Change of China's Tungsten Resource and the Current Decomposing Technology AITranslate
Abstract AITranslate
The change of tungsten resource and the current decomposing technology inour country were summarized in this paper. It was shown that the tungsten resource hasbeen changed structurally in recently. According to this change, it is essential that the current process in our country's tungsten plants must be upgraded with advanced technology.
KeyWords AITranslate
1廖贡越,严培生,林中梁.热球磨碱分解技术在我厂的应用[J].中国钨业,1992(12):13-17. 被引量:1
2盛继福.我国钨矿资源形势[J].中国钨业,1992(9):5-9. 被引量:4
3孙培梅,李洪桂,刘茂盛.选冶联合法处理钨矿物原料的效益分析[J]稀有金属与硬质合金,1988(01).
4Honggui Li,Maosheng Liu,Peimei Sun,Yunjiao Li. Caustic decomposition of scheelite and scheelite-wolframite concentrates through mechanical activation[J] 1995,Journal of Central South University of Technology(2):16~20
1李军,谢金明,龙水秀.黑白钨混合矿碱分解试验研究[J].江西有色金属,2008,22(3):19-21. 被引量:4
2张立,陶小平.粗颗粒碳化钨粉制取过程中的质量控制[J].硬质合金,2000,17(1):26-29. 被引量:5
3后宝明.热压浸出法从黑白钨精矿中浸出钨的试验研究[J].矿冶,2012,21(4):73-77. 被引量:2
4李玲.高纯粉状钨酸制备工艺的研究[J].硬质合金,2000,17(4):208-213. 被引量:1
5李停停,钟祥熙,张威,张津,沈岩柏,魏德洲.白钨矿浸出工艺现状及发展趋势[J].金属矿山,2017,46(10):128-134. 被引量:8
6李俊杰,何德文,周康根,龚丹丹.钨渣综合利用研究现状[J].矿产保护与利用,2019,39(3):125-132. 被引量:8
7何德文,李俊杰,周康根,陈伟,龚丹丹.白钨矿焙烧转料的氢氧化钠浸出动力学研究[J].稀有金属,2022,46(7):926-934.
1何宪峰,石建华.优质粗晶WC碳化工艺研究[J].稀有金属快报,2005,24(10):28-35. 被引量:23
2黄新,孙亚丽,刘清才,颜杰,金永中.WC粉末中的生长孪晶[J].中国钨业,2005,20(6):27-30. 被引量:1
3郭圣达,羊建高,陈颢.粗晶粒WC-Co类硬质合金研究现状[J].粉末冶金工业,2011,21(4):58-63. 被引量:17
4何利华,刘旭恒,赵中伟,梁勇.钨矿物原料碱分解的理论与工艺[J].中国钨业,2012,27(2):22-27. 被引量:15
5刘文胜,龙路平,马运柱.高纯钨研究现状及制备工艺方法综述[J].粉末冶金技术,2012,30(3):223-228. 被引量:13
6黄万抚,肖良.钨矿选矿工艺研究进展[J].有色金属科学与工程,2013,4(1):57-61. 被引量:19
7谢刚,田林.2012年云南冶金年评[J].云南冶金,2013,42(2):42-55.
8孙五四,伏坤,李行,粟一峰,周建华.超粗晶WC粉的制备工艺研究[J].稀有金属与硬质合金,2016,44(2):13-17. 被引量:5
9何鲁华,沈裕军,彭俊,刘强,周小舟.从低品位锡钨混合粗精矿中提取钨[J].矿冶工程,2016,36(3):87-90.
10左珍新,高玉德.中国黑白钨混合矿选矿工艺研究进展[J].中国钨业,2016,31(3):41-45. 被引量:2
1宋杰.棒材生产线电气传动及自动化控制系统分析[J].现代冶金,2014,41(3):65-67. 被引量:3
2李东,覃昌倬.武钢炼铁工序能耗现状分析[J].炼铁,2004,23(5):48-51. 被引量:4
3段维民.低硅高碱度烧结矿工业试验的启示[J].包钢科技,1999(3):31-32.
4况百梁.新钢600m^3高炉炼铁技术进步[J].炼铁,2000,19(1):30-31.
5杨淼,张峰,李光耀.井下采矿技术的发展趋势探析[J].技术与市场,2016,23(7):231-231. 被引量:1
6汤宝军,唐文明,杨俊冬,李杰.高炉降低综合焦比的实践[J].河北冶金,2009(4):30-32.
7杨腾跃.1996年重钢三烧结生产技术进步[J].重钢技术,1997,40(2):7-11.
8茅洪祥,车哲锋.硅尘的应用现状及其开发前景[J].河北冶金,1997(4):60-64.
9岳庆光.远红外加热法在钨矿分解反应釜上的应用和改进[J].中国钨业,2000,15(5):35-36.
10蒋大军,王军荣.攀钢炼铁厂能耗现状与节能实践探索[J].冶金能源,2001,20(2):3-8. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TD954[矿业工程—选矿];TF841.1[冶金工程—有色金属冶金]
Citation Information:
The change of tungsten resource and the current decomposing technology inour country were summarized in this paper. It was shown that the tungsten resource hasbeen changed structurally in recently. According to this change, it is essential that the current process in our country's tungsten plants must be upgraded with advanced technology.
quote
| GB/T 7714-2015 | [1] LI Yun-jiao, CHEN Shi-rui. Change of China's Tungsten Resource and the Current Decomposing Technology[J]. Rare Metals and Cemented Carbides, 1997(2): 43-48. |
| MLA | [1] LI Yun-jiao, and CHEN Shi-rui. "Change of China's Tungsten Resource and the Current Decomposing Technology." Rare Metals and Cemented Carbides, no. 2, 1997, pp. 43-48. |
| APA | [1] LI Yun-jiao, & CHEN Shi-rui. (1997). Change of China's Tungsten Resource and the Current Decomposing Technology. Rare Metals and Cemented Carbides(2), 43-48. |
| IEEE | [1] LI Yun-jiao and CHEN Shi-rui, "Change of China's Tungsten Resource and the Current Decomposing Technology," Rare Metals and Cemented Carbides, no. 2, pp. 43-48, 1997. keywords: {tungsten, resource, concentrate, decomposition} |