One-Step Formation of Plasmonic Cu Nanodomains in p-Type Cu2O Matrix Films for Enhanced Photoconversion of n-ZnO/p-Cu2O Heterojunctions One-Step Formation of Plasmonic Cu Nanodomains in p-Type Cu2O Matrix Films for Enhanced Photoconversion of n-ZnO/p-Cu2O Heterojunctions AITranslate

University of Havana; University of Havana;Université de Lorraine;Université de Lorraine;Université de Lorraine;Université de Lorraine;Université de Lorraine
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Plasmonic Cu nanoparticles were in situ grown into a Cu2O semiconductor matrix by using reactive magnetron sputtering and adjusting the amount of oxygen available during the synthesis in order to prevent the oxidation of part of the copper atoms landing on the film surface. Varying only the oxygen flow rate (OFR) and using a single Cu target, it was possible to observe the evolution in the simultaneous formation of metallic Cu and Cu2O phases for oxygen-poor conditions. Such formation is accompanied by the development of the surface plasmon band (SPB) corresponding to Cu, as evidenced by UV–vis spectrophotometry and spectroscopic ellipsometry. The bandgap values of the elaborated composites containing embedded Cu plasmonic nanodomains were lower than the bandgap of single-phase Cu2O films, likely due to the higher defect density associated with the nanocrystalline nature of films promoted by the presence of metallic Cu. The resistivity of the thin films increased with more oxidative deposition conditions and was associated with an increase in Cu2O/Cu ratio and smaller and more isolated Cu particles, as evidenced by high-resolution transmission electron microscopy and X-ray diffraction. Photoconversion devices based on the studied nanocomposites were characterized by I–V and spectral photocurrent measurements, showing an increase in the photocurrent density under light illumination as a consequence of the plasmonic particle excitation leading to hot carrier injection in the nearby ZnO and Cu2O semiconductors.

KeyWords AITranslate

copper nanodomains localized surface plasmon resonance reactive magnetron sputtering surface plasmon band hot carriersShow More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01132

Chinese Library Classification Number:

Citation Information:

Plasmonic Cu nanoparticles were in situ grown into a Cu2O semiconductor matrix by using reactive magnetron sputtering and adjusting the amount of oxygen available during the synthesis in order to prevent the oxidation of part of the copper atoms landing on the film surface. Varying only the oxygen flow rate (OFR) and using a single Cu target, it was possible to observe the evolution in the simultaneous formation of metallic Cu and Cu2O phases for oxygen-poor conditions. Such formation is accompanied by the development of the surface plasmon band (SPB) corresponding to Cu, as evidenced by UV–vis spectrophotometry and spectroscopic ellipsometry. The bandgap values of the elaborated composites containing embedded Cu plasmonic nanodomains were lower than the bandgap of single-phase Cu2O films, likely due to the higher defect density associated with the nanocrystalline nature of films promoted by the presence of metallic Cu. The resistivity of the thin films increased with more oxidative deposition conditions and was associated with an increase in Cu2O/Cu ratio and smaller and more isolated Cu particles, as evidenced by high-resolution transmission electron microscopy and X-ray diffraction. Photoconversion devices based on the studied nanocomposites were characterized by I–V and spectral photocurrent measurements, showing an increase in the photocurrent density under light illumination as a consequence of the plasmonic particle excitation leading to hot carrier injection in the nearby ZnO and Cu2O semiconductors.

quote

GB/T 7714-2015 [1] Yerila RodríguezMartínez, Lídice VaillantRoca, Jaafar Ghanbaja, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01132.
MLA [1] Yerila RodríguezMartínez, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01132.
APA [1] Yerila RodríguezMartínez, Lídice VaillantRoca, Jaafar Ghanbaja, Sylvie Migot, Yann Battie, Sidi Ould Saad Hamady, & David Horwat. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01132
IEEE [1] Yerila RodríguezMartínez, Lídice VaillantRoca, Jaafar Ghanbaja, Sylvie Migot, Yann Battie, Sidi Ould Saad Hamady, and David Horwat, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01132. keywords: {copper nanodomains localized surface plasmon resonance reactive magnetron sputtering surface plasmon band hot carriersShow More}