Abstract AITranslate
In this study,a self-supporting CoMoO4@MnMoO4 composite electrode material on a nickel foam substrate was prepared through a two-step hydrothermal method followed by annealing and calcina-tion treatments.The phase composition and microstructure of the electrode material were investigated using X-ray diffractometer(XRD)and scanning electron microscope(SEM).The electrochemical perfor-mance of the electrode material was evaluated using an electrochemical workstation.The results reveal that the CoMoO4@MnMoO4 electrode material possesses a dense nanosheet structure with numerous nanopar-ticles attached on the surface.The abundant nanosheet interlayer pores significantly facilitate ion transport and provide ample active sites,thereby promoting Faradaic redox reactions between the active materials and electrolyte.The electrode demonstrates an charge/discharge duration of 1500 s and achieves an exceptional specific capacitance of 726.6 C/g at a current density of 1 A/g.Furthermore,the CoMoO4@MnMoO4 com-posite electrode material shows significantly better rate performance than the individual CoMoO4 and MnMoO4 electrodes.The CoMoO4@MnMoO4 composite electrode material exhibits superior electrochemi-cal performance compared to its individual-components.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:TQ152[化学工程]
Citation Information:
In this study,a self-supporting CoMoO4@MnMoO4 composite electrode material on a nickel foam substrate was prepared through a two-step hydrothermal method followed by annealing and calcina-tion treatments.The phase composition and microstructure of the electrode material were investigated using X-ray diffractometer(XRD)and scanning electron microscope(SEM).The electrochemical perfor-mance of the electrode material was evaluated using an electrochemical workstation.The results reveal that the CoMoO4@MnMoO4 electrode material possesses a dense nanosheet structure with numerous nanopar-ticles attached on the surface.The abundant nanosheet interlayer pores significantly facilitate ion transport and provide ample active sites,thereby promoting Faradaic redox reactions between the active materials and electrolyte.The electrode demonstrates an charge/discharge duration of 1500 s and achieves an exceptional specific capacitance of 726.6 C/g at a current density of 1 A/g.Furthermore,the CoMoO4@MnMoO4 com-posite electrode material shows significantly better rate performance than the individual CoMoO4 and MnMoO4 electrodes.The CoMoO4@MnMoO4 composite electrode material exhibits superior electrochemi-cal performance compared to its individual-components.
quote
| GB/T 7714-2015 | [1] LIU Xin-yu, XIANG Jun, MA Dong-mei, et al. Preparation and Electrochemical Performance of CoMoO4@MnMoO4 Composite Electrode Material[J]. Rare Metals and Cemented Carbides, 2025(4): 140-147. |
| MLA | [1] LIU Xin-yu, et al., "Preparation and Electrochemical Performance of CoMoO4@MnMoO4 Composite Electrode Material." Rare Metals and Cemented Carbides, no. 4, 2025, pp. 140-147. |
| APA | [1] LIU Xin-yu, XIANG Jun, MA Dong-mei, & LI Wei. (2025). Preparation and Electrochemical Performance of CoMoO4@MnMoO4 Composite Electrode Material. Rare Metals and Cemented Carbides(4), 140-147. |
| IEEE | [1] LIU Xin-yu, XIANG Jun, MA Dong-mei, and LI Wei, "Preparation and Electrochemical Performance of CoMoO4@MnMoO4 Composite Electrode Material," Rare Metals and Cemented Carbides, no. 4, pp. 140-147, 2025. keywords: {CoMoO@MnMoO;composite electrode material;hydrothermal method;annealing;calcination;electrochemical property;microstructure} |