications in the fields of physics,chemistry,mechanics,material science.Brief description is made of the preparation of WS_2 nanofibers by thermal decomposition.
KeyWords AITranslate
1Bachtold Adrian,et al.Logic circuits with carbon nanotube transistors[J].Science,2001,294:1317.
2Iijima S.Helical microtubes of graphitic carbon[J].Nature.1991,354:56.
3李斌 等.什么是准一维纳米材料[J].机械工程师,1991,(2):27-27.
4Wang Y W,et al.Catalytic growth of semiconducting zinc oxide nanowires and their photoluminescence Properties[J].J of Crystal Growth, 2002, 234:171.
5Zhang H Z,et al.Ga2O3 nanowires prepared by physical evaporation[J].Solid State Communications,1999,109 (11):677.
6Yacaman M J,et al.Catalytic growth of carbon microtubules with fullerene structure[J].Appliediedied Physicsicsics Lettersersers,1993,62(6):657.
7Dai H,et al.Synthesis and characterization of carbide nanorodes[J].Nature,1995, 375:769.
8Endo M,et al.The production and structure of pyrolytic carbon nanotubes[J].Journal of Physics and Chemistry of Solids,1993,54(12):1 841.
9Tenne Y,et al.Bulk synthesis of inorganic fullerene-like MS2(M=Mo,W) from the respective trioxides and reaction mechanism[J].J Am Chem Soc,1996,118:5 362.
10Feldman Y,et al.High-rate gas-phase growth of MoS2 nested inorganic fullerenes and nanotubes[J].Science,1995,267(13):222.
1冯其明,杨艳霞,刘琨,肖愉.纤蛇纹石纳米纤维的制备及表征[J].中南大学学报:自然科学版,2006,37(6):1081-1086. 被引量:4
2卢义刚,王炳喜,金新颖.准一维NiO纳米材料的制备研究进展[J].兵器材料科学与工程,2007,30(3):68-72. 被引量:3
3李莉,王宝辉,童茂松.一维V_2O_5纳米材料的性质及其应用进展[J].材料工程,2007,35(12):73-78. 被引量:2
4李春梅,罗康碧,李沪萍,陈锐.硫酸钙微米/纳米材料的研究进展[J].化工科技,2009,17(4):57-60. 被引量:7
5赵婷婷.一维纳米材料的制备、表征及应用[J].广州化工,2014,42(20):24-26. 被引量:3
1宋鹏程,彭同江,孙红娟,余玉操.纤蛇纹石焙烧去金属氧化物制备纤维状二氧化硅[J].硅酸盐学报,2015,43(5):692-698. 被引量:9
2冯其明,杨艳霞,刘琨,肖愉,张国范.采用纤蛇纹石制备纳米纤维状多孔氧化硅[J].中南大学学报:自然科学版,2007,38(6):1088-1093. 被引量:13
3彭红瑞,丁洁,王宁,李桂村.钼掺杂五氧化二钒纳米带的制备及表征[J].青岛科技大学学报:自然科学版,2009,30(6):480-482. 被引量:1
4刘兰,聂福德,曾贵玉,谯志强.超音速气流粉碎下NiO纳米棒的低温固相制备[J].应用化学,2010,27(4):454-457. 被引量:1
5湛菁,邬建辉,张传福,岳建峰.形貌控制合成纤维状氧化亚镍粉末新型前驱体[J].矿冶工程,2010,30(2):64-69. 被引量:5
6杨大锦.2009年云南冶金年评[J].云南冶金,2010,39(2):37-55. 被引量:2
7周林,张家敏.2009年云南金属材料与加工年评[J].云南冶金,2010,39(2):60-69.
8湛菁,岳建峰,张传福,樊友奇.准一维镍钴合金材料的制备研究及应用现状[J].材料导报,2010,24(9):93-96. 被引量:4
9赵喆,雷鸣,肖德明,熊建义,马经野,许蕴,陈旭红,彭福宁.改性医用胶为纳米骨胶的体外实验[J].中国组织工程研究与临床康复,2010,14(47):8818-8823. 被引量:8
10王力,刘聪,庄春艳,孟德芹,方杰.不同工艺条件对球形纳米硫酸钙制备的影响[J].功能材料,2012,43(6):740-743. 被引量:1
1段兴凯,江跃珍.电弧等离子体合成Sb_2Te_3粉末材料的微结构研究[J].热加工工艺,2011,40(10):88-89. 被引量:4
2安希忠,李长兴,刘国权,沈峰满,李友清.CVD金刚石膜反应器内气相化学的理论研究进展[J].中南大学学报:自然科学版,2010,41(3):896-905.
3吴承康,潘文霞,马维.层流电弧等离子体射流的材料表面处理方法[J].科技开发动态,2004(12):41-41.
4C.Arnoult,X.Devaux,H.Rinnert,M.Vergnat.Characterization and Photoluminescence Properties of Alumina Nanowires Elaborated by Arc-Plasma[J].材料科学技术:英文版,2006,22(1):127-129. 被引量:1
5常琛,郝春成.电弧法制备的TiC催化生长碳纤维[J].青岛科技大学学报:自然科学版,2015,36(3):272-275. 被引量:2
6田亚峻,谢克昌,樊友三.用煤合成碳纳米管新方法[J].高等学校化学学报,2001,22(9):1456-1458. 被引量:18
7段兴凯,江跃珍.电弧工艺参数对合成Sb_2Te_3热电粉末材料的影响[J].热加工工艺,2011,40(12):28-30. 被引量:1
8Wei-Ming Yeoh,Kim-Yang Lee,Siang-Piao Chai,Keat-Teong Lee,Abdul Rahman Mohamed.Co-Mo/MgO催化剂上甲烷化学气相沉积制备高纯度多壁碳纳米管(英文)[J].新型炭材料,2009,24(2):119-123. 被引量:2
9朱晓东,温晓辉,詹如娟,周海洋.EACVD沉积金刚石过程中气相化学研究[J].核技术,2000,23(9):621-625. 被引量:2
10韩红梅,邱介山,周颖,朱盛伟,粱长海,李灿.碳纳米管的制备及其热稳定性和表面性质的研究[J].炭素技术,2001,20(4):5-9. 被引量:10
Basic Information:
DOI:
Chinese Library Classification Number:TB383[一般工业技术—材料科学与工程]
Citation Information:
The paper reviews the latest development of one-dimensional nanometer structures.Description is made of the preparation of one-dimensional nanometer structures such asnanotubes,nanorods,nanowires and nanobands by chemical vapor deposition,thermal decomposition precursor,formwork synthesis and arc plasma synthesis,etc.The author has summarized its characterization,the growth mechanism and the applications in the fields of physics,chemistry,mechanics,material science.Brief description is made of the preparation of WS_2 nanofibers by thermal decomposition.
quote
| GB/T 7714-2015 | [1] MA Jiang-hong, DI Yu-chun, YU Xu-guang, et al. Latest Development of One-dimensional Nanometer-materials[J]. Rare Metals and Cemented Carbides, 2004(4): 41-45. |
| MLA | [1] MA Jiang-hong, et al., "Latest Development of One-dimensional Nanometer-materials." Rare Metals and Cemented Carbides, no. 4, 2004, pp. 41-45. |
| APA | [1] MA Jiang-hong, DI Yu-chun, YU Xu-guang, & TIAN Yan-wen. (2004). Latest Development of One-dimensional Nanometer-materials. Rare Metals and Cemented Carbides(4), 41-45. |
| IEEE | [1] MA Jiang-hong, DI Yu-chun, YU Xu-guang, and TIAN Yan-wen, "Latest Development of One-dimensional Nanometer-materials," Rare Metals and Cemented Carbides, no. 4, pp. 41-45, 2004. keywords: {one-dimensional nanometer material;preparation method;growthmechanism;application;WS_2 nanofiber} |