Starch Films Plasticized by Imidazolium-Based Ionic Liquids: Effect of Mono- and Dicationic Structures and Different Anions AITranslate
Abstract AITranslate
Recently, imidazole-based ionic liquids have been widely used as starch plasticizers. These salts are very effective in transforming starch, a widely available and inexpensive biopolymer, into biodegradable films with good mechanical properties and ionic conductivity. These films could have interesting applications in flexible electronics and solid polymer electrolytes. Since a wide variety of cation–anion combinations can be used, it is useful to evaluate the impact of different anion and cation structures on the properties of plasticized starch to select the most suitable ionic liquid for each specific application. In this work, starch films plasticized with imidazolium-based ionic liquids were prepared by the solution casting method. 1-Ethyl-3-methyl imidazolium was chosen as a cation and the effect of different anions such as [SO4Et]−, [N(CN)2]−, [OAc]−, and [Cl]− on the film properties was investigated. In addition, a dicationic structure, consisting of two closely bonded imidazolium rings, was also considered. The characteristics of the corresponding starch-based films were analyzed and compared with those of films prepared with monocationic ionic liquids.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01235
Chinese Library Classification Number:
Citation Information:
Recently, imidazole-based ionic liquids have been widely used as starch plasticizers. These salts are very effective in transforming starch, a widely available and inexpensive biopolymer, into biodegradable films with good mechanical properties and ionic conductivity. These films could have interesting applications in flexible electronics and solid polymer electrolytes. Since a wide variety of cation–anion combinations can be used, it is useful to evaluate the impact of different anion and cation structures on the properties of plasticized starch to select the most suitable ionic liquid for each specific application. In this work, starch films plasticized with imidazolium-based ionic liquids were prepared by the solution casting method. 1-Ethyl-3-methyl imidazolium was chosen as a cation and the effect of different anions such as [SO4Et]−, [N(CN)2]−, [OAc]−, and [Cl]− on the film properties was investigated. In addition, a dicationic structure, consisting of two closely bonded imidazolium rings, was also considered. The characteristics of the corresponding starch-based films were analyzed and compared with those of films prepared with monocationic ionic liquids.
quote
| GB/T 7714-2015 | [1] Susanna Romano, Serena De Santis, Andrea Martinelli, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01235. |
| MLA | [1] Susanna Romano, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01235. |
| APA | [1] Susanna Romano, Serena De Santis, Andrea Martinelli, Lorenzo Augusto Rocchi, Daniele Rocco, Giovanni Sotgiu, & Monica Orsini. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01235 |
| IEEE | [1] Susanna Romano, Serena De Santis, Andrea Martinelli, Lorenzo Augusto Rocchi, Daniele Rocco, Giovanni Sotgiu, and Monica Orsini, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01235. keywords: {thermoplastic starch;ionic liquid plasticizers;mono/dicationic imidazolium structure;anion effect;conductive films} |