daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Recyclable, Repairable, and Fire-Resistant High-Performance Carbon Fiber Biobased Epoxy AITranslate

Université Côte d’Azur;ESA;Thales Alenia Space, 5 Allée des Gabians; Université Côte d’Azur;Université Côte d’Azur
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Due to the global environmental concerns caused by the ever-increasing environmental impact, landfill materials, and CO2 emission, there is a critical need in the elaboration of sustainable composite materials. Advanced material composites used in the production of high-performance products to solve some of the most difficult engineering challenges are having a key role in decarbonization by their light weight, higher performance, and increasing durability. In this work, sustainable carbon fiber reinforced composites (CFRCs) have been engineered with an environmentally friendly epoxy resin derived from natural and renewable compounds employing an industrial feasible manufacturing protocol. The thermosetting resin with a biobased organic carbon content (BOC) of ∼77% was synthesized by combining a renewable based monomer, the triglycidyl ether of phloroglucinol (TGPh), with hexahydro-4-methylphthalic anhydride (HMPA). The developed CFRCs show high performance with high glass transitions Tg > 350 °C, a high storage modulus ∼42 GPa, a high interlaminar shear strength ∼63 MPa, and a compressive strength ∼400 MPa. In addition, the outgassing tests show that both the resin and the CFRCs are compliant for space application. Moreover, the biobased CFRCs exhibit chemical recyclability, reprocessability, and excellent intrinsic flame resistance.

KeyWords AITranslate

polymer−matrix composites (PMCs) recycling thermosetting resin hightemperature properties repairable fireresistance Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c02184

Chinese Library Classification Number:

Citation Information:

Due to the global environmental concerns caused by the ever-increasing environmental impact, landfill materials, and CO2 emission, there is a critical need in the elaboration of sustainable composite materials. Advanced material composites used in the production of high-performance products to solve some of the most difficult engineering challenges are having a key role in decarbonization by their light weight, higher performance, and increasing durability. In this work, sustainable carbon fiber reinforced composites (CFRCs) have been engineered with an environmentally friendly epoxy resin derived from natural and renewable compounds employing an industrial feasible manufacturing protocol. The thermosetting resin with a biobased organic carbon content (BOC) of ∼77% was synthesized by combining a renewable based monomer, the triglycidyl ether of phloroglucinol (TGPh), with hexahydro-4-methylphthalic anhydride (HMPA). The developed CFRCs show high performance with high glass transitions Tg > 350 °C, a high storage modulus ∼42 GPa, a high interlaminar shear strength ∼63 MPa, and a compressive strength ∼400 MPa. In addition, the outgassing tests show that both the resin and the CFRCs are compliant for space application. Moreover, the biobased CFRCs exhibit chemical recyclability, reprocessability, and excellent intrinsic flame resistance.

quote

GB/T 7714-2015 [1] Roxana Dinu, Ugo Lafont, Olivier Damiano, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02184.
MLA [1] Roxana Dinu, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02184.