daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study of the Adsorption Behavior of C-900 Amino Phosphonic Acid Resin for Vanadium(Ⅳ) AITranslate

Hunan Provincial Product Quality Supervision and Inspection Institute;Hunan Provincial Product Quality Supervision and Inspection Institute;Hunan Provincial Product Quality Supervision and Inspection Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The optimum adsorption conditions of vanadium(Ⅳ) were determined by static and dynamic adsorption experiments.The results from static adsorption experiment show that the static saturated adsorption capacity of vanadium(Ⅳ) is 203.67 mg/g at pH2.0,resin amount 1 g and temperature 60 ℃.The results from dynamic adsorption experiment show that low flow rate and relatively high temperature are good for resin adsorption of vanadium(Ⅳ).

KeyWords AITranslate

amino phoshonic acid resin static adsorption dynamic adsorption vanadium ion

1陆芝华,周邦娜,余仲兴,陈世.石煤氧化焙烧-稀碱溶液浸出提钒工艺研究[J].稀有金属,1994,18(5):321-327. 被引量:24

2Deleon A. Proceeding of the Second International Symposium of Icsoba[M].Moscow:Russian,1971.359.

3焦芸芬,何小林,廖春发,姜平国.氨基膦酸螯合树脂吸附重稀土的研究[J].离子交换与吸附,2009,25(4):306-312. 被引量:11

4杨丽梅,李玲,黄松涛,武名麟,刘美林.氨基膦酸型螯合树脂对水溶液中Ni^(2+),Fe^(2+),Fe^(3+)吸附行为的研究[J].稀有金属,2009,33(3):401-405. 被引量:10

5张启伟,熊春华.氨基膦酸树脂对汞的吸附性能及其机理[J].离子交换与吸附,2003,19(6):525-531. 被引量:17

6张启伟,王桂仙.氨基膦酸树脂对汞、铅混合液的吸附研究[J].江西师范大学学报:自然科学版,2004,28(4):355-357. 被引量:7

7张启伟,王桂仙.氨基膦酸树脂对铜的吸附性能研究[J].河北师范大学学报:自然科学版,2006,30(1):75-78. 被引量:6

8施林妹,莫建军,熊春华.氨基膦酸树脂吸附钴的研究[J].有色金属,2003,55(1):86-89. 被引量:13

9王惠君,高伟彪,孙静亚.氨基膦酸树脂吸附镍(Ⅱ)的反应机理探讨[J].浙江海洋学院学报:自然科学版,2003,22(4):336-339. 被引量:12

10莫建军,熊春华,王永江.氨基膦酸树脂吸附锌的研究[J].有色金属,2002,54(1):27-29. 被引量:4

1焦芸芬,何小林,姜平国.D418氨基膦酸螯合树脂吸附铥镱镥混合稀土离子的机理研究[J].有色金属:冶炼部分,2014(2):39-42. 被引量:2

2张一敏,包申旭.含钒浸出液净化富集技术现状及前景[J].金属矿山,2016,45(7):64-70. 被引量:9

3段继华,包申旭,张一敏,周嘉郁.D860树脂对V(Ⅳ)的吸附性能研究[J].有色金属:冶炼部分,2016,0(12):32-36. 被引量:6

4罗大双,黄晶,张一敏,刘红,刘涛.N235-煤油支撑液膜体系中钒萃取分离性能研究[J].有色金属:冶炼部分,2018(6):33-38. 被引量:6

5谢凯明,陶媛媛,张娅,项朋志.吸附法回收除去钒研究进展[J].广州化工,2021,49(5):50-53.

6朱思琴,叶国华,亢选雄,梁雪崟.含钒酸浸液净化与富集的研究进展[J].钢铁钒钛,2022,43(5):10-22. 被引量:1

1焦芸芬,余党华,何小林,苏佳,刘庆生,王宗俊.稀土冶炼含C_2O_4^(2-)废水的治理与回收利用技术[J].中国资源综合利用,2016,34(7):41-44. 被引量:2

2吴广强,贾建福,付建建,刘华朋,于兆强.改性树脂脱除焦化蜡油中碱氮物及安全性分析[J].当代化工,2016,45(12):2743-2746. 被引量:2

3郑汝伟,包申旭,张一敏,杨晓.CL-P204萃淋树脂对溶液中钒的吸附性能研究[J].有色金属:冶炼部分,2017(1):45-48. 被引量:7

4王魁,张一敏,黄晶,刘涛,汪劲鹏.扩散渗析法应用于石煤提钒酸浸液预处理研究[J].有色金属:冶炼部分,2017(4):39-44.

5陈波,包申旭,张一敏.N235浸渍树脂的制备及对钒的吸附研究[J].稀有金属,2018,42(8):891-896. 被引量:9

6郑巧巧,张一敏,黄晶,包申旭.吹脱—离子交换耦合工艺处理页岩提钒高浓度氨氮废水研究[J].有色金属:冶炼部分,2019,0(6):67-71. 被引量:9

7杨海,黄新,林子增,何秋玫,丁炜.离子交换法处理重金属废水的研究进展[J].应用化工,2019,48(7):1675-1680. 被引量:34

8何野,黄晶,张一敏,刘红,胡鹏程,罗大双.Mextral 984H从页岩提钒浸出液中萃取V(Ⅴ)的研究[J].有色金属:冶炼部分,2019,0(10):33-38. 被引量:4

9刘子帅,张一敏,戴子林,刘聪.N235萃取法从钒钛磁铁矿沉钒废水中回收钒[J].有色金属:冶炼部分,2019,0(11):87-92. 被引量:11

10谢伟芳,阮小燕,程婷,戚琳,吴先亮,黄先飞.Keggin离子改性凹凸棒土去除水溶液中Zn(Ⅱ)的研究[J].有色金属:冶炼部分,2019,0(11):93-98. 被引量:2

1黄慧敏,陈惠,司士辉,邓春艳.某螯合树脂对钒(Ⅳ)离子的吸附行为研究[J].稀有金属与硬质合金,2012,40(1):18-20. 被引量:1

2刘树惠.碳还原后的氧化轨中钒(Ⅲ)钒(Ⅳ)钒(Ⅴ)的测定[J].钢铁钒钛,1989,10(4):67-70. 被引量:2

3Б.,ЛХ,国强.用二—2—乙基己基磷酸从硫酸溶液中萃取钒(Ⅳ)的动力学[J].钒钛,1990(4):3-5.

4刘玉鑫,王槐三,邱陵,贾东方,林雪,何炳林.TMB对模拟氰化液中AU(Ⅰ)的静态吸附选择性的影响[J].黄金,1992,13(8):36-40. 被引量:2

5А.,ЗИ,汪镜亮.在有苏打的还原介质中钒(Ⅲ)的氧化[J].钒钛,1992(5):21-23.

6阳亚玲,颜文斌,高峰.离子交换树脂分离钒渣浸出液中钒与铬[J].过程工程学报,2017,17(1):84-91. 被引量:6

7李尚勇,谢刚,俞小花.从含钒浸出液中萃取钒的研究现状[J].有色金属,2011,63(1):100-104. 被引量:22

8范保建,佐太东.氰化炭浆工艺浓密回水活性炭吸附生产实践[J].黄金,2016,37(11):55-57. 被引量:3

9Ipin.,KO,许孙曲.在化学动力学控制区内萃取钒(Ⅳ)的机理[J].钒钛,1991(3):10-13. 被引量:1

10丁瑞锋,刘桂华.溶液中钒分离富集技术的研究进展[J].湖南有色金属,2011,27(3):15-19. 被引量:8

Basic Information:

DOI:

Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]

Citation Information:

The optimum adsorption conditions of vanadium(Ⅳ) were determined by static and dynamic adsorption experiments.The results from static adsorption experiment show that the static saturated adsorption capacity of vanadium(Ⅳ) is 203.67 mg/g at pH2.0,resin amount 1 g and temperature 60 ℃.The results from dynamic adsorption experiment show that low flow rate and relatively high temperature are good for resin adsorption of vanadium(Ⅳ).

quote

GB/T 7714-2015 [1] CENG Xiao-ming, HUANG Hui-min, SI Shi-hui. Study of the Adsorption Behavior of C-900 Amino Phosphonic Acid Resin for Vanadium(Ⅳ)[J]. Rare Metals and Cemented Carbides, 2012(2): 6-9.
MLA [1] CENG Xiao-ming, et al., "Study of the Adsorption Behavior of C-900 Amino Phosphonic Acid Resin for Vanadium(Ⅳ)." Rare Metals and Cemented Carbides, no. 2, 2012, pp. 6-9.
APA [1] CENG Xiao-ming, HUANG Hui-min, & SI Shi-hui. (2012). Study of the Adsorption Behavior of C-900 Amino Phosphonic Acid Resin for Vanadium(Ⅳ). Rare Metals and Cemented Carbides(2), 6-9.
IEEE [1] CENG Xiao-ming, HUANG Hui-min, and SI Shi-hui, "Study of the Adsorption Behavior of C-900 Amino Phosphonic Acid Resin for Vanadium(Ⅳ)," Rare Metals and Cemented Carbides, no. 2, pp. 6-9, 2012. keywords: {amino phoshonic acid resin;static adsorption;dynamic adsorption;vanadium ion}