Study on the Gradient Cemented Carbides Produced By Carbon-adding Sintering AITranslate

National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

New development of gradient cemented carbides is summarized in this paper.The technology,principle of carbon-adding sintering are introduced.The application and prospects of gradient cemented carbides are also discussed.

KeyWords AITranslate

cemented carbides WC-Co gradient structure carbon-adding sintering

1杨维才,吴恩熙.真空渗碳制备双相梯度硬质合金的研究[J].硬质合金,1999,16(3):154-158. 被引量:9

2吴恩熙.国外梯度硬质合金的发展[J].稀有金属与硬质合金,1995,23(3):57-60. 被引量:18

3张立,黄伯云,吴恩熙.双相结构梯度硬质合金的研究现状[J].材料导报,2000,14(12):17-19. 被引量:17

4覃伟坚.功能梯度硬质合金球齿的研制[J].中国钨业,1999,14(5):198-201. 被引量:11

5高荣根,李沐山.梯度结构硬质合金的开发与应用[J].硬质合金,2000,17(2):77-84. 被引量:15

6孙绪新.梯度硬质合金的研制[J].粉末冶金技术,1998,16(4):260-264. 被引量:20

7张立,陶小平.粗颗粒碳化钨粉制取过程中的质量控制[J].硬质合金,2000,17(1):26-29. 被引量:5

1肖逸锋,贺跃辉,黄自谦,张丽娟.梯度结构硬质合金制备技术的研究进展[J].中国钨业,2005,20(3):31-36. 被引量:4

2张利平,张国珍,张久兴,周美玲.叠层加压SPS烧结制备梯度硬质合金[J].稀有金属材料与工程,2006,35(1):70-73. 被引量:3

3张梅琳,朱世根,朱守星.超细及纳米硬质合金中碳含量的变化及对组织性能的影响[J].材料导报,2006,20(8):65-68. 被引量:24

4史留勇,张守全,黄继华.WC-Co功能梯度硬质合金研究进展[J].粉末冶金技术,2010,28(4):305-312. 被引量:15

5羊建高,戴煜.硬质合金的发展趋势及特殊粉末的制备技术[J].稀有金属与硬质合金,2011,39(1):48-51. 被引量:9

6娄静,易健宏,鲍瑞,彭元东,张浩泽.碳含量对微波烧结亚微米硬质合金组织与性能的影响[J].中国钨业,2011,26(1):30-33. 被引量:4

7刘海波,刘兆强.LWD电阻率新型耐磨带的研制[J].西部探矿工程,2011,23(9):61-62.

8刘伟,李重典,杨新宇,王雁洁,张旭辉,董定乾.WC-15%TiC-6%Co合金表面不同钴含量对切削寿命的影响[J].工具技术,2019,53(11):34-36.

1曹鼎,熊计,郭智兴.表面脱β层梯度结构硬质合金研究进展[J].硬质合金,2006,23(1):38-41. 被引量:2

2刘书祯.超细晶硬质合金晶粒长大抑制剂的研究[J].稀有金属与硬质合金,2007,35(4):51-56. 被引量:21

3吴悦梅,熊计,赖人铭.碳含量对WC-Co硬质合金显微组织的影响及其控制[J].硬质合金,2008,25(3):179-185. 被引量:25

4郑建智,承新,郑勇,严永林,赵能伟.烧结工艺和碳加入量对Mo_2FeB_2基金属陶瓷显微组织和力学性能的影响[J].机械工程材料,2009,33(3):31-34. 被引量:8

5李壮,王家君,林晨光,崔舜.WC-Co超细硬质合金微观结构对其性能的影响[J].硬质合金,2009,26(3):188-193. 被引量:22

6傅又红.钨钛钴类硬质合金表面亮花的形成及其对产品性能的影响[J].硬质合金,2010,27(1):27-32. 被引量:2

7史留勇,张守全,黄继华.WC-Co功能梯度硬质合金研究进展[J].粉末冶金技术,2010,28(4):305-312. 被引量:15

8宗霞,鲁玉祥.稀土硬质合金的发展现状[J].矿山机械,2010,38(22):1-6. 被引量:7

9SUN Lan,YANG Tian'en,JIA Chengchang,XIONG Ji.Effects of graphite on the microstructure and properties of ultrafine WC-11Co composites by spark plasma sintering[J].稀有金属:英文版,2011,30(1):63-67. 被引量:1

10刘芳,严峰,张勇,杨贺,陆兴.热压烧结制备无粘结剂碳化钨硬质合金[J].大连交通大学学报,2011,32(1):56-60. 被引量:2

1张武装,刘咏,黄伯云,羊建高.WC-Co梯度结构硬质合金的研究进展[J].粉末冶金材料科学与工程,2004,9(2):121-125. 被引量:5

2张武装,高海燕,刘咏.粘结相梯度结构硬质合金的研究现状[J].材料导报,2006,20(11):62-64. 被引量:7

3孙绪新.梯度硬质合金的研制[J].粉末冶金技术,1998,16(4):260-264. 被引量:20

4高荣根,李沐山.梯度结构硬质合金的开发与应用[J].硬质合金,2000,17(2):77-84. 被引量:15

5曹鼎,熊计,郭智兴.表面脱β层梯度结构硬质合金研究进展[J].硬质合金,2006,23(1):38-41. 被引量:2

6孙东平.高质量低钴矿用硬质合金的研制和生产[J].稀有金属与硬质合金,1996,24(1):15-19. 被引量:2

7黄钢祥.快淬Nd—Fe—B粘结磁体应用开发前景[J].金属材料研究,1993,19(3):47-58.

8张武装,刘咏,贺跃辉,黄伯云.一种特殊烧结技术对梯度结构硬质合金性能影响的研究[J].功能材料,2007,38(2):292-294. 被引量:1

9史留勇,刘义敏,张守全,黄继华,赵兴科,张华.烧结工艺对脱β层梯度硬质合金梯度结构的影响[J].北京科技大学学报,2011,33(4):462-467. 被引量:4

10叶永权,成晓玲,匡同春,白晓军,雷淑梅,向雄志,袁高群.梯度结构硬质合金的最新研究进展[J].稀有金属,2005,29(3):357-362. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]

Citation Information:

New development of gradient cemented carbides is summarized in this paper.The technology,principle of carbon-adding sintering are introduced.The application and prospects of gradient cemented carbides are also discussed.

quote

GB/T 7714-2015 [1] ZHANG Wu-zhuang, LIU Yong, YANG Jian-gao, et al. Study on the Gradient Cemented Carbides Produced By Carbon-adding Sintering[J]. Rare Metals and Cemented Carbides, 2004(1): 32-35.
MLA [1] ZHANG Wu-zhuang, et al., "Study on the Gradient Cemented Carbides Produced By Carbon-adding Sintering." Rare Metals and Cemented Carbides, no. 1, 2004, pp. 32-35.
APA [1] ZHANG Wu-zhuang, LIU Yong, YANG Jian-gao, & HUANG Bo-yun. (2004). Study on the Gradient Cemented Carbides Produced By Carbon-adding Sintering. Rare Metals and Cemented Carbides(1), 32-35.
IEEE [1] ZHANG Wu-zhuang, LIU Yong, YANG Jian-gao, and HUANG Bo-yun, "Study on the Gradient Cemented Carbides Produced By Carbon-adding Sintering," Rare Metals and Cemented Carbides, no. 1, pp. 32-35, 2004. keywords: {cemented carbides;WC-Co;gradient structure;carbon-adding sintering}