Epoxy resins are one of the important and intensively used thermosetting adhesives in the automotive and electronic industries. Understanding and improving the interfacial interactions between epoxy adhesives and metal adherends are essential and urgent issues that need to be overcome to expand the scope of adhesive applications. In this study, a bioinspired acetate-protected vinyl catechol (Ac2VCa) monomer derived from natural caffeic acid was copolymerized with glycidyl methacrylate (GMA) to prepare a catechol-containing polymer─PGMA-co-P(Ac2VCa)─for the enhancement of interfacial adhesion. The deprotection of acetate protecting groups using a diamine was validated, allowing the achievement of the deprotection and adsorption of the PGMA-co-P(Ac2VCa) promoter in one processing procedure for its direct usage as the primer or additive. With the incorporation of catechol moieties, the strengthened interfacial interactions can effectively improve the lap shear strength of epoxy-adhesive-bonded metallic joints.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00226
Chinese Library Classification Number:
Citation Information:
Epoxy resins are one of the important and intensively used thermosetting adhesives in the automotive and electronic industries. Understanding and improving the interfacial interactions between epoxy adhesives and metal adherends are essential and urgent issues that need to be overcome to expand the scope of adhesive applications. In this study, a bioinspired acetate-protected vinyl catechol (Ac2VCa) monomer derived from natural caffeic acid was copolymerized with glycidyl methacrylate (GMA) to prepare a catechol-containing polymer─PGMA-co-P(Ac2VCa)─for the enhancement of interfacial adhesion. The deprotection of acetate protecting groups using a diamine was validated, allowing the achievement of the deprotection and adsorption of the PGMA-co-P(Ac2VCa) promoter in one processing procedure for its direct usage as the primer or additive. With the incorporation of catechol moieties, the strengthened interfacial interactions can effectively improve the lap shear strength of epoxy-adhesive-bonded metallic joints.
quote
| GB/T 7714-2015 | [1] ChienWei Chu, Yucheng Zhang, Tomohiro Kubo, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00226. |
| MLA | [1] ChienWei Chu, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00226. |
| APA | [1] ChienWei Chu, Yucheng Zhang, Tomohiro Kubo, Shiho Tanizaki, Ken Kojio, Kotaro Satoh, & Atsushi Takahara. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00226 |
| IEEE | [1] ChienWei Chu, Yucheng Zhang, Tomohiro Kubo, Shiho Tanizaki, Ken Kojio, Kotaro Satoh, and Atsushi Takahara, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00226. keywords: {adhesion promoter;catechol;epoxy resin adhesive;primer coating;radical polymerization} |