Study on Technology for Recycling Cobalt from Li-ion Secondary Battery Anode Scrap of Al-Co Film AITranslate

Department of Metallurgical Science and Engineering, Central South University;Department of Metallurgical Science and Engineering, Central South University;Department of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

According to the property of LiCoO 2 in Li-ion secondary battery anode wastes of Al Co film,dissolution reaction of LiCoO 2 in a system of H 2SO 4 and H 2O 2 was put forward: 2LiCoO 2+3H 2SO 4+H 2O 2→Li 2SO 4+2CoSO 4+4H 2O+O 2↑ A simple process for recycling cobalt and aluminum was determined,including alkali leaching of wastes,acid dissolution of slag,purification of cobalt containing solution and precipitation of cobalt.The recovery of cobalt reaches 95.75%.Aluminum in alkali leaching solution was neutralized with H 2SO 4 and the product Al(OH) 3with a chemical purity was obtained,the recycling rate is 94.84%.The profit of 45600.6 RMB Yuan can be obtained in treating l ton waste by the technology.

KeyWords AITranslate

Li ion secondary battery anode material scrap LiCoO 2 recycling cobalt cobalt oxalate

1郭鸣凤,杨瑞敏,张泽波,叶劲草.LiCoO_2的合成及其在锂蓄电池中的行为[J].电化学,1995,1(1):70-77. 被引量:8

2吴国良,杨新河,阚素荣,金维华.锂离子电池及其电极材料的研制[J].电池,1998,28(6):258-262. 被引量:31

3《有色金属提取冶金手册》编辑委员会.有色金属提取冶金手册(锌镉铅铋分册)[M].北京:冶金工业出版社,1992.246.

4文德荣.草酸钴和氧化钴[J].江西冶金,1997,17(5):55-56. 被引量:9

5彭忠东,杨建红,邓朝阳,刘业翔.锂离子二次电池正极材料的研制进展[J].电池,1999,29(3):125-127. 被引量:18

6章福平.酒石酸法合成的LiCoO_2的结构及其二次锂电池行为研究[J].电化学,1995,1(3):342-347. 被引量:21

1南俊民,韩东梅,崔明,左晓希.溶剂萃取法从废旧锂离子电池中回收有价金属[J].电池,2004,34(4):309-311. 被引量:45

2吴晓东,傅小明,柴永新,傅明喜,戴起勋.蓝色氧化钨氢还原制取超细钨粉的工艺研究[J].稀有金属与硬质合金,2005,33(1):14-17. 被引量:5

3王永利,赵丽霞.从含钴废料中提取钴的研究进展[J].再生资源研究,2005(2):29-32. 被引量:22

4欧秀芹,孙新华,赵庆云,范飞.锂离子废电池资源化技术进展[J].无机盐工业,2005,37(9):11-14. 被引量:14

5童东革,赖琼钰,吉晓洋.废旧锂离子电池正极材料钴酸锂的回收[J].化工学报,2005,56(10):1967-1970. 被引量:28

6张正洁,杨金侠.废锂离子电池的资源化回收方法[J].有色矿冶,2005,21(6):46-47. 被引量:11

7秦毅红,齐申.有机溶剂分离法处理废旧锂离子电池[J].有色金属:冶炼部分,2006(1):13-16. 被引量:17

8谭海翔,胡启阳,李新海,王志兴,郭华军.含铝硫酸钴溶液中回收氧化钴新工艺的研究[J].稀有金属与硬质合金,2006,34(1):33-35.

9刘云建,胡启阳,李新海,王志兴,郭华军,彭文杰.从不合格锂离子蓄电池中直接回收钴酸锂[J].电源技术,2006,30(4):308-310. 被引量:14

10何汉兵,秦毅红.从废旧锂离子蓄电池中回收钴[J].电源技术,2006,30(4):311-314. 被引量:7

1汪成东,施素杰,朱浪,李春滢,石贵明.废旧锂电池的回收处理进展及趋势[J].玉溪师范学院学报,2020(3):59-67. 被引量:2

2吴晓伟,秦佩.基于三元电池正极材料制程的废水资源化回用工艺技术[J].电子技术(上海),2020(2):165-167.

3唐娜娜,马少健,莫伟.从某锰矿浸渣中回收钴的浮选试验研究[J].有色矿冶,2006,22(S1):8-9. 被引量:4

4唐娜娜,莫伟,马少健.钴矿资源及其选矿研究进展[J].有色矿冶,2006,22(S1):5-7. 被引量:7

5安洪力,吴宁宁,范茂松,李其其格.锰酸锂动力锂离子二次电池中主要化学元素的回收研究[J].北京大学学报:自然科学版,2006,42(S1):83-86. 被引量:6

6孟燕莎.低碳发展标准化实践之废旧手机回收再利用[J].标准科学,2013(12):17-19. 被引量:1

7刘庄,黄旭江,许开华,张翔.废旧锂离子电池制备硬脂酸钴的研究[J].化工新型材料,2011,39(S2):111-113. 被引量:2

8程家蓉,潘伦,陈先玉,许新.废旧手机电池资源综合利用现状[J].消费导刊,2009,0(14):197-197.

9胡宝磊,周雍茂.红土镍矿硫酸铵焙烧-水浸实验研究[J].现代冶金,2013,41(3):11-14. 被引量:2

10戴长松,路密,熊岳平,江洪伟.废旧锂离子电池处理处置现状及污染防治对策[J].环境科学与技术,2013,36(S2):332-335. 被引量:13

1丁慧,潘帅军,吕经康,张登科,陈得军,石起增,卢雁.由锂离子电池正极废料制备电池级硫酸钴的研究[J].河南师范大学学报:自然科学版,2007,35(2):193-194. 被引量:8

2谭海翔,胡启阳,李新海,王志兴,郭华军.含铝硫酸钴溶液中回收氧化钴新工艺的研究[J].稀有金属与硬质合金,2006,34(1):33-35.

3张永禄,王成彦,杨卜,杨永强.废旧锂离子电池LiCoO_2电极中钴的浸出动力学[J].有色金属:冶炼部分,2012(8):4-6. 被引量:6

4王文军.硫酸-双氧水体系氧化浸出铅冰铜的试验研究[J].湖南有色金属,2016,32(6):30-32. 被引量:2

5宾智勇,刘景槐,吴海国,李婕.废旧锂离子电池的综合利用试验研究[J].湖南有色金属,2008,24(5):27-31. 被引量:8

6新技术[J].中国金属通报,2002,0(18):17-13.

7吉鸿安.锂离子电池正极废料中钴和锂的回收[J].甘肃冶金,2012,34(4):63-66. 被引量:3

8张守全,程登峰,王海峰,肖伟.粗大钴团在硬质合金烧结过程中的演变[J].粉末冶金材料科学与工程,2010,15(6):661-666. 被引量:7

9苏树发,曹高劭,赵新兵.金属锑薄膜用作锂离子电池负极的研究[J].稀有金属材料与工程,2005,34(3):452-454. 被引量:10

10张文钲,刘燕.钼冶金技术发展近况[J].中国钼业,2013,37(3):1-5. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF816.052[冶金工程—有色金属冶金]

Citation Information:

According to the property of LiCoO 2 in Li-ion secondary battery anode wastes of Al Co film,dissolution reaction of LiCoO 2 in a system of H 2SO 4 and H 2O 2 was put forward: 2LiCoO 2+3H 2SO 4+H 2O 2→Li 2SO 4+2CoSO 4+4H 2O+O 2↑ A simple process for recycling cobalt and aluminum was determined,including alkali leaching of wastes,acid dissolution of slag,purification of cobalt containing solution and precipitation of cobalt.The recovery of cobalt reaches 95.75%.Aluminum in alkali leaching solution was neutralized with H 2SO 4 and the product Al(OH) 3with a chemical purity was obtained,the recycling rate is 94.84%.The profit of 45600.6 RMB Yuan can be obtained in treating l ton waste by the technology.

quote

GB/T 7714-2015 [1] ZHONG Hai-yun, LI Jian, CHAI Li-yuan. Study on Technology for Recycling Cobalt from Li-ion Secondary Battery Anode Scrap of Al-Co Film[J]. Rare Metals and Cemented Carbides, 2001(1): 1-4.
MLA [1] ZHONG Hai-yun, et al., "Study on Technology for Recycling Cobalt from Li-ion Secondary Battery Anode Scrap of Al-Co Film." Rare Metals and Cemented Carbides, no. 1, 2001, pp. 1-4.
APA [1] ZHONG Hai-yun, LI Jian, & CHAI Li-yuan. (2001). Study on Technology for Recycling Cobalt from Li-ion Secondary Battery Anode Scrap of Al-Co Film. Rare Metals and Cemented Carbides(1), 1-4.
IEEE [1] ZHONG Hai-yun, LI Jian, and CHAI Li-yuan, "Study on Technology for Recycling Cobalt from Li-ion Secondary Battery Anode Scrap of Al-Co Film," Rare Metals and Cemented Carbides, no. 1, pp. 1-4, 2001. keywords: {Li ion secondary battery;anode material scrap;LiCoO 2;recycling;cobalt;cobalt oxalate}