Research on Cobalt Removal by Deep Purification from Zinc Pressure Leach Solution AITranslate
Abstract AITranslate
The fresh solution from the previous purification process of zinc hydrometallurgy in Danxia Smelting Plant contains a relatively high content of impurity cobalt ions, so it cannot meet the requirement for the cobalt content for the electrolysis process after zinc pressure leaching. Therefore,the cobalt ion content in the purified solution from the new process is simulated. The effects of dosage of the zinc powder,copper sulfate and antimony white on the cobalt removal are investigated by orthogonal tests. The results show that when the consumption of zinc powder, copper sulfate and antimony white is 2 g/L, 5 mg/L and 2.5 mg/L respectively,the S/N ratio of the cobalt removal is optimal and the cobalt redissolving ratio is also minimum.
KeyWords AITranslate
1虢振强.Pb-Sb-Zn合金锌粉在硫酸锌溶液净化中的应用研究[J].湖南有色金属,2006,22(2):19-21. 被引量:6
2马春来.Pb-Zn合金锌粉用于电解锌净化除钴的研究[J].有色矿冶,2006,22(3):30-33. 被引量:11
3徐采栋 林蓉 汪大成.锌冶金物理化学[M].上海:上海科学技术出版社,1978..
4马林,马逢时,杨跃进,等.六西格玛管理[M].北京:中国人民大学出版社,2003.
5李志强.逆锑深度净化工艺中添加CuSO_4的除钴效果研究[J].甘肃冶金,2003,25(B12):87-90. 被引量:4
6曾初升,司云森,余强.铜离子对硫酸锌溶液中钴返溶的影响及机理[J].南方金属,2007(1):14-16. 被引量:5
1赵光明,李向阳,张广积,杨超.铜离子在硫酸锌电解液深度净化除钴中的作用[J].过程工程学报,2010,10(3):482-487. 被引量:3
2吴钧,曾鹏,周中华,邱伟佳,张少博,杨全胜,姜艳.常规两段浸出法提高锌焙烧矿中铜回收率的研究[J].铜业工程,2022(6):74-78. 被引量:2
1孙备,张斌,阳春华,桂卫华.有色冶金净化过程建模与优化控制问题探讨[J].自动化学报,2017,43(6):880-892. 被引量:10
2王建华.贫镉液利用净化钴渣除钴的研究及生产实践[J].中国有色冶金,2020,49(1):1-3. 被引量:1
3彭情亮,黄文浩,张旭泳.福美钠应用于硫酸锌溶液除钴的试验研究[J].铜业工程,2023(3):152-158.
4刘磊,路殿坤,谢锋,郜伟,张坤坤.硫酸锌中性浸出液净化除钴[J].有色金属:冶炼部分,2023(8):9-16.
5杨明学,罗庆教,楚立军,尹延西.锌冶炼过程中浸渣加压还原酸浸除铁工艺优化[J].铜业工程,2023(4):159-164.
1李有刚,李波.锌氧压浸出工艺现状及技术进展[J].中国有色冶金,2010,39(3):26-29. 被引量:14
2张晓林.锌氧压浸出工艺中管道材料的选用[J].湖南有色金属,2009,25(1):23-25. 被引量:3
3仝一喆.锌氧压浸出工艺的应用及推广[J].矿冶,2011,20(4):94-97. 被引量:16
4骆昌运.针铁矿除铁工艺在丹霞冶炼厂的应用实践[J].有色金属工程,2011,1(3):44-46. 被引量:10
5滕年高,罗自然,徐波.改善工艺提高锌氧压浸出镓锗回收率[J].科技经济导刊,2016(18). 被引量:1
6马军,黄剑,郑良才.杭钢电炉EAF炉底石灰的应用[J].浙江冶金,2012(3):38-39. 被引量:1
7廖华,吴芳,罗爱平.废旧镍氢电池正极材料中镍和钴的回收[J].五邑大学学报:自然科学版,2003,17(1):52-56. 被引量:22
8左小红,何醒民.一段锌氧压浸出与焙烧浸出工艺的比较[J].铜业工程,2015(4):62-66. 被引量:4
9骆昌运.丹霞冶炼厂氧压浸出炼锌系统的节能措施及效果[J].有色冶金节能,2012,27(6):12-14. 被引量:3
10尹朝晖.从丹霞冶炼厂锌浸出渣中综合回收镓和锗[J].有色金属,2009,61(4):94-97. 被引量:9
Basic Information:
DOI:
Chinese Library Classification Number:TF803.25[冶金工程—有色金属冶金]
Citation Information:
The fresh solution from the previous purification process of zinc hydrometallurgy in Danxia Smelting Plant contains a relatively high content of impurity cobalt ions, so it cannot meet the requirement for the cobalt content for the electrolysis process after zinc pressure leaching. Therefore,the cobalt ion content in the purified solution from the new process is simulated. The effects of dosage of the zinc powder,copper sulfate and antimony white on the cobalt removal are investigated by orthogonal tests. The results show that when the consumption of zinc powder, copper sulfate and antimony white is 2 g/L, 5 mg/L and 2.5 mg/L respectively,the S/N ratio of the cobalt removal is optimal and the cobalt redissolving ratio is also minimum.
quote
| GB/T 7714-2015 | [1] WEN Jian. Research on Cobalt Removal by Deep Purification from Zinc Pressure Leach Solution[J]. Rare Metals and Cemented Carbides, 2009(1): 19-22. |
| MLA | [1] WEN Jian. "Research on Cobalt Removal by Deep Purification from Zinc Pressure Leach Solution." Rare Metals and Cemented Carbides, no. 1, 2009, pp. 19-22. |
| APA | [1] WEN Jian. (2009). Research on Cobalt Removal by Deep Purification from Zinc Pressure Leach Solution. Rare Metals and Cemented Carbides(1), 19-22. |
| IEEE | [1] WEN Jian, "Research on Cobalt Removal by Deep Purification from Zinc Pressure Leach Solution," Rare Metals and Cemented Carbides, no. 1, pp. 19-22, 2009. keywords: {zinc pressure leach solution;deep purification;zinc powder;copper sulfate;antimony white;cobalt removal} |