Study on Dimensional Stability of Isostatically Pressed Beryllium Material AITranslate
Abstract AITranslate
By testing the micro-yield strength,thermal expansion coefficient,and dimensional changes of the isostatically pressed beryllium material,its dimensional stability against load and temperature changes was studied.The results show that the micro-yield strength of isostatically pressed beryllium material is relatively high,with an average value of 127.4 MPa,which is 53.5%higher than the equivalent beryllium materials published in the United States.Isostatically pressed beryllium material has a relatively low thermal expansion coefficient,and its longitudinal and horizontal average linear expansion coefficients in the temperature range of 25~100℃are 12.02×10-6/℃and 11.89×10-6/℃,respectively.The total axial resi-dual strain of isostatically pressed beryllium material is small after repeated cooling and heating cycles,about-18×10-6after 15 cycles,and its dimensional thermal stability is excellent.
KeyWords AITranslate
1F. Yang, C. H. Wu and D. L. Sun School of Materials Science & Engineering, Harbin Institute of Technology, Harbin 150001, China.STUDY ON MICRO-PLASTIC DEFORMATION BEHAVIOR OF 2024 A1 ALLOY[J].金属学报:英文版,2000,0(2):502-507. 被引量:3
2钟景明,高勇,王东新,王学泽,王零森.金属铍的微屈服行为及机理[J].中国有色金属学报,2004,14(10):1637-1641. 被引量:14
3许德美,秦高梧,李峰,王东新,夏洪先,任玉平,裴文利.BeO杂质形态与分布对金属铍力学性能的影响[J].中国有色金属学报,2011,21(4):769-776. 被引量:17
4钟景明,孙本双,付晓旭,王零森.宇航精密仪表及零件用金属材料的尺寸稳定性[J].中国有色金属学报,1998,8(A01):229-233. 被引量:6
1王军锋,宫灯,王晓光,姜龙涛.基于磁性能和尺寸稳定性的G1J50M合金综合性能优化[J].金属热处理,2019,44(12):148-153. 被引量:1
2肖福星.沈阳市北海高架桥3#桥结构静载试验研究[J].科学技术创新,2021(10):138-139.
3曾志斌.纤维增强复合材料轨枕的技术参数和试验方法[J].铁道建筑,2021,61(2):107-112. 被引量:3
4席鹏,孙培培,郑亚峰,南海,潘文.典型浇注PBX炸药的准静态压缩力学行为[J].爆破器材,2021,50(2):41-44. 被引量:1
5贺志荣,王芳,叶俊杰,张坤刚,杜雨青.Ti-50.8Ni-0.5V形状记忆合金的相变、组织与性能[J].中国有色金属学报,2021,31(2):322-332. 被引量:6
Basic Information:
DOI:
Chinese Library Classification Number:TG146.24[金属学及工艺—金属材料]
Citation Information:
By testing the micro-yield strength,thermal expansion coefficient,and dimensional changes of the isostatically pressed beryllium material,its dimensional stability against load and temperature changes was studied.The results show that the micro-yield strength of isostatically pressed beryllium material is relatively high,with an average value of 127.4 MPa,which is 53.5%higher than the equivalent beryllium materials published in the United States.Isostatically pressed beryllium material has a relatively low thermal expansion coefficient,and its longitudinal and horizontal average linear expansion coefficients in the temperature range of 25~100℃are 12.02×10-6/℃and 11.89×10-6/℃,respectively.The total axial resi-dual strain of isostatically pressed beryllium material is small after repeated cooling and heating cycles,about-18×10-6after 15 cycles,and its dimensional thermal stability is excellent.
quote
| GB/T 7714-2015 | [1] LI Mei-sui, LI Zhi-nian, ZHANG Zi-fu, et al. Study on Dimensional Stability of Isostatically Pressed Beryllium Material[J]. Rare Metals and Cemented Carbides, 2021(1): 72-76. |
| MLA | [1] LI Mei-sui, et al., "Study on Dimensional Stability of Isostatically Pressed Beryllium Material." Rare Metals and Cemented Carbides, no. 1, 2021, pp. 72-76. |
| APA | [1] LI Mei-sui, LI Zhi-nian, ZHANG Zi-fu, ZHANG Jian kang, LYU Yi-ge, XU De mei, LI Shu-rong, & YANG Chao. (2021). Study on Dimensional Stability of Isostatically Pressed Beryllium Material. Rare Metals and Cemented Carbides(1), 72-76. |
| IEEE | [1] LI Mei-sui, LI Zhi-nian, ZHANG Zi-fu, ZHANG Jian kang, LYU Yi-ge, XU De mei, LI Shu-rong, and YANG Chao, "Study on Dimensional Stability of Isostatically Pressed Beryllium Material," Rare Metals and Cemented Carbides, no. 1, pp. 72-76, 2021. keywords: {isostatically pressed beryllium;dimensional stability;micro-yield strength;thermal expansion coefficient;cooling and heating cycle} |