daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Experimental Study on Roasting-Leaching of Vanadium-bearing Carbonaceous Shale Blended with Na_2CO_3 AITranslate

School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Experimental study was made on the influence of Na2CO3 as the additive and leaching agent on roasting-leaching of vanadium-bearing carbonaceous shale from Hunan.The results show that vanadium leaching rate changes with different roasting temperature and time and Na2CO3 dosage.The optimal roasting conditions are 800 ℃×2h and 2% Na2CO3 relative to the amount of ore.

KeyWords AITranslate

vanadium-bearing carbonaceous shale vanadium extraction mixed roasting Na2CO3 leaching

1宁顺明,马荣骏.我国石煤提钒的技术开发及努力方向[J].矿冶工程,2012,32(5):57-61. 被引量:25

2雷辉,陈建梅,胡盛强,胡蓝双,高峰,颜文斌.复合添加剂对石煤提钒焙烧与浸出工艺研究[J].无机盐工业,2012,44(1):33-36. 被引量:13

3李建华,张一敏,刘涛,黄晶,陆岷,杨建祥.石煤提钒钠化焙烧过程复合添加剂的研究[J].矿业快报,2008,24(4):43-45. 被引量:12

4蔡晋强.石煤提钒在湖南的发展[J].稀有金属与硬质合金,2001,29(1):42-46. 被引量:21

5许国镇,张秀荣,尹光衡.江西玉山石煤烧结包裹与钒转化的研究[J].现代地质,1993,7(1):109-117. 被引量:9

6许国镇.氯化钠在石煤提钒中的作用[J]矿冶工程,1988(04).

7钱定福.湖北广石崖石煤钠化焙烧提钒相变机理的研究[J].矿产综合利用,1982,0(3):8-15. 被引量:6

1李文翔,王虎.钠化钒渣代替纯碱与普通钒渣混合焙烧试验[J].马钢科研,1991(1):81-84.

2刘吉波.锌阳极泥—硫化锌精矿中锰锌分离的焙烧参数研究[J].中国锰业,2014,32(3):33-35. 被引量:1

3刘斌.离析渣搭配砷渣砷灰回转窑混合焙烧脱砷[J].有色冶炼,1997(3):9-12. 被引量:1

4卤铵盐焙烧赤泥富集有价金属及综合利用方法[J].化工环保,2007,27(3):221-221.

5赵常青,雷霆,邹平,宫伟.由钛精矿直接制取富钛料新工艺煅烧条件的研究[J].云南冶金,2009,38(6):34-37.

6吴艳,赵惠民,都昱,阿衣加马力.西克然木.粉煤灰与硫酸铵混合焙烧提取氧化铝的研究[J].轻金属,2016(5):14-16. 被引量:10

7李坤林,任少龙,成丰.高钙低品位钒渣提钒试验研究[J].钢铁钒钛,2014,35(1):16-20. 被引量:2

8宫伟,雷霆,邹平,赵常青.钛渣制备高品质富钛料新工艺——焙烧条件的研究[J].云南冶金,2010,39(3):38-42. 被引量:3

9张硕,刘坤,刘广强,张睿文,赵晶.碳质石煤与生物质混合焙烧提钒工艺研究[J].钢铁钒钛,2016,37(4):14-19. 被引量:1

10李明琴,毛德明,黎文辉,陶大权.提高褐锰矿氧化率的试验研究[J].化工矿物与加工,2000,29(12):5-7.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]

Citation Information:

Experimental study was made on the influence of Na2CO3 as the additive and leaching agent on roasting-leaching of vanadium-bearing carbonaceous shale from Hunan.The results show that vanadium leaching rate changes with different roasting temperature and time and Na2CO3 dosage.The optimal roasting conditions are 800 ℃×2h and 2% Na2CO3 relative to the amount of ore.

quote

GB/T 7714-2015 [1] QI Zhao-shu, LI Qing-gang. Experimental Study on Roasting-Leaching of Vanadium-bearing Carbonaceous Shale Blended with Na_2CO_3[J]. Rare Metals and Cemented Carbides, 2015(1): 7-9.
MLA [1] QI Zhao-shu, and LI Qing-gang. "Experimental Study on Roasting-Leaching of Vanadium-bearing Carbonaceous Shale Blended with Na_2CO_3." Rare Metals and Cemented Carbides, no. 1, 2015, pp. 7-9.
APA [1] QI Zhao-shu, & LI Qing-gang. (2015). Experimental Study on Roasting-Leaching of Vanadium-bearing Carbonaceous Shale Blended with Na_2CO_3. Rare Metals and Cemented Carbides(1), 7-9.
IEEE [1] QI Zhao-shu and LI Qing-gang, "Experimental Study on Roasting-Leaching of Vanadium-bearing Carbonaceous Shale Blended with Na_2CO_3," Rare Metals and Cemented Carbides, no. 1, pp. 7-9, 2015. keywords: {vanadium-bearing carbonaceous shale;vanadium extraction;mixed roasting;Na2CO3;leaching}