InSb Nanowire Direct Growth on Plastic for Monolithic Flexible Device Fabrication AITranslate

Aalto University; Aalto University; Military University of Technology; Military University of Technology; Military University of Technology; Aalto University; Aalto University; Aalto University; Aalto University; Aalto University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We report direct growth of InSb nanowires (NWs) and monolithic device fabrication on flexible plastic substrates. The nanowires were grown using metal–organic vapor-phase epitaxy (MOVPE) in self-catalyzed mode. The InSb NWs are shown to form in the zinc-blende crystal structure and to exhibit strong photoluminescence at room temperature. The NW array light-trapping properties are evidenced by reflectance that is significantly reduced compared to bulk material. Finally, the InSb NWs are used to demonstrate a metal–semiconductor–metal photoresistor directly on the flexible plastic substrate. The results are believed to advance the integration of III–V nanowires to flexible devices, and infrared photodetectors in particular.

KeyWords AITranslate

InSb nanowires flexible bendable photoluminescence MOVPE/MOCVD photoresistor
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01175

Chinese Library Classification Number:

Citation Information:

We report direct growth of InSb nanowires (NWs) and monolithic device fabrication on flexible plastic substrates. The nanowires were grown using metal–organic vapor-phase epitaxy (MOVPE) in self-catalyzed mode. The InSb NWs are shown to form in the zinc-blende crystal structure and to exhibit strong photoluminescence at room temperature. The NW array light-trapping properties are evidenced by reflectance that is significantly reduced compared to bulk material. Finally, the InSb NWs are used to demonstrate a metal–semiconductor–metal photoresistor directly on the flexible plastic substrate. The results are believed to advance the integration of III–V nanowires to flexible devices, and infrared photodetectors in particular.

quote

GB/T 7714-2015 [1] Vladislav Khayrudinov, Tomi Koskinen, Kacper Grodecki, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01175.
MLA [1] Vladislav Khayrudinov, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01175.
APA [1] Vladislav Khayrudinov, Tomi Koskinen, Kacper Grodecki, Krzysztof Murawski, Małgorzata Kopytko, Lide Yao, Hua Jiang, Ilkka Juhani Tittonen, Harri Lipsanen, & Tuomas Haggren. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01175
IEEE [1] Vladislav Khayrudinov, Tomi Koskinen, Kacper Grodecki, Krzysztof Murawski, Małgorzata Kopytko, Lide Yao, Hua Jiang, Ilkka Juhani Tittonen, Harri Lipsanen, and Tuomas Haggren, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01175. keywords: {InSb nanowires flexible bendable photoluminescence MOVPE/MOCVD photoresistor}