Sr2+ Sustained Release System Augments Bioactivity of Polymer Scaffold AITranslate
Abstract AITranslate
Strontium ion (Sr2+) enabled us to endow polymer bone scaffolds with bioactivity owing to its excellent osteoinductive capacity. Nevertheless, the burst release of Sr2+ hindered its further application. Herein, strontium substituted hydroxyapatite (SrHA) was constructed to achieve a sustained release system. Specifically, Sr2+ could substitute Ca2+ in a HA lattice framework through ion exchange due to their similar ion radius. The ionic bond formed by Sr2+ and surrounding ions could prevent the rapid escape of Sr2+ and thereby achieve the sustained release of Sr2+. Subsequently, SrHA was introduced into the poly-l-lactic (PLLA) scaffold fabricated by selective laser sintering. Results demonstrated that PLLA/SrHA scaffolds presented a sustained Sr2+ release with a cumulative concentration of 5.6 mg/L over 28 days. The released Sr2+ significantly promoted the cell proliferation and differentiation. Furthermore, the tensile and compressive strengths of PLLA/SrHA scaffolds were also greatly enhanced in comparison with that of PLLA scaffolds. These positive findings demonstrated that PLLA/SrHA scaffolds had considerable potential for bone repair.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00024
Chinese Library Classification Number:
Citation Information:
Strontium ion (Sr2+) enabled us to endow polymer bone scaffolds with bioactivity owing to its excellent osteoinductive capacity. Nevertheless, the burst release of Sr2+ hindered its further application. Herein, strontium substituted hydroxyapatite (SrHA) was constructed to achieve a sustained release system. Specifically, Sr2+ could substitute Ca2+ in a HA lattice framework through ion exchange due to their similar ion radius. The ionic bond formed by Sr2+ and surrounding ions could prevent the rapid escape of Sr2+ and thereby achieve the sustained release of Sr2+. Subsequently, SrHA was introduced into the poly-l-lactic (PLLA) scaffold fabricated by selective laser sintering. Results demonstrated that PLLA/SrHA scaffolds presented a sustained Sr2+ release with a cumulative concentration of 5.6 mg/L over 28 days. The released Sr2+ significantly promoted the cell proliferation and differentiation. Furthermore, the tensile and compressive strengths of PLLA/SrHA scaffolds were also greatly enhanced in comparison with that of PLLA scaffolds. These positive findings demonstrated that PLLA/SrHA scaffolds had considerable potential for bone repair.
quote
| GB/T 7714-2015 | [1] Fangwei Qi, Zhihui Wang, Yang Shuai, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00024. |
| MLA | [1] Fangwei Qi, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00024. |
| APA | [1] Fangwei Qi, Zhihui Wang, Yang Shuai, Shuping Peng, & Cijun Shuai. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00024 |
| IEEE | [1] Fangwei Qi, Zhihui Wang, Yang Shuai, Shuping Peng, and Cijun Shuai, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00024. keywords: {bone scaffold;strontium ion;sustained release;selective laser sintering;polyllactic} |