Kill Two Birds with One Stone: Multifunctional Porous SiOC–Fe2O3 Composite for Li Ion Energy Conversion and Electromagnetic Wave Absorption Kill Two Birds with One Stone: Multifunctional Porous SiOC–Fe2O3 Composite for Li Ion Energy Conversion and Electromagnetic Wave Absorption AITranslate
Abstract AITranslate
It is necessary to design a scalable composite material with a rational structure for Li-ion batteries and electromagnetic wave absorption. Herein, we developed a modified precursor-driven method of spacer-assisted oxidation to prepare heterogeneous multi-interface SiOC-based composite ceramic nanoparticles. The outstanding structural design regulated by the ratio of raw materials tailored its functional potential in the fields of Li-ion batteries and electromagnetic wave absorption. The addition of a small amount of iron-sol produced small-sized ceramic nanoparticles bridged by carbon ribbons, which can provide efficient charge transfer kinetics and volumetric buffering capacity. Used in Li-ion battery anodes, it exhibited a specific discharge capacity of 514.4 mAh/g after 1000 cycles at a current density of 0.5 A/g with durable long cycling performance. In addition, the addition of high iron-sol induced the formation of porous core–shell nanoparticles and performed excellent electromagnetic wave absorption ability. The ceramic nanoparticles with carbon content of about 30% had the lowest reflection loss in the X-band of −55.5 dB, and the effective absorption range was 8.48–12.4 GHz, which basically covered the entire X-band. This strategy enriches the preparation and application of multifunctional composite ceramic nanoparticles.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01305
Chinese Library Classification Number:
Citation Information:
It is necessary to design a scalable composite material with a rational structure for Li-ion batteries and electromagnetic wave absorption. Herein, we developed a modified precursor-driven method of spacer-assisted oxidation to prepare heterogeneous multi-interface SiOC-based composite ceramic nanoparticles. The outstanding structural design regulated by the ratio of raw materials tailored its functional potential in the fields of Li-ion batteries and electromagnetic wave absorption. The addition of a small amount of iron-sol produced small-sized ceramic nanoparticles bridged by carbon ribbons, which can provide efficient charge transfer kinetics and volumetric buffering capacity. Used in Li-ion battery anodes, it exhibited a specific discharge capacity of 514.4 mAh/g after 1000 cycles at a current density of 0.5 A/g with durable long cycling performance. In addition, the addition of high iron-sol induced the formation of porous core–shell nanoparticles and performed excellent electromagnetic wave absorption ability. The ceramic nanoparticles with carbon content of about 30% had the lowest reflection loss in the X-band of −55.5 dB, and the effective absorption range was 8.48–12.4 GHz, which basically covered the entire X-band. This strategy enriches the preparation and application of multifunctional composite ceramic nanoparticles.
quote
| GB/T 7714-2015 | [1] Chao Liu, Pengfei Wu, Shaohong Chen, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01305. |
| MLA | [1] Chao Liu, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01305. |
| APA | [1] Chao Liu, Pengfei Wu, Shaohong Chen, Zhiming Su, Sambhav Vishwakarma, Xiaoxin Guo, Zhicheng Zheng, Jiayang Yu, Shucai Wen, Sujiang Xu, Binbin Xu, Anhua Liu, & Zhaoju Yu. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01305 |
| IEEE | [1] Chao Liu, Pengfei Wu, Shaohong Chen, Zhiming Su, Sambhav Vishwakarma, Xiaoxin Guo, Zhicheng Zheng, Jiayang Yu, Shucai Wen, Sujiang Xu, Binbin Xu, Anhua Liu, and Zhaoju Yu, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01305. keywords: {SiOCbased ceramic composite porous structure carbon ribbon lithiumion battery electromagnetic wave absorption} |