Investigation on TiNiLaZr Alloy Film Coated by Magnetron Sputter and Their Electro-chemical Property AITranslate
Abstract AITranslate
In this paper, the Tio. 56Ni0. 37La0. 02Zr0. 05 and Tio. 53Ni0. 38La0. 09 alloy film was made by magnetron sputter. The results show that the maximum electro-chemical capacity of the former is 243mAh/g, about 30% higher than the latter.
KeyWords AITranslate
1王春生,雷永泉.Ti—Ni系贮氢电极[J].稀有金属材料与工程,1994,23(5):1-8. 被引量:5
2钱久信,张亚文,陈旭东.TiFe+xwt-%La合金吸氢性能研究[J].金属学报,1992,28(4). 被引量:2
1陈红,王庆伟,别晓非,杜菲,王春忠,寇春雷.立方晶系Li_(0.29)Ni_(0.71)O的电化学性质[J].吉林大学学报:理学版,2013,51(1):120-123.
2吕成学,褚嘉宜,翟玉春,田彦文.锂离子电池锡基复合氧化物负极材料的研究[J].分子科学学报,2004,20(4):31-34. 被引量:7
3泡沫镍的应用[J].金川科技,2005(4):11-11.
4牟宗信,李国卿,郭宝海,孙俊才,季世军.Ti-Ni非晶合金贮氢薄膜制备及电化学性能研究[J].金属功能材料,1999,6(1):25-28. 被引量:4
5冯艳,袁华堂,乔林军,刘强.Mg_(0.9)M_(0.1)Ni(M=Cr,Al,Ti,Zr)三元镁基储氢合金的制备及其电化学性能的研究[J].南开大学学报:自然科学版,2005,38(2):74-79. 被引量:5
6李蓉,吴建民,周少雄,钱九红.钴含量和制备方法对AB_5型储氢合金不同温度电化学容量的影响[J].中国稀土学报,2006,24(3):356-356.
7牟宗信,林国强,李国卿.阴极电弧法制备Ti-Ni合金贮氢薄膜及其性能研究[J].大连理工大学学报,2001,41(5):527-529.
Basic Information:
DOI:
Chinese Library Classification Number:O484[理学—固体物理];TG146.23[金属学及工艺—金属材料]
Citation Information:
In this paper, the Tio. 56Ni0. 37La0. 02Zr0. 05 and Tio. 53Ni0. 38La0. 09 alloy film was made by magnetron sputter. The results show that the maximum electro-chemical capacity of the former is 243mAh/g, about 30% higher than the latter.
quote
| GB/T 7714-2015 | [1] ZHANG Dong-ming, ZHANG Qiao-xin. Investigation on TiNiLaZr Alloy Film Coated by Magnetron Sputter and Their Electro-chemical Property[J]. Rare Metals and Cemented Carbides, 1998(1): 25-27. |
| MLA | [1] ZHANG Dong-ming, and ZHANG Qiao-xin. "Investigation on TiNiLaZr Alloy Film Coated by Magnetron Sputter and Their Electro-chemical Property." Rare Metals and Cemented Carbides, no. 1, 1998, pp. 25-27. |
| APA | [1] ZHANG Dong-ming, & ZHANG Qiao-xin. (1998). Investigation on TiNiLaZr Alloy Film Coated by Magnetron Sputter and Their Electro-chemical Property. Rare Metals and Cemented Carbides(1), 25-27. |
| IEEE | [1] ZHANG Dong-ming and ZHANG Qiao-xin, "Investigation on TiNiLaZr Alloy Film Coated by Magnetron Sputter and Their Electro-chemical Property," Rare Metals and Cemented Carbides, no. 1, pp. 25-27, 1998. keywords: {magnetron sputter;alloy film preparation;electrol-chemical property} |