daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Design, testing, and mechanical behavior of additively manufactured casing with optimized lattice structure AITranslate

United Technologies Research Center, 411 Silver Lane;United Technologies Research Center, 411 Silver Lane; University of Pittsburgh; University of Pittsburgh
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Additively manufactured internal lattice structures offer a unique approach to lightweight components and adding multi-functionality. Design methods for parts based on lattices are emerging and include a family of topology optimization schemes for tailoring local cell density to service loadings. In order to gain confidence, these methods must be validated in a controlled manner. In this paper, we report optimization, analysis, manufacturing, and mechanical test validation of a casing-like test article. The test article was optimized using a stress-based homogenized topology optimization approach and achieved a 53% weight reduction versus a solid, fully-dense casing with the same form factor. The optimized geometry was studied with high-fidelity finite element analysis and then additively manufactured. Mechanical testing was performed and demonstrated good correlation between the homogenized finite element model used for optimization, the high-fidelity finite element model, and experimental results. The findings validate the optimization approach for the particular use and load case and start to build confidence in the approach as an accepted method.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.addma.2018.05.021

Chinese Library Classification Number:

Citation Information:

Additively manufactured internal lattice structures offer a unique approach to lightweight components and adding multi-functionality. Design methods for parts based on lattices are emerging and include a family of topology optimization schemes for tailoring local cell density to service loadings. In order to gain confidence, these methods must be validated in a controlled manner. In this paper, we report optimization, analysis, manufacturing, and mechanical test validation of a casing-like test article. The test article was optimized using a stress-based homogenized topology optimization approach and achieved a 53% weight reduction versus a solid, fully-dense casing with the same form factor. The optimized geometry was studied with high-fidelity finite element analysis and then additively manufactured. Mechanical testing was performed and demonstrated good correlation between the homogenized finite element model used for optimization, the high-fidelity finite element model, and experimental results. The findings validate the optimization approach for the particular use and load case and start to build confidence in the approach as an accepted method.

quote

GB/T 7714-2015 [1] Matthew E. Lynch, Matthew Mordasky, Lin Cheng, et al. Additive Manufacturing, 2018(22). DOI:10.1016/j.addma.2018.05.021.
MLA [1] Matthew E. Lynch, et al., Additive Manufacturing, no. 22, 2018, https://doi.org/10.1016/j.addma.2018.05.021.
APA [1] Matthew E. Lynch, Matthew Mordasky, Lin Cheng, & Albert To. (2018). Additive Manufacturing(22). https://doi.org/10.1016/j.addma.2018.05.021
IEEE [1] Matthew E. Lynch, Matthew Mordasky, Lin Cheng, and Albert To, Additive Manufacturing, no. 22, 2018, doi: 10.1016/j.addma.2018.05.021.