Preparation Technology and Development Trend of Ultra-Coarse Grained WC-Co Cemented Carbides AITranslate
Abstract AITranslate
Ultra-coarse grained cemented carbides have attracted much attention because of its unique microstructure characteristics in the field of cemented carbide,showing good impact resistance,wear resistance,thermal fatigue resistance,and other advantages,and have great development potential in rock drilling,stamping die,and hot rolling.This paper summarizes the characteristics and the toughening mechanism of the ultra-coarse grained cemented carbides,and introduces the current preparation of coarse-grained WC raw powders and ultra-coarse grained cemented carbides,as well as the exploration situation of the strengthening method of the ultra-coarse grained cemented carbides.Finally,some thoughts about the development trend of the ultra-coarse grained cemented carbides are put forward.
KeyWords AITranslate
1黄伯云,韦伟峰,李松林,张立,李丽娅,刘锋,李瑞迪.现代粉末冶金材料与技术进展[J].中国有色金属学报,2019,29(9):1917-1933. 被引量:38
2孙东平,夏斌华.超粗晶粒凿岩硬质合金研究的新进展[J].凿岩机械气动工具,2009,35(4):41-46. 被引量:14
3吴厚平,张立,王元杰,黄伯云,程鑫.化学包裹粉工艺制备粗晶粒WC-Co硬质合金[J].中国有色金属学报,2010,20(4):701-705. 被引量:19
4蔡海燕.超粗晶硬质合金的研究现状与发展趋势[J].硬质合金,2018,35(4):297-303. 被引量:10
5高德强,刘雪梅,冯浩,孙婷,刘超,宋晓艳.超粗晶WC-8Co硬质合金循环压缩过程中组织演变的研究[J].中国体视学与图像分析,2020(2):135-143. 被引量:2
6张立,程鑫,陈述,马鋆,吴厚平,熊湘君.Cr、V、RE添加剂对特粗晶与超粗晶硬质合金微观组织与性能的影响[J].中国有色金属学报,2012,22(9):2620-2625. 被引量:9
7孙五四,伏坤,李行,粟一峰,周建华.超粗晶WC粉的制备工艺研究[J].稀有金属与硬质合金,2016,44(2):13-17. 被引量:5
8谢俊杰,张龙辉,常卿卿,黄一春.掺杂与湿氢工艺制备超粗钨粉及其对合金性能的影响[J].硬质合金,2018,35(1):37-43. 被引量:3
9谭征,刘咏,贡太敏.Na元素掺杂方式对超粗晶碳化钨及其合金性能的影响[J].中国锰业,2017,35(2):108-112. 被引量:4
10李勇,谢淑华.粗晶硬质合金的研究现状及其发展前景[J].江西冶金,2008,28(6):42-46. 被引量:8
1王晨,刘雪梅,吕皓,宋晓艳.含添加剂形成相硬质合金的制备及界面结合强度评估[J].中国体视学与图像分析,2022,27(1):1-8.
2来金晶.基于现代学徒制的校企协同育人探索与实践[J].中文科技期刊数据库(全文版)教育科学,2021(9):0329-0330.
3高福海.中学体育教学中分层教学法的应用途径探索[J].中文科技期刊数据库(全文版)教育科学,2021(9):0181-0182.
4郑丽娟.农村地区九年级化学教材分析与教学建议[J].中文科技期刊数据库(引文版)教育科学,2022(3):0102-0105.
5顾金宝,刁椿珉,时凯华,高建,董定乾,张文科,曾伟,董凯林.包覆法制备超粗及特粗晶硬质合金研究进展[J].四川冶金,2023,45(1):6-11.
6张世良,刘伯恩,李青青.关于完善省级自然资源督察制度的若干思考[J].中国国土资源经济,2023,36(2):47-54. 被引量:4
7袁玉兰,刘含莲,黄传真,刘洋,王利梅,季良刚.Cr_(3)C_(2)含量对热压烧结WC基硬质合金材料微观组织和力学性能的影响[J].粉末冶金材料科学与工程,2023,28(1):55-62.
8沈吴毅,赵鸿金,田海霞.钴铁镍复合黏结相超细硬质合金显微组织与性能[J].有色金属科学与工程,2023,14(1):86-98.
9杨宗辉,沈以赴,张旭,李晓泉.核聚变堆钨/钢复合结构连接的研究现状[J].机械工程材料,2022,46(12):9-17.
10王芳.“课程思政”与二维动画技术课程教学的融合探索[J].中文科技期刊数据库(全文版)社会科学,2021(9):0060-0061.
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
Ultra-coarse grained cemented carbides have attracted much attention because of its unique microstructure characteristics in the field of cemented carbide,showing good impact resistance,wear resistance,thermal fatigue resistance,and other advantages,and have great development potential in rock drilling,stamping die,and hot rolling.This paper summarizes the characteristics and the toughening mechanism of the ultra-coarse grained cemented carbides,and introduces the current preparation of coarse-grained WC raw powders and ultra-coarse grained cemented carbides,as well as the exploration situation of the strengthening method of the ultra-coarse grained cemented carbides.Finally,some thoughts about the development trend of the ultra-coarse grained cemented carbides are put forward.
quote
| GB/T 7714-2015 | [1] ZHANG Wen-ke, GU Jin-bao, SHI Kai-hua, et al. Preparation Technology and Development Trend of Ultra-Coarse Grained WC-Co Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2023(1): 97-101. |
| MLA | [1] ZHANG Wen-ke, et al., "Preparation Technology and Development Trend of Ultra-Coarse Grained WC-Co Cemented Carbides." Rare Metals and Cemented Carbides, no. 1, 2023, pp. 97-101. |
| APA | [1] ZHANG Wen-ke, GU Jin-bao, SHI Kai-hua, DONG Ding-qian, XIANG Xin, XIONG Xiao, HE Feng-yuan, LIAO Jun, & ZHANG Li. (2023). Preparation Technology and Development Trend of Ultra-Coarse Grained WC-Co Cemented Carbides. Rare Metals and Cemented Carbides(1), 97-101. |
| IEEE | [1] ZHANG Wen-ke, GU Jin-bao, SHI Kai-hua, DONG Ding-qian, XIANG Xin, XIONG Xiao, HE Feng-yuan, LIAO Jun, and ZHANG Li, "Preparation Technology and Development Trend of Ultra-Coarse Grained WC-Co Cemented Carbides," Rare Metals and Cemented Carbides, no. 1, pp. 97-101, 2023. keywords: {ultra-coarse grained WC-Co cemented carbide;WC powder;preparation technology;mechanical property} |