Efficient Floatation Tests on Peru As-containing Cu-Mo Ore AITranslate
Abstract AITranslate
Flotation property of a Peru As-containing Cu-Mo ore was studied. The results show that the qualified copper concentrate containing 26.65% Cu,0. 637% Mo and 0. 348% As can be obtained from the closed-circuit flotation process with modified thiourea Mac-12 as the collector and AH-1 as the inhibitor for arsenic minerals. And the recovery rates of Cu,Mo and As in the copper concentrate are 88.15%, 85.77% and 33.80%, respectively.
KeyWords AITranslate
1王雅静,田锋.提高某低品位难选铜钼矿铜钼粗选回收率的试验研究[J].有色金属:选矿部分,2008(3):12-15. 被引量:24
2谷志君,王越,苏凯,杨宝东.某大型铜钼矿铜钼可浮性研究[J].有色金属:选矿部分,2009(2):1-4. 被引量:13
3罗小华.含砷铜矿物的除砷研究[J].金属矿山,2000(7):56-57. 被引量:15
4殷志勇,成海芳,张文彬.浅谈含砷铜矿的砷害治理[J].四川有色金属,2006(4):57-59. 被引量:4
5傅文章,张裕书,洪秉信,张渊.某高砷银铜精矿的利用研究[J].矿产综合利用,2001(4):1-6. 被引量:4
6廖祥文,李成秀.某高砷铜锡矿选铜除砷试验研究[J].矿产综合利用,2007(3):3-6. 被引量:13
7刘四清,张文彬.高砷硫精矿除砷的研究[J].矿产保护与利用,2005,25(6):28-31. 被引量:20
1彭蓉,魏志聪,王衡嵩,白睿.铜砷矿物分离研究进展[J].矿产保护与利用,2020,40(2):93-99. 被引量:2
2石海兰,朱文龙,邹松.某高泥低品位难选钼矿高效浮选回收研究[J].稀有金属与硬质合金,2022,50(6):11-17.
3Zhi-xiong Liu,Lin Sun,Liang-dong Tang,Jie Hu,Yang Xiao,Yi-guang Chen,Zhou-lan Yin.Removal of Metallic Impurities from Off-Grade Copper Concentrate in Alkaline Solution[J].有色冶金(英文),2018,7(2):9-23.
1门靖,杨芳,牛国龙,温锦荣,郭洁芬,梁春梅,吴英纪,孙洋娟.苹果酸的应用研究进展[J].化工与医药工程,2022,43(5):62-69.
2李绍英,赵留成,于晓东,赵礼兵,白丽梅.国外某难选高砷铜金矿石选冶联合工艺研究[J].金属矿山,2023(2):101-106.
1于宏东,金建文.秘鲁某斑岩型含砷铜钼矿工艺矿物学研究[J].矿冶,2012,21(1):91-94. 被引量:8
2张春明.BC-12型露天矿装药车[J].矿山机械,1998,26(12):25-26. 被引量:3
3李成秀,王昌良.铜砷浮选分离的进展[J].国外金属矿选矿,2005,42(9):9-12. 被引量:20
4周斌.C-12G型气动装岩机行走、提升系统的改造[J].矿山机械,2006,34(10):118-119.
5周德炎,陈志文.长坡选矿厂锌浮选尾矿硫砷分离试验研究[J].大众科技,2012,14(1):133-135. 被引量:2
6罗时军.Mac-12新型捕收剂提高铜金钼回收率的试验研究[J].稀有金属,2008,32(2):230-233. 被引量:4
7甘清海.乳化炸药HP型灌装机与RC-12型装药机配套使用可行性探讨[J].技术与市场,2016,23(4):64-65. 被引量:1
8冯忠伟,陆爱民.某采矿废方浮选回收雄黄等砷矿物试验研究[J].大众科技,2009,11(10):96-96.
9孟宪瑜,刘学胜,马忠臣,秦贵杰.雄黄坡难选高砷金矿石选矿试验研究[J].有色矿冶,2001,17(4):15-18. 被引量:5
10黄锦庆.广西某高砷铜锌矿选矿工艺研究[J].有色金属:选矿部分,2007(3):18-21. 被引量:7
Basic Information:
DOI:
Chinese Library Classification Number:TD954[矿业工程—选矿]
Citation Information:
Flotation property of a Peru As-containing Cu-Mo ore was studied. The results show that the qualified copper concentrate containing 26.65% Cu,0. 637% Mo and 0. 348% As can be obtained from the closed-circuit flotation process with modified thiourea Mac-12 as the collector and AH-1 as the inhibitor for arsenic minerals. And the recovery rates of Cu,Mo and As in the copper concentrate are 88.15%, 85.77% and 33.80%, respectively.
quote
| GB/T 7714-2015 | [1] CAO Zhan-fang, ZHONG Hong, LIU Guang-yi, et al. Efficient Floatation Tests on Peru As-containing Cu-Mo Ore[J]. Rare Metals and Cemented Carbides, 2012(3): 1-4. |
| MLA | [1] CAO Zhan-fang, et al., "Efficient Floatation Tests on Peru As-containing Cu-Mo Ore." Rare Metals and Cemented Carbides, no. 3, 2012, pp. 1-4. |
| APA | [1] CAO Zhan-fang, ZHONG Hong, LIU Guang-yi, WANG Shuai, & XIA Liu-yin. (2012). Efficient Floatation Tests on Peru As-containing Cu-Mo Ore. Rare Metals and Cemented Carbides(3), 1-4. |
| IEEE | [1] CAO Zhan-fang, ZHONG Hong, LIU Guang-yi, WANG Shuai, and XIA Liu-yin, "Efficient Floatation Tests on Peru As-containing Cu-Mo Ore," Rare Metals and Cemented Carbides, no. 3, pp. 1-4, 2012. keywords: {As-containing Cu-Mo ore;flotation;collector;inhibitor} |