Chromatic Dendrimer/Polydiacetylene Nanoparticles AITranslate
Abstract AITranslate
Polydiacetylenes (PDAs) constitute a unique class of chromatic conjugated polymers, and their optical properties have been employed in diverse biological and chemical diagnostic applications. We constructed composite nanoparticles (NPs) comprising PDA and a dendritic amphiphilic polymer. The dendrimer/PDA NPs exhibit structural and chromatic stability and constitute an excellent platform for sensing and analysis of biomolecular membrane interactions, both in model vesicle systems and in a live-cell environment. Interestingly, the dendritic polymer shielded the PDA matrix and modulated its interactions with external stimuli such as heat and amphiphilic biomolecules. Furthermore, the dendrimer-layer-mediated association of the composite NPs with lipid bilayers in giant vesicles and live mammalian cells, thereby facilitating microscopic analysis of lipid bilayer interactions in actual membrane environments. The dendrimer/PDA NPs may serve as a broad-based vehicle for analysis of membrane interactions in diverse model and natural environments.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00053
Chinese Library Classification Number:
Citation Information:
Polydiacetylenes (PDAs) constitute a unique class of chromatic conjugated polymers, and their optical properties have been employed in diverse biological and chemical diagnostic applications. We constructed composite nanoparticles (NPs) comprising PDA and a dendritic amphiphilic polymer. The dendrimer/PDA NPs exhibit structural and chromatic stability and constitute an excellent platform for sensing and analysis of biomolecular membrane interactions, both in model vesicle systems and in a live-cell environment. Interestingly, the dendritic polymer shielded the PDA matrix and modulated its interactions with external stimuli such as heat and amphiphilic biomolecules. Furthermore, the dendrimer-layer-mediated association of the composite NPs with lipid bilayers in giant vesicles and live mammalian cells, thereby facilitating microscopic analysis of lipid bilayer interactions in actual membrane environments. The dendrimer/PDA NPs may serve as a broad-based vehicle for analysis of membrane interactions in diverse model and natural environments.
quote
| GB/T 7714-2015 | [1] Reut Israeli, Sofiya Kolusheva, Pablo MateosGil, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00053. |
| MLA | [1] Reut Israeli, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00053. |
| APA | [1] Reut Israeli, Sofiya Kolusheva, Pablo MateosGil, Electra Gizeli, & Raz Jelinek. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00053 |
| IEEE | [1] Reut Israeli, Sofiya Kolusheva, Pablo MateosGil, Electra Gizeli, and Raz Jelinek, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00053. keywords: {dendrimer;hyperbranched polymers;polydiacetylene;polymer nanoparticles;acoustic sensing;cell labeling} |