Research on Adsorption Performance of P204 Solvent Impregnated Resins for Gallium(Ⅲ)in Sulfuric Acid Solution AITranslate
Abstract AITranslate
P204 solvent impregnated resins(P204 SIRs)were prepared by using styrene-divinylbenzene macroporous resin(HZ818)as a carrier and bis(2-ethylhexyl)phosphoric acid(P204)as an extractant,and were characterized by scanning electron microscope(SEM),infrared spectrometer(IR),and thermogravimetric analyzer(TG)to investigate the adsorption performance of P204 SIRs for Ga(Ⅲ)in sulfuric acid solution.The results show that the optimal pH value for Ga(Ⅲ)adsorption by P204 SIRs is 1.8.The adsorption equilibrium time of Ga(Ⅲ)at 298 K is approximately 20 h,with a saturation adsorption capacity of 10.9 mg/g,and the kinetic adsorption behavior could be described by a pseudo-second-order kinetic equation as t/Qt=0.2173+0.0962t.The isothermal adsorption of Ga(Ⅲ)by P204 SIRs follows the Langmuir isothermal adsorption model of Ce/Qe=0.4482+0.0588Ce,and the fitted saturation adsorption capacity of Ga(Ⅲ)at 298 K is about 17 mg/g.
KeyWords AITranslate
1尹富强,赵玉辰,李赵春.镓基液态金属应用的研究进展[J].现代化工,2022,42(5):24-29. 被引量:7
2郭文超,李望,朱晓波,张治国,张传祥.P507萃取煤矸石硫酸浸出液中镓的实验研究[J].稀有金属与硬质合金,2022,50(4):28-32. 被引量:3
3刘凯华.用P204从硫酸体系中萃取分离铟镓[J].湿法冶金,2021,40(5):386-389. 被引量:5
4廖亚龙,曹磊,王祎洋,叶朝.溶液中镓的提取与分离研究进展[J].材料导报,2017,31(15):133-138. 被引量:6
5李超,王丽萍,郭昭华,王永旺,陈东.盐酸体系下镓的提取技术研究进展[J].稀有金属与硬质合金,2019,47(1):6-10. 被引量:9
6刘延红,郭昭华,池君洲,王永旺,陈东.镓回收方法与技术的研究与进展[J].稀有金属与硬质合金,2016,44(1):1-8. 被引量:17
7熊英,张莹莹,娄振宁,单炜军,宋玉林.镓的萃取分离研究进展[J].辽宁大学学报:自然科学版,2016,43(4):335-342. 被引量:7
8宋金如,龚治湘,丁红芳.P_(350)萃淋树脂分离微量镓的性能研究[J].华东地质学院学报,1997,20(2):135-140. 被引量:6
9刘建,闫英桃,邵海欣,陈长江.CL-TBP萃淋树脂吸附分离镓(Ga)研究[J].化学通报,2001,64(2):119-121. 被引量:11
10刘军深,蔡伟民.萃淋树脂技术分离稀散金属的研究现状及展望[J].稀有金属与硬质合金,2003,31(4):36-39. 被引量:26
1张占元,宁豪,李铭,陈思,刘荣,毛佳伟.气相色谱直接进样分析醇基液体燃料中甲醇和水含量[J].中国石油和化工标准与质量,2023,43(6):39-41.
2吴勉,梁星,李小兵.PPA@UiO-66破乳剂的制备及在油-水分离中的应用[J].中国矿业大学学报,2023,52(5):990-1001.
3冯健,谢媛媛.利用二氧化锰制备2-硝基-4-甲砜基苯甲酸的绿色合成方法[J].嘉兴学院学报,2023,35(6):126-130.
4徐鑫鑫,窦伟,戎有祺,孙晨智,钟秋月,陈永雷.壳聚糖功能化的茶基水凝胶膜材料的制备及其在Pb^(2+)吸附中的应用[J].环境化学,2023,42(9):3136-3147.
5周展,王健,龚桂胜,李雪,宋桂霞,刘杰军,吕雨农.无卤阻燃不饱和聚酯浸渍树脂的研究[J].绝缘材料,2023,56(11):23-27.
6景长勇,梁贇,金泥沙,董冰.磁混凝技术处理微污染河水实验研究[J].河北水利电力学院学报,2023,33(3):45-50.
7郭焱,何雯,吴丹,张雅清,代加南.好氧反硝化菌Pseudomonas sp. J-5的分离及脱氮性能研究[J].绿色科技,2023,25(14):224-229.
8李德谦,王忠怀,张长平,乐少明.2-乙基己基膦酸单(2-乙基己基)酯萃取稀土元素机理的研究 III.高浓度稀土元素(III)在H^(+)(HNO_(3),HCl)-H_(2)O-HEH(EHP)-煤油体系中的分配及萃取反应[J].化学学报,1988(6):586-589.
9谢雨涵,杨璨雨,欧杨,马婷,董佳甜,李向东.剩余污泥裂解灰吸附去除黑臭水体中磷的研究[J].环境科技,2023,36(5):19-23.
10刘森萍,夏新珂,信博文,张洋榕,白玉,金辉,李成威.改性活性炭负载纳米零价铁吸附Cr(Ⅵ)的机理研究[J].辽宁科技大学学报,2023,46(4):287-295.
Basic Information:
DOI:
Chinese Library Classification Number:TF843.1[冶金工程—有色金属冶金]
Citation Information:
P204 solvent impregnated resins(P204 SIRs)were prepared by using styrene-divinylbenzene macroporous resin(HZ818)as a carrier and bis(2-ethylhexyl)phosphoric acid(P204)as an extractant,and were characterized by scanning electron microscope(SEM),infrared spectrometer(IR),and thermogravimetric analyzer(TG)to investigate the adsorption performance of P204 SIRs for Ga(Ⅲ)in sulfuric acid solution.The results show that the optimal pH value for Ga(Ⅲ)adsorption by P204 SIRs is 1.8.The adsorption equilibrium time of Ga(Ⅲ)at 298 K is approximately 20 h,with a saturation adsorption capacity of 10.9 mg/g,and the kinetic adsorption behavior could be described by a pseudo-second-order kinetic equation as t/Qt=0.2173+0.0962t.The isothermal adsorption of Ga(Ⅲ)by P204 SIRs follows the Langmuir isothermal adsorption model of Ce/Qe=0.4482+0.0588Ce,and the fitted saturation adsorption capacity of Ga(Ⅲ)at 298 K is about 17 mg/g.
quote
| GB/T 7714-2015 | [1] LI Zhi-ling, XU Cui-ping, LIU Jun-shen, et al. Research on Adsorption Performance of P204 Solvent Impregnated Resins for Gallium(Ⅲ)in Sulfuric Acid Solution[J]. Rare Metals and Cemented Carbides, 2023(5): 15-21. |
| MLA | [1] LI Zhi-ling, et al., "Research on Adsorption Performance of P204 Solvent Impregnated Resins for Gallium(Ⅲ)in Sulfuric Acid Solution." Rare Metals and Cemented Carbides, no. 5, 2023, pp. 15-21. |
| APA | [1] LI Zhi-ling, XU Cui-ping, LIU Jun-shen, LIU Qing-qing, & CHEN Xiao-liang. (2023). Research on Adsorption Performance of P204 Solvent Impregnated Resins for Gallium(Ⅲ)in Sulfuric Acid Solution. Rare Metals and Cemented Carbides(5), 15-21. |
| IEEE | [1] LI Zhi-ling, XU Cui-ping, LIU Jun-shen, LIU Qing-qing, and CHEN Xiao-liang, "Research on Adsorption Performance of P204 Solvent Impregnated Resins for Gallium(Ⅲ)in Sulfuric Acid Solution," Rare Metals and Cemented Carbides, no. 5, pp. 15-21, 2023. keywords: {impregnated resin;adsorption;gallium(Ⅲ);sulfuric acid;kinetic equation;isothermal adsorption model} |