Abstract AITranslate

Transformation of multifunctional homogeneous catalysts to the corresponding heterogeneous catalytic systems makes catalytic reactions interesting from both economic and environmental points of view. Here, we have devised a controllable and efficient strategy for the preparation of supported multifunctional catalysts by taking the Cu/2,2,6,6-tetramethyl-1-piperidine-N-oxyl (TEMPO) catalytic system as an example. Polystyrene-supported Cu/TEMPO catalysts were, for the first time, prepared via nanoprecipitation of polymers in water and efficient for aerobic oxidation of benzyl alcohol (BnOH). Cooperative behaviors could be regulated by precise control of local concentrations of functional groups. We have demonstrated that the incorporation of functional groups into polystyrene supports can make better use of catalytic components, resulting from confinement-enhanced cooperation. This strategy provides access to build more efficient multifunctional heterogeneous catalysts through establishing structure–activity relationships.

KeyWords AITranslate

multifunctional catalyst cooperative behavior nanoprecipitation aerobic oxidation polystyrene
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00909

Chinese Library Classification Number:

Citation Information:

Transformation of multifunctional homogeneous catalysts to the corresponding heterogeneous catalytic systems makes catalytic reactions interesting from both economic and environmental points of view. Here, we have devised a controllable and efficient strategy for the preparation of supported multifunctional catalysts by taking the Cu/2,2,6,6-tetramethyl-1-piperidine-N-oxyl (TEMPO) catalytic system as an example. Polystyrene-supported Cu/TEMPO catalysts were, for the first time, prepared via nanoprecipitation of polymers in water and efficient for aerobic oxidation of benzyl alcohol (BnOH). Cooperative behaviors could be regulated by precise control of local concentrations of functional groups. We have demonstrated that the incorporation of functional groups into polystyrene supports can make better use of catalytic components, resulting from confinement-enhanced cooperation. This strategy provides access to build more efficient multifunctional heterogeneous catalysts through establishing structure–activity relationships.

quote

GB/T 7714-2015 [1] Tianyou Chen, Zihao Wang, Wei Xiao, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00909.
MLA [1] Tianyou Chen, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00909.
APA [1] Tianyou Chen, Zihao Wang, Wei Xiao, Changfeng Yi, & Zushun Xu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00909
IEEE [1] Tianyou Chen, Zihao Wang, Wei Xiao, Changfeng Yi, and Zushun Xu, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00909. keywords: {multifunctional catalyst;cooperative behavior;nanoprecipitation;aerobic oxidation;polystyrene}